Toner for developing electrostatic image, developer for developing electrostatic image, and method for forming image
    12.
    发明授权
    Toner for developing electrostatic image, developer for developing electrostatic image, and method for forming image 有权
    用于显影静电图像的调色剂,用于静电图像显影的显影剂和形成图像的方法

    公开(公告)号:US08039186B2

    公开(公告)日:2011-10-18

    申请号:US11505918

    申请日:2006-08-18

    IPC分类号: G03G9/087

    摘要: A toner for developing an electrostatic image comprises: a binder resin; and a releasing agent, wherein the binder resin comprises a polycondensation resin obtained by polycondensing a polycondensation monomer in the presence of a polycondensation catalyst, the releasing agent comprises a condensation compound obtained by condensing a condensation monomer in the presence of a condensation catalyst, the toner contains a metallic element derived from the polycondensation catalyst and the condensation catalyst in an amount of from 0 to 10 ppm, and the toner contains a sulfur component in an amount of from 100 to 20,000 ppm.

    摘要翻译: 用于显影静电图像的调色剂包括:粘合剂树脂; 和脱模剂,其中粘合剂树脂包括通过在缩聚催化剂存在下使缩聚单体缩聚得到的缩聚树脂,该脱模剂包括在缩合催化剂存在下缩合缩合单体得到的缩合化合物,调色剂 含有衍生自缩聚催化剂的金属元素和0〜10ppm的缩合催化剂,调色剂含有100〜20000ppm的硫成分。

    Image forming method using toner having block copolymer
    14.
    发明授权
    Image forming method using toner having block copolymer 有权
    使用具有嵌段共聚物的调色剂的成像方法

    公开(公告)号:US07645553B2

    公开(公告)日:2010-01-12

    申请号:US11352362

    申请日:2006-02-13

    IPC分类号: G03G15/20

    摘要: An image forming method, which comprises: forming an electrostatic latent image on a surface of a latent image supporting member; developing the electrostatic latent image formed on the surface of the latent image supporting member with a toner for developing an electrostatic latent image or an electrostatic latent image developer containing the toner and a carrier to form a toner image; transferring the toner image formed on the surface of the latent image supporting member onto a surface of a transfer receiving material; and fixing the toner image transferred onto the transfer receiving material under pressure, wherein the toner comprises a block copolymer having a crystalline polyester block and a non-crystalline polyester block, and wherein a maximum pressure applied when the image is fixed is 1 MPa or greater but not greater than 10 MPa.

    摘要翻译: 一种图像形成方法,包括:在潜像支撑构件的表面上形成静电潜像; 利用用于显影静电潜像的调色剂或含有调色剂和载体的静电潜像显影剂来形成在潜像支撑构件的表面上形成的静电潜像以形成调色剂图像; 将形成在所述潜像支撑构件的表面上的调色剂图像转印到转印接收材料的表面上; 以及在压力下转印到转印接收材料上的调色剂图像,其中调色剂包括具有结晶聚酯嵌段和非结晶聚酯嵌段的嵌段共聚物,并且其中当图像固定时施加的最大压力为1MPa或更大 但不大于10MPa。

    Binder resin for electrostatic image developing toner, binder resin liquid dispersion for electrostatic image developing toner, electrostatic image developing toner and production processes thereof
    15.
    发明申请
    Binder resin for electrostatic image developing toner, binder resin liquid dispersion for electrostatic image developing toner, electrostatic image developing toner and production processes thereof 有权
    用于静电图像显影调色剂的粘合剂树脂,用于静电图像显影调色剂的粘合剂树脂液体分散体,静电图像显影调色剂及其制备方法

    公开(公告)号:US20070148579A1

    公开(公告)日:2007-06-28

    申请号:US11445230

    申请日:2006-06-02

    IPC分类号: G03G9/087

    摘要: A binder resin for an electrostatic image developing toner is obtained by a polycondensation reaction of a polycarboxylic acid and a polyol, wherein the polycarboxylic acid includes a compound represented by at least one of formula (1) and formula (2) as defined in the specification in an amount of from about 50 to about 100 mol %; the polyol includes a compound represented by formula (3) as defined in the specification in an amount of from about 10 to about 100 mol %; and a content of a catalyst-originated metal element in the binder resin is about 100 ppm or less. R1OOCA1mB1nA1lCOOR1′   (1) R2OOCA2pB2qA2rCOOR2′   (2) HOXh—Ph—Y—Ph—XkOH   (3)

