Endless metal belt with strengthened edges
    42.
    发明授权
    Endless metal belt with strengthened edges 失效
    无边金属带加强边缘

    公开(公告)号:US5127885A

    公开(公告)日:1992-07-07

    申请号:US633027

    申请日:1990-12-24

    IPC分类号: C21D1/34 C21D9/52 F16G1/20

    摘要: Ductility of belt material is increased at least at one edge of an endless metal belt, thus reducing the likelihood of premature failure of the belt. The inner region of the belt maintains the inherent strength of the metal. The endless metal belt so formed is particularly useful as a driving member for a continuously-variable transmission.

    摘要翻译: 至少在环形金属带的一个边缘处,带材的延展性增加,从而减少了带子过早失效的可能性。 皮带的内部区域保持金属的固有强度。 这样形成的无端金属带作为无级变速器的驱动部件是特别有用的。

    Fuse holder
    43.
    发明授权
    Fuse holder 失效
    保险丝座

    公开(公告)号:US4968269A

    公开(公告)日:1990-11-06

    申请号:US173410

    申请日:1988-03-25

    IPC分类号: H01H85/54

    CPC分类号: H01H85/542

    摘要: The fuse holder for receiving a cylindrical fuse having conductive ends includes a cap having a fuse carrier disposed in part therein for receiving one end of the fuse and a barrel having a fuse cavity for receiving the cap and fuse. The barrel includes a bottom terminal extending through the barrel for contact with one conductive end of the fuse and a side terminal having tines extending through apertures in the side of the barrel for engagement with the fuse carrier which in turn is in electrical contact with the other end of the fuse. The body of the side terminal is disposed on the exterior of the barrel and, in conjunction with the wall of the barrel, isolates the interior of the barrel from the body of the side terminal such that only that portion of the side terminal required to complete the electrical path from the fuse carrier to the side terminal is exposed interior the barrel.

    摘要翻译: 用于接收具有导电端的圆柱形熔断器的熔断器保持器包括具有设置在其中的用于容纳熔断器的一端的熔丝托架的盖,以及具有用于接收盖和熔丝的保险丝腔的筒体。 枪管包括延伸穿过枪管的底部端子,用于与保险丝的一个导电端接触,侧面端子具有延伸穿过枪管侧面的孔的尖端,用于与保险丝支架接合,而保险丝支架又与另一个电气接触 保险丝的末端 侧端子的主体设置在筒的外部,并且与筒的壁结合,将筒的内部与侧端子的主体隔离,使得仅需要完成的侧端的那部分 从保险丝托架到侧端子的电气路径暴露在枪管内部。

    Electroforming process
    44.
    发明授权
    Electroforming process 失效
    电铸工艺

    公开(公告)号:US4501646A

    公开(公告)日:1985-02-26

    申请号:US624164

    申请日:1984-06-25

    CPC分类号: C25D1/00 C25D1/02 Y10S204/13

    摘要: An electroforming process comprising providing a core mandrel having an electrically conductive, adhesive outer surface, a coefficient of expansion of at least about 8.times.10.sup.-5 in./in./.degree.F., a segmental cross-sectional area of less than about 1.8 square inches and an overall length to segmental cross-sectional area ratio greater than about 0.6, establishing an electroforming zone between an anode selected from a metal and alloys thereof having a coefficient of expansion of between about 6.times.10.sup.-6 in./in./.degree.F. and about 10.times.10.sup.-6 in./in./.degree.F. and a cathode comprising the core mandrel, the cathode and the anode being separated by a bath comprising a salt solution of the metal or alloys thereof, heating the bath and the cathode to a temperature sufficient to expand the cross-sectional area of the mandrel, applying a ramp current across the cathode and the anode to electroform a coating of the metal on the core mandrel, the coating having a thickness at least about 30 Angstroms and stress-strain hysteresis of at least about 0.00015 in./in., rapidly applying a cooling fluid to the exposed surface of the coating to cool the coating prior to any significant cooling and contracting of the core mandrel whereby a stress of between about 40,000 p.s.i. and about 80,000 p.s.i. are imparted to the cooled coating to permanently deform the coating and to render the length of the inner perimeter of the coating incapable of contracting to less than 0.04 percent greater than the length of the outer perimeter of the core mandrel after the core mandrel is cooled and contracted, cooling and contracting the core mandrel, and removing the coating from the core mandrel.

    摘要翻译: 一种电铸工艺,包括提供具有导电粘合剂外表面的芯心轴,至少约8×10 -5英寸/英寸/°F的膨胀系数,小于约1.8平方的节段横截面积 英寸,并且总截面积横截面积比大于约0.6的整个长度,在选自金属的阳极和其合金之间建立一个电铸区,膨胀系数为约6×10 -6英寸/英寸/°F 和约10×10 -6 in./in./°F,并且包括芯心轴的阴极,阴极和阳极由包含金属或其合金的盐溶液的浴分开,加热浴和阴极 达到足以扩大心轴的横截面面积的温度,在阴极和阳极上施加斜坡电流以电铸模芯上的金属涂层,该涂层具有至少约30埃的厚度和应力 - 在至少约0.00015英寸/英寸的应变滞后之前,快速地将冷却流体施加到涂层的暴露表面,以在芯棒的任何显着冷却和收缩之前冷却涂层,由此应力在约40,000p.s.i. 约80,000 p.s.i。 被赋予冷却的涂层以使涂层永久变形,并且使得在芯心轴被冷却之后,涂层的内周边长度不能超过芯心的外周长度的小于0.04%,并且 收缩,冷却和收缩