POSITIVE ELECTRODE SHEET AND LITHIUM-ION BATTERY

    公开(公告)号:US20240405209A1

    公开(公告)日:2024-12-05

    申请号:US18804688

    申请日:2024-08-14

    Abstract: A positive electrode sheet includes a positive electrode current collector and a positive electrode active material layer arranged on at least a surface of the positive electrode current collector. The positive electrode active material layer includes a positive electrode active material, which includes a first lithium iron phosphate material and a second lithium iron phosphate material. When the cumulative volume distribution percentage of the first lithium iron phosphate material is 50%, the particle size is D1v50 μm. When the cumulative volume distribution percentage of the second lithium iron phosphate material is 50%, the particle size is D2v50 μm. D1v50 is 0.3-0.95, and D2v50 is 1.0-3.5. When the volume density of the positive electrode active material reaches a maximum value, the particle size is Dmo μm, the compaction density of the positive electrode sheet is PD g/cm3 under a pressure of 1.5 Mpa, and 0.45≤PD×Dmo≤12.38.

    LITHIUM IRON PHOSPHATE POSITIVE ELECTRODE ACTIVE MATERIAL, POSITIVE ELECTRODE SHEET AND LITHIUM ION BATTERY

    公开(公告)号:US20240405217A1

    公开(公告)日:2024-12-05

    申请号:US18802786

    申请日:2024-08-13

    Abstract: A lithium iron phosphate positive electrode active material includes: a first lithium iron phosphate material having a particle size of D1v50 μm in a range of 0.3-0.95 at 50% cumulative volume distribution of the first lithium iron phosphate material, and a second lithium iron phosphate material having a particle size of D2v50 μm in a range of 1.0-3.5 at 50% cumulative volume distribution of the second lithium iron phosphate material. Particle sizes of the lithium iron phosphate positive electrode active material are respectively Dv90 μm, Dv10 μm, and Dv50 μm at 90%, 10%, and 50% cumulative volume distribution of the lithium iron phosphate positive electrode active material, a particle size of the lithium iron phosphate positive electrode active material is Dn50 μm at 50% cumulative number distribution of the lithium iron phosphate positive electrode active material, and 0.16 ≤ D v ⁢ 90 - D v ⁢ 10 D v ⁢ 50 + D v ⁢ 50 × D n ⁢ 50 ≤ 31.1 .

Patent Agency Ranking