POLYMER PROPPANT MATERIAL AND METHOD FOR PRODUCING SAME
    22.
    发明申请
    POLYMER PROPPANT MATERIAL AND METHOD FOR PRODUCING SAME 审中-公开
    聚合物专用材料及其制造方法

    公开(公告)号:US20160075938A1

    公开(公告)日:2016-03-17

    申请号:US14786598

    申请日:2014-05-13

    CPC classification number: C09K8/80 C08F232/08 C08G61/08 C08G2261/418

    Abstract: A polymer material for proppant in the form of a metathesis-radically cross-linked mixture of oligocyclopentadienes and methylcarboxy norbornene esters is obtained by mixing dicyclopentadiene with methacrylic esters and polymer stabilizers, heating the mixture to a temperature of 150-220° C., holding at said temperature for 15-360 minutes, and then cooling down to 20-50° C. A radical initiator and a catalyst are added successively to the resultant mixture of oligocyclopentadienes and methylcarboxy norbornene esters. The polymer matrix is heated to a temperature of 50-340° C., is held at this temperature for 1-360 minutes and then is cooled to room temperature. A technical result achieved by implementation of the present invention is an increase in thermal strength of the proppant material, providing a compressive strength of at least 150 MPa at a temperature of not less than 100° C.

    Abstract translation: 通过将二环戊二烯与甲基丙烯酸酯和聚合物稳定剂混合,将该混合物混合至150-220℃的温度,通过将该混合物加热至150-220℃的温度,得到支链剂聚合物材料,该聚合物材料为易位 - 自由基交联的低聚环戊二烯和甲基碳代降冰片烯酯的混合物 在所述温度下15-360分钟,然后冷却至20-50℃。自由基引发剂和催化剂依次加入到所得的低聚环戊二烯和甲基碳代降冰片烯酯的混合物中。 将聚合物基体加热到50-340℃的温度,在该温度下保持1-360分钟,然后冷却至室温。 通过实施本发明而获得的技术结果是支撑剂材料的热强度增加,在不低于100℃的温度下提供至少150MPa的抗压强度。

Patent Agency Ranking