2XXX ALUMINUM LITHIUM ALLOYS
    1.
    发明申请

    公开(公告)号:US20210404038A1

    公开(公告)日:2021-12-30

    申请号:US17307453

    申请日:2021-05-04

    Abstract: New 2xxx aluminum alloys having are disclosed. The new 2xxx aluminum alloys generally include 2.5-3.9 wt. % Cu, 0.82-1.20 wt. % Li, 0.5-2.0 wt. % Zn, 0.10-0.60 wt. % Mn, 0.05-0.35 wt. % Mg, from 0.05 to 0.50 wt. % of at least one grain structure control element, wherein the at least one grain structure control element is selected from the group consisting of Zr, Sc, Cr, V, Hf, other rare earth elements, and combinations thereof, up to 0.22 wt. % Ag, up to 0.15 wt. % Fe, up to 0.12 wt. % Si, and up to 0.15 wt. % Ti, the balance being aluminum, incidental elements and impurities. The new 2xxx aluminum alloys may realize an improved combination of two or more of strength, fracture toughness, elongation, and corrosion resistance.

    2XXX aluminum lithium alloys
    3.
    发明授权

    公开(公告)号:US12194529B2

    公开(公告)日:2025-01-14

    申请号:US17307453

    申请日:2021-05-04

    Abstract: New 2xxx aluminum alloys having are disclosed. The new 2xxx aluminum alloys generally include 2.5-3.9 wt. % Cu, 0.82-1.20 wt. % Li, 0.5-2.0 wt. % Zn, 0.10-0.60 wt. % Mn, 0.05-0.35 wt. % Mg, from 0.05 to 0.50 wt. % of at least one grain structure control element, wherein the at least one grain structure control element is selected from the group consisting of Zr, Sc, Cr, V, Hf, other rare earth elements, and combinations thereof, up to 0.22 wt. % Ag, up to 0.15 wt. % Fe, up to 0.12 wt. % Si, and up to 0.15 wt. % Ti, the balance being aluminum, incidental elements and impurities. The new 2xxx aluminum alloys may realize an improved combination of two or more of strength, fracture toughness, elongation, and corrosion resistance.

    METHODS OF PRODUCING 2XXX ALUMINUM ALLOYS
    4.
    发明公开

    公开(公告)号:US20240175114A1

    公开(公告)日:2024-05-30

    申请号:US18435464

    申请日:2024-02-07

    CPC classification number: C22F1/057 C22C21/14 C22C21/16 C22C21/18

    Abstract: Methods of making new 2xxx aluminum alloy sheet products are disclosed. In one approach, a method comprises artificially aging a 2xxx aluminum alloy in at least two-steps. In one embodiment, the first aging step comprises first aging a 2xxx aluminum alloy at a first temperature of from 300° F. to 450ºF and for a first aging time of from 4 to 120 hours, and second aging the 2xxx aluminum alloy at a second temperature for a second aging time of from 30 minutes to 120 hours, wherein the second temperature is from 20° F. to 150° F. lower than the first temperature. The new two-step artificial aging step may facilitate an improved combination of properties, such as an improved combination of two or more of strength, ductility, fracture toughness, and corrosion resistance.

    7XXX ALUMINUM ALLOYS
    6.
    发明申请

    公开(公告)号:US20210340656A1

    公开(公告)日:2021-11-04

    申请号:US17308794

    申请日:2021-05-05

    Abstract: New 7xxx aluminum alloys are disclosed. The new 7xxx aluminum alloys generally include from 0.05 to 1.0 wt. % Ag. In one approach, a new 7xxx aluminum alloy includes from 0.05 to 1.0 wt. % Ag, from 5.5 to 9.0 wt. % Zn, from 1.2 to 2.6 wt. % Cu, from 1.3 to 2.5 wt. % Mg, up to 0.60 wt. % Mn, up to 1.0 wt. % of at least one grain structure control material, wherein the at least one grain structure control material is selected from the group consisting of Zr, Cr, V, Hf, other rare earth elements, and combinations thereof, up to 0.30 wt. % Fe, up to 0.30 wt. % Si, up to 0.15 wt. % Ti, not greater than 0.08 wt. % Sc, and not greater than 0.05 wt. % Li, the balance being aluminum, optional incidental elements and impurities.