摘要: A carbon brush is provided that improves motor efficiency and achieves a longer service life. A carbon brush (1) to be pressed against an electrically-conductive rotor (2) is characterized by containing mesocarbon powder and an aggregate material containing carbon as at least one component thereof. It is preferable that the mesocarbon powder have a substantially spherical shape, and it is also preferable that the mesocarbon powder has been subjected to a preheating treatment. In addition, it is preferable that the temperature of the preheating treatment be from 500° C. to 700° C.
摘要翻译: 提供了一种提高电机效率并实现更长使用寿命的碳刷。 压在导电转子(2)上的碳刷(1)的特征在于,含有中间相碳粉末和含有至少一种碳的骨料。 中间相碳粉末优选为大致球状,优选中间相碳粉已进行预热处理。 此外,预热处理的温度优选为500〜700℃。