公开(公告)号:US20170137617A1
公开(公告)日:2017-05-18
申请号:US15310283
申请日:2015-05-18
Applicant: BOREALIS AG
Inventor: Jingbo WANG , Luigi RESCONI , Petar DOSHEV , Markus GAHLEITNER
IPC: C08L23/14
Abstract: Polypropylene composition comprising a heterophasic propylene copolymer and a mineral filler, wherein said heterophasic propylene copolymer has a melting temperature in the range of 140 to 155° C., a xylene cold soluble content in the range of 20 to 35 wt.-% and a comonomer content of the xylene cold soluble fraction in the range of 18 to 95 wt.-%, wherein further the weight ratio between heterophasic propylene copolymer and the mineral filler is in the range of 2/1 to 4/1.
-
公开(公告)号:US20160333175A1
公开(公告)日:2016-11-17
申请号:US15109855
申请日:2015-01-06
Applicant: BOREALIS AG
Inventor: Jingbo WANG , Petar DOSHEV , Luigi RESCONI , Wilfried TOLTSCH
CPC classification number: C08L23/142 , C08F210/06 , C08J5/18 , C08J2323/16 , C08J2423/16 , C08F110/06 , C08F2500/03 , C08F2500/12 , C08F2500/17 , C08F2500/20 , C08F210/16 , C08F2/001
Abstract: A heterophasic propylene ethylene copolymer having an MFR2 of 0.5 to 100 g/10m in and obtained using single site catalysis comprising: (i) a propylene homopolymer or propylene ethylene copolymer matrix having up to 4 wt % ethylene; and (ii) an ethylene propylene rubber (EPR) dispersed in the matrix; said heterophasic propylene ethylene copolymer having a xylene cold soluble content (XS) of 20 to 40%; wherein the ethylene content of the xylene cold soluble fraction of said heterophasic propylene ethylene copolymer is between 70 and 90 wt.%; wherein the xylene cold soluble fraction of said heterophasic propylene ethylene copolymer has an intrinsic viscosity (IV) of 3.0 dl/g or more; and wherein the melting enthalpy (AHM) of the heterophasic propylene ethylene copolymer is between 10 and 30 J/g at a temperature of 0 to 130° C.
Abstract translation: 使用单位点催化得到MFR 2为0.5至100g / 10m的多相丙烯乙烯共聚物,其包含:(i)具有至多4重量%乙烯的丙烯均聚物或丙烯乙烯共聚物基质; 和(ii)分散在基质中的乙丙橡胶(EPR); 所述异相丙烯乙烯共聚物具有20至40%的二甲苯冷可溶物含量(XS); 其中所述多相丙烯乙烯共聚物的二甲苯冷可溶部分的乙烯含量为70-90重量%; 其中所述多相丙烯乙烯共聚物的二甲苯冷可溶部分的特性粘度(IV)为3.0dl / g以上; 并且其中异相丙烯乙烯共聚物的熔融焓(AHM)在0至130℃的温度下为10至30J / g。
-
公开(公告)号:US20170218172A1
公开(公告)日:2017-08-03
申请号:US15514641
申请日:2015-10-02
Applicant: BOREALIS AG
Inventor: Jingbo WANG , Daniela MILEVA , Petar DOSHEV , Markus GAHLEITNER
CPC classification number: C08K5/0083 , C08J3/203 , C08J5/18 , C08J2323/10 , C08J2323/12 , C08L2203/16 , C08L2205/24 , C08L23/10
Abstract: The present invention presents a new method for preparation of an α-nucleated crystalline polypropylene based on polymeric nucleating agents and very high cooling rates, further the α-nucleated crystalline polypropylene based on polymeric nucleating agents derived thereof and its use in final articles derivable thereof.
-
公开(公告)号:US20160237270A1
公开(公告)日:2016-08-18
申请号:US15029493
申请日:2014-10-23
Applicant: BOREALIS AG
Inventor: Jingbo WANG , Katja KLIMKE , Petar DOSHEV , Pauli LESKINEN
CPC classification number: C08L23/142 , B65D1/0207 , C08L23/14 , C08L2203/10 , C08L2205/02 , C08L2205/025
Abstract: Blow molded article comprising a propylene copolymer composition, the propylene copolymer composition comprises (a) a propylene copolymer (A) having a comonomer content of 0.1 to 2.5 mol-%, the comonomers are C5 to C12 α-olefins, and (b) a propylene copolymer (B) having a comonomer content of 1.0 to 7.0 mol-%, the comonomers are C5 to C12 α-olefins, wherein further (i) the comonomer content in the propylene copolymer (A) is lower compared to the comonomer content in the propylene copolymer (B), (ii) the propylene copolymer composition has a comonomer content of 0.4 to 5.0 mol-%, the comonomers are C5 to C12 α-olefins.
Abstract translation: 包含丙烯共聚物组合物的吹塑制品,丙烯共聚物组合物包含(a)共聚单体含量为0.1至2.5摩尔%的丙烯共聚物(A),共聚单体为C 5至C 12α-烯烃,和(b) 丙烯共聚物(B)的共聚单体含量为1.0〜7.0摩尔%,共聚单体为C 5〜C 12α-烯烃,其中,(i)丙烯共聚物(A)中的共聚单体含量比共聚单体含量低 丙烯共聚物(B),(ii)丙烯共聚物组合物的共聚单体含量为0.4〜5.0摩尔%,共聚单体为C 5〜C 12α-烯烃。
-
-
-