Gallium-modified titanium aluminum alloys and method of preparation
    91.
    发明授权
    Gallium-modified titanium aluminum alloys and method of preparation 失效
    镓改性钛铝合金及其制备方法

    公开(公告)号:US4902474A

    公开(公告)日:1990-02-20

    申请号:US293035

    申请日:1989-01-03

    CPC classification number: C22C14/00

    Abstract: A TiAl composition is prepared to have high strength and to have improved ductility by altering the atomic ratio of the titanium and aluminum to have what has been found to be a highly desirable effective aluminum concentration by addition of gallium according to the approximate formula Ti.sub.52-47 Al.sub.42-46 Ga.sub.3-7.

    Abstract translation: 通过改变钛和铝的原子比来制备TiAl组合物以具有高强度并具有改善的延展性,通过根据近似式Ti52-47Al42,通过添加镓,发现已经发现是非常理想的有效铝浓度 -46Ga3-7。

    Carbon containing boron doped tri-nickel aluminide
    92.
    发明授权
    Carbon containing boron doped tri-nickel aluminide 失效
    含硼硼掺杂的三镍铝化物

    公开(公告)号:US4725322A

    公开(公告)日:1988-02-16

    申请号:US783513

    申请日:1985-10-03

    CPC classification number: C22C19/007

    Abstract: A tri-nickel aluminide base alloy composition is provided with a desirable combination of tensile strength and ductility. The composition is prepared to include boron dopant in combination with relatively low percentages of carbon for the high increase in strength achieved. The composition has an Ll.sub.2 of crystalline structure. It is prepared by rapid solidification at a cooling rate of at least 10.sup.3 .degree. C. per second.

    Abstract translation: 三镍铝基合金组合物具有拉伸强度和延展性的理想组合。 制备组合物以包含硼掺杂剂与相对低百分比的碳的组合,以实现高强度的增加。 该组合物具有晶体结构的L12。 通过以每秒至少103℃的冷却速度快速固化而制备。