    摘要翻译: 用于静电图像显影调色剂的粘合剂树脂通过多元羧酸和多元醇的缩聚反应获得,其中多元羧酸包括由说明书中定义的至少一种式(1)和式(2)表示的化合物 其量为约50至约100摩尔%; 多元醇包括按说明书中定义的式(3)表示的化合物,其量为约10至约100摩尔%; 并且粘合剂树脂中催化剂起始的金属元素的含量为约100ppm以下。 <?in-line-formula description =“In-line Formulas”end =“lead”?> R&lt; 1&lt; OOCA&lt; 1&lt; (1)&lt; 1&gt;&lt; 1&gt;&lt; 1&gt; -formulae description =“In-line Formulas”end =“tail”?> <?in-line-formula description =“In-line Formulas”end =“lead”?> R&lt; 2&lt; OOCA& 第2类 <2> (2)<?in-line-formula description =“In-line Formulas”end =“tail”?> <?in-line-formula description =“In-line Formulas”end =“lead”→HOX -Ph-Y-Ph-XK OH(3)<?in-line-formula description =“In-line Formulas” end =“tail”?>

    Method of producing toner for developing electrostatic charge image, toner for developing electrostatic charge image, developer for electrostatic charge image and method for forming image
    16.
    发明申请
    Method of producing toner for developing electrostatic charge image, toner for developing electrostatic charge image, developer for electrostatic charge image and method for forming image 失效
    用于制造用于显影静电荷图像的调色剂的方法,用于显影静电荷图像的调色剂,用于静电荷图像的显影剂和用于形成图像的方法

    公开(公告)号:US20070092822A1

    公开(公告)日:2007-04-26

    申请号:US11345307

    申请日:2006-02-02

    IPC分类号: G03G9/087 G03G15/20

    摘要: A method of producing a toner for developing electrostatic charge image, the method comprising: aggregating particles containing a crystalline polyester resin, particles containing a non-crystalline polyester resin and particles of a releasing agent in an aqueous medium, so as to form aggregated particles; and heating the aggregated particles to fuse into a coalescent body, wherein at least one of the crystalline polyester resin and the non-crystalline polyester resin is obtained by polymerization at temperatures not higher than 150° C. with a Bronsted acid containing a sulfur atom as a catalyst, and wherein a first onset temperature A(° C.) of the toner and a glass transition temperature B(° C.) of the non-crystalline polyester resin as measured by differential scanning calorimeter satisfy a relation (B−A)≦10, and wherein a weight average molecular weight of the crystalline polyester resin is ½ or lower of a weight average molecular weight of the non-crystalline polyester resin.

    摘要翻译: 一种制备用于显影静电荷图像的调色剂的方法,所述方法包括:在水性介质中聚集含有结晶聚酯树脂的颗粒,含有非结晶性聚酯树脂的颗粒和脱模剂颗粒,以形成凝集颗粒; 并且将聚集的颗粒加热熔化成聚结体,其中通过在不高于150℃的温度下聚合得到结晶聚酯树脂和非结晶聚酯树脂中的至少一种,其中含有硫原子的布朗斯台德酸作为 催化剂,并且其中通过差示扫描量热计测量的调色剂的第一起始温度A(℃)和非结晶聚酯树脂的玻璃化转变温度B(℃)满足关系式(BA) 10,其中结晶性聚酯树脂的重均分子量为非结晶性聚酯树脂的重均分子量的1/2以下。

    Process for producing resin particle liquid dispersion for electrostatic image developing toner, electrostatic image developing toner and production process thereof
    17.
    发明申请
    Process for producing resin particle liquid dispersion for electrostatic image developing toner, electrostatic image developing toner and production process thereof 有权
    静电图像显影用调色剂用树脂粒子分散液,静电图像显影用调色剂及其制造方法

    公开(公告)号:US20060263709A1

    公开(公告)日:2006-11-23

    申请号:US11230529

    申请日:2005-09-21

    IPC分类号: G03G9/08 G03G9/00

    摘要: A process for producing a resin particle liquid dispersion for an electrostatic image developing toner, the process comprising: polycondensing a polycondensable monomer by utilizing an acid having a surface activating effect as a polycondensation catalyst, so as to obtain a polycondensed resin; and dispersing the polycondensed resin in an aqueous medium to which a base is added, so as to obtain a resin particle liquid dispersion in which a median diameter of resin particles is from 0.05 to 2.0 μm, or the process comprising: polycondensing a polycondensable monomer by utilizing an acid having a surface activating effect as a polycondensation catalyst in a co-presence of a polycondensed resin, so as to obtain a polycondensed resin-containing material; and dispersing the polycondensed resin-containing material in an aqueous medium, so as to obtain a resin particle liquid dispersion in which a median diameter of resin particles is from 0.05 to 2.0 μm.

