公开(公告)号:US20220073718A1
公开(公告)日:2022-03-10
申请号:US17423407
申请日:2020-01-15
Applicant: BOREALIS AG
Inventor: Jingbo WANG , Markus GAHLEITNER , Friedrich BERGER , Karlheinz FRIEDRICH
IPC: C08L23/14 , C08F2/00 , C08F210/02 , C08F210/14 , C08F4/646 , C08F4/649 , C08F4/654 , B29C49/04
Abstract: The present invention is directed to a propylene polymer composition comprising at least one propylene copolymer (C-PP), and an α-nucleating agent (NU), wherein the propylene copolymer (C-PP) comprises two propylene copolymer fractions (PP1) and (PP2), wherein propylene copolymer fraction (PP1) is contained in the propylene copolymer (C-PP) in an amount of 30 to 70 wt. % and the propylene copolymer fraction (PP2) is contained in the propylene copolymer (C-PP) in an amount of 70 to 30 wt. %, the comonomer content of propylene copolymer fraction (PP1) is in the range of 0.5 to 2.5 wt.-% and the comonomer content of the propylene copolymer fraction (PP1) is lower compared to the comonomer content of the propylene copolymer fraction (PP2), and the propylene polymer composition has (a) a melt flow rate MFR2 (230° C.) measured according to according to ISO 1133 of 1 to 5 g/10 min., and (b) a comonomer content of 4.0 to 8.0 wt. %, the comonomer(s) being ethylene and/or at least one C4 to C12 α-olefin. The above propylene polymer composition has improved impact and optical properties. The invention further provides a method of producing the above propylene polymer composition and an extrusion blow molded article comprising the above propylene polymer composition.