Abstract:
There is provided a carrier including a magnetic core material having a surface coated with a surfactant-containing resin mixture of an elemental fluorine-containing resin and a polyimide resin. The carrier has an elution amount of an eluted material into water in an elution test ranging from 180 ppm to 3,500 ppm.
Abstract:
A magnetic core material for electrophotographic developer, satisfying a value of Expression (1): a+b×10+c+d+e+f, being from 300 to 1,300, when an amount of fluorine ion is denoted by a (ppm), an amount of chlorine ion is denoted by b (ppm), an amount of bromide ion is denoted by c (ppm), an amount of nitrite ion is denoted by d (ppm), an amount of nitrate ion is denoted by e (ppm), and an amount of sulfate ion is denoted by f (ppm), which are measured by combustion ion chromatography, and having a BET specific surface area being from 0.06 to 0.25 m2/g.
Abstract:
Disclosed are a resin-filled ferrite carrier core material for an electrophotographic developer, including a porous ferrite particle having an average compression strength of 100 mN or more and a coefficient of variation of the compression strength of 50% or less, a ferrite carrier obtained by filling a resin in the voids of the ferrite carrier core material, and an electrophotographic developer using the ferrite carrier.