摘要:
The present invention provides a method for producing a toner, the method including: preparing a wax dispersion liquid by cooling a wax solution, in which a wax is heated and dissolved or dispersed in an organic solvent, in a container so that a standard deviation σ of a temperature distribution between a center portion of the container and an inner wall of the container is 0.5 or less and the cooling rate is 2.0° C./min or more, to precipitate wax particles in the wax solution; forming toner base precursor particles by adding an aqueous phase containing resin fine particles into an oil phase containing at least the wax dispersion liquid, a colorant and a binder resin and mixing the oil phase and the aqueous phase with each other; and preparing toner base particles by removing the solvent from the toner base precursor particles.
摘要:
A toner including at least one polyester resin serving as a binder resin, a colorant, a releasing agent, and a fixing aid, wherein the fixing aid includes a fatty acid amide-based compound, and the fatty acid amide-based compound is at least one of a fatty acid amide compound having a mono- or higher valent amide bond and a fatty acid amide-based compound having a mono- or higher valent amino group or a hydroxyl group.
摘要:
A toner, including a colorant; a binder resin; a release agent; and a fixing supplemental component, wherein the toner has a storage elastic modulus G′ (Pa) satisfying the following conditions: 5.0×104
摘要:
To provide a toner produced by emulsifying or dispersing in an aqueous medium particles containing at least polyester resin particles and by aggregating the polyester resin particles, wherein the polyester resin particles contain a polyester resin, the polyester resin is produced by condensation polymerization of an alcohol component containing 65 mol % or more 1,2-propanediol in a dihydroxy alcohol component and a carboxylic acid component containing purified rosin, and the softening point of the polyester resin is 80° C. or more and less than 120° C., and wherein the toner comprises a colorant and a releasing agent.
摘要:
A method of manufacturing toner including melting, mixing, and kneading a releasing agent and a coloring agent with at least part of a polyester binder resin, and suspending and granulating an oil phase comprising the binder resin, the coloring agent, and the releasing agent in an aqueous medium.
摘要:
A toner, including a colorant; a binder resin; a release agent; and a fixing supplemental component, wherein the toner has a storage elastic modulus G′ (Pa) satisfying the following conditions: 5.0×104
摘要:
A toner including at least one polyester resin serving as a binder resin, a colorant, a releasing agent, and a fixing aid, wherein the fixing aid includes a fatty acid amide-based compound, and the fatty acid amide-based compound is at least one of a fatty acid amide compound having a mono- or higher valent amide bond and a fatty acid amide-based compound having a mono- or higher valent amino group or a hydroxyl group.
摘要:
The present invention provides a toner containing at least a binder resin, a releasing agent, and a colorant, wherein the binder resin contains at least a polyester resin (A) having a softening point Tm(A) of 120° C. to 160° C., a polyester resin (B) having a softening point Tm(B) of 80° C. or more and less than 120° C. and a composite resin (C) containing a condensation polymerization monomer and an addition polymerization monomer, at least any one of the polyester resins (A) and (B) is a polyester resin prepared by condensation-polymerizing an alcohol component substantially composed of only aliphatic alcohol with a carboxylic acid component, and 65% or more of the alcohol component is 1,2-propanediol.
摘要:
A method of manufacturing toner including melting, mixing, and kneading a releasing agent and a coloring agent with at least part of a polyester binder resin, and suspending and granulating an oil phase comprising the binder resin, the coloring agent, and the releasing agent in an aqueous medium.
摘要:
The present invention provides a toner containing at least a binder resin, a releasing agent, and a colorant, wherein the binder resin contains at least a polyester resin (A) having a softening point Tm (A) of 120° C. to 160° C., a polyester resin (B) having a softening point Tm (B) of 80° C. or more and less than 120° C. and a composite resin (C) containing a condensation polymerization monomer and an addition polymerization monomer, at least any one of the polyester resins (A) and (B) is a polyester resin prepared by condensation-polymerizing an alcohol component substantially composed of only aliphatic alcohol with a carboxylic acid component, and 65% or more of the alcohol component is 1,2-propanediol.