High shrinkage polyester fibers and method of preparation
    11.
    发明授权
    High shrinkage polyester fibers and method of preparation 失效
    高收缩聚酯纤维及其制备方法

    公开(公告)号:US5070185A

    公开(公告)日:1991-12-03

    申请号:US503084

    申请日:1990-03-30

    申请人: Wayne S. Stanko

    发明人: Wayne S. Stanko

    IPC分类号: D01F6/62

    CPC分类号: D01F6/62

    摘要: High shrinkage polyester fibers having good strength and uniform dyeability are disclosed, along with a method of producing the high shrinkage polyester fibers, by drawing a feeder yarn having a birefringence (n) of at least 0.0175 at a temperature below the glass transition temperature for the polyester and with carefully controlled draw ratios.