    摘要翻译: 一种用于静电图像显影调色剂的树脂颗粒分散液的制备方法,该方法包括:通过利用具有表面活化作用的酸缩聚缩聚单体作为缩聚催化剂,以获得缩聚树脂; 并将缩聚树脂分散在添加有碱的水性介质中,得到树脂粒子的中值粒径为0.05〜2.0μm的树脂粒子分散液,或者将缩聚单体缩聚为 在缩聚树脂的共存下,利用具有表面活化作用的酸作为缩聚催化剂,得到含缩聚树脂的材料; 并将含缩聚树脂的材料分散在水性介质中,得到树脂粒子的中值粒径为0.05〜2.0μm的树脂粒子分散液。

    Method for producing binder resin, particulate resin dispersion and method for producing same, electrostatic image development toner and method for producing same, electrostatic image developer, and image forming method
    19.
    发明授权
    Method for producing binder resin, particulate resin dispersion and method for producing same, electrostatic image development toner and method for producing same, electrostatic image developer, and image forming method 有权
    粘结剂树脂的制造方法,粒状树脂分散体及其制造方法,静电图像显影用调色剂及其制造方法,静电图像显影剂及成像方法

    公开(公告)号:US08637632B2

    公开(公告)日:2014-01-28

    申请号:US11444421

    申请日:2006-06-01

    IPC分类号: C08G63/82 C08G63/87

    摘要: A method for producing a binder resin comprises polycondensing a polycondensable monomer by using a polycondensation catalyst that comprises: at least one of compounds of formula (I) or (II); and at least one of compounds represented of formula (III) or (IV), wherein weight ratio of total amount of the compounds of formula (I) or (II) to total amount of the compounds of formula (III) or (IV) is from 5:95 to 95:5: wherein R1 represents a C8-C20 straight-chain alkyl group; R2 represents a monovalent organic group; and number n of substituents R2 represents an integer of from 0 to 4; R3—SO3H  (II) wherein R3 represents a C8-C20 straight-chain alkyl group; wherein R4 represents a C8-C20 branched alkyl group; R5 represents a monovalent organic group; and number m of substituents R5 represents an integer of from 0 to 4; and R6—SO3H  (IV) wherein R6 represents a C8-C20 branched alkyl group.

    摘要翻译: 粘合剂树脂的制造方法包括使用缩聚催化剂缩聚缩聚单体,所述缩聚催化剂包含:式(I)或(II)的化合物中的至少一种; 和式(III)或(IV)化合物中的至少一种化合物,其中式(I)或(II)化合物与式(III)或(IV)化合物的总量的总量的重量比 为5:95〜95:5,其中R1表示C8-C20直链烷基; R2表示一价有机基团; 取代基R2的数量n表示0〜4的整数, R3-SO3H(Ⅱ)其中R3代表C8-C20直链烷基; 其中R4代表C8-C20支链烷基; R5代表一价有机基团; 取代基R 5的数m表示0〜4的整数, 和R6-SO3H(IV),其中R6表示C8-C20支链烷基。

    Resin particle dispersion liquid, and method for producing the same
    20.
    发明授权
    Resin particle dispersion liquid, and method for producing the same 有权
    树脂粒子分散液及其制造方法

    公开(公告)号:US07776994B2

    公开(公告)日:2010-08-17

    申请号:US11730147

    申请日:2007-03-29

    IPC分类号: C08G63/02

    摘要: A resin particle dispersion liquid comprises: resin particles comprising polyester having terminal carboxyl groups, the polyester being obtained by polycondensation of a polycondensable monomer, wherein the polyester has the terminal carboxyl groups that are partially neutralized to form carboxyl anions, the resin particles in the resin particle dispersion liquid having a value of (da/(da+dc)) of from approximately 0.30 to approximately 0.90, when in an absorption spectrum of the resin particles measured with an infrared spectrometer, dc represents a peak intensity of the terminal carboxyl group in a range of from 1,780 to 1,680 cm−1, and da represents a peak intensity of the neutralized carboxyl anion in a range of from 1,670 to 1,550 cm−1, the polyester has an acid value of approximately 1 mg·KOH/g or more and less than approximately 15 mg·KOH/g before neutralization, the resin particles dispersion liquid comprises a divalent or higher organic acid in an amount of from approximately 0.1 to approximately 20 parts by weight per 100 parts by weight of the resin particles, and the resin particles have a median diameter of from approximately 0.1 to approximately 2.0 μm.

    摘要翻译: 树脂颗粒分散液包括:包含具有末端羧基的聚酯的树脂颗粒,所述聚酯通过缩聚单体的缩聚获得,其中所述聚酯具有部分中和以形成羧基阴离子的末端羧基,树脂中的树脂颗粒 具有大约0.30至大约0.90的值(da /(da + dc))的颗粒分散液,当在用红外光谱仪测量的树脂颗粒的吸收光谱中,dc表示末端羧基的峰强度 从1,780至1,680cm -1的范围,da表示中和的羧基阴离子在1,670至1,550cm -1范围内的峰强度,该聚酯具有约1mg·KOH / g以上的酸值 并且在中和之前小于约15mg·KOH / g,所述树脂颗粒分散液包含二价或更高有机酸,其量约为 相对于100重量份的树脂粒子为0.1〜约20重量份,树脂粒子的中值粒径为约0.1〜约2.0μm。