摘要:
A composition comprising water atomised prealloyed iron-based steel powder is provided which steel powder comprises by weight-%: 0.2-1.5 Cr, 0.05-0.4 V, 0.09-0.6 Mn, less than 0.1 Mo, less than 0.1 Ni, less than 0.2 Cu, less than 0.1 C, less than 0.25 O, less than 0.5 of unavoidable impurities, the balance being iron. A method of forming a sintered component, and component additionally are provided.
摘要:
A water atomised prealloyed iron-based steel powder is provided which comprises by weight-%: 0.2-1.5 Cr, 0.05-0.4 V, 0.09-0.6 Mn, less than 0.1 Mo, less than 0.1 Ni, less than 0.2 Cu, less than 0.1 C, less than 0.25 O, less than 0.5 of unavoidable impurities, the balance being iron.
摘要:
An iron-based powder composition for metal injection molding having an average particle size of 20-60 μm, and having 99% of the particles less than 120 μm wherein the iron-based powder composition includes, by weight percent of the iron-based powder composition: Mo: 0.3-1.6, P: 0.1-0.6, optionally Cu: up to 3.0, optionally Si: up to 0.6, optionally Cr: up to 5, optionally, unavoidable impurities: up to 1.0, whereof carbon is less than 0.1, the balance being iron, and wherein the sum of Mo and 8*P content is within the range of 2-4.7.
摘要:
An iron-based powder composition for metal injection molding having an average particle size of 20-60 μm, and having 99% of the particles less than 120 μm wherein the iron-based powder composition includes, by weight percent of the iron-based powder composition: Mo: 0.3-1.6, P: 0.1-0.6, optionally Cu: up to 3.0, optionally Si: up to 0.6, optionally Cr: up to 5, optionally, unavoidable impurities: up to 1.0, whereof carbon is less than 0.1, the balance being iron, and wherein the sum of Mo and 8*P content is within the range of 2-4.7.