公开(公告)号:US3904426A
公开(公告)日:1975-09-09
申请号:US49501474
申请日:1974-08-05
Applicant: IBM
Inventor: FRIESER RUDOLF G , POWELL JIMMIE L , TUMMALA RAO R
CPC classification number: C03C8/245 , C03C3/0745
Abstract: A process for manufacturing a sealing glass composition consisting essentially of the following ingredients in the following proportions:
The process comprises the steps of providing the batch of ingredients to the above proportions and insuring a full mixture or mixing of the same. Thereafter, in one embodiment of the process, the batch may be heated to between 750 and 850*C to form a liquid melt and then the liquid melt is further heated until the temperature is 1,100 + OR - 20*C. The temperature of the melt is held between the aforementioned limits for a period of at least 3 hours and no longer than 3 1/2 hours, and thereafter the temperature of the melt is lowered to effectively inhibit bubbling of the liquid melt, and then the melt is removed for further processing.Abstract translation: 一种密封玻璃组合物的制造方法,主要由下列成分组成:}重量%} PbO 66.0} B2O3 14.0} SiO2 2.0} Al2O3 3.5} ZnO 10.5} CuO 2.5} Bi2O3 1。