公开(公告)号:US20220025142A1
公开(公告)日:2022-01-27
申请号:US17254916
申请日:2020-02-26
Applicant: SEIKO PMC CORPORATION
Inventor: Ryo MIYAMORI , Daisuke KUROKI , Hideya SEKIGUCHI , Akihiro SATO
Abstract: [Problem] An object of the present invention is to provide a foam including a thermoplastic resin and rubber as a main component, in which a micronized product of a cellulose fiber is uniformly dispersed, and uniformity and mechanical properties are excellent. [Solution] A foam includes a modified cellulose fiber (A) covalently bonded with a diene-based polymer, a thermoplastic resin and/or rubber (B), and a diene-based polymer (C) having a functional group capable of covalently bonding with a cellulose fiber, in which the fiber (A) is micronized, the fiber (A) has a content of 0.05 to 20% by mass, and the thermoplastic resin and/or rubber (B) has a glass transition point of −130° C. to 120° C.
-
2.
公开(公告)号:US20180162960A1
公开(公告)日:2018-06-14
申请号:US15578631
申请日:2016-06-22
Applicant: SEIKO PMC CORPORATION
Inventor: Ryo MIYAMORI , Syuichi OHIRA , Daisuke KUROKI
CPC classification number: C08C19/28 , B29B7/002 , B29B7/005 , B29B7/7495 , B29B7/905 , B29B7/92 , C08B3/20 , C08G81/00 , C08J5/045 , C08L1/08 , C08L7/00 , C08L9/00 , C08L15/00 , C08L21/00 , C08L97/02 , C08L2205/16
Abstract: Provided are modified plant fibers suitable for addition to rubber; an additive for rubber comprising the modified plant fibers which can be micronized and dispersed easily and highly when adding to rubber; a method of preparing the additive for rubber; and a rubber composition comprising the additive for rubber. Modified plant fibers (A) in which plant fibers (a) and a modified synthetic rubber (B) are covalently bonded wherein the ratio of the modified synthetic rubber (B) relative to 100 parts by weight of the plant fibers (a) is 5 to 100 parts by weight. An additive for rubber comprising 20 to 75 weight % of the modified plant fibers (A) according to claim 1 and 25 to 80 weight % of a processing agent for rubber (C), wherein the number average molecular weight of the processing agent for rubber (C) is 400 to 60,000, and the glass transition point of the processing agent for rubber (C) is 100° C. or less, and wherein the additive for rubber includes plant fibers in the ratio of 10 to 65 weight %.
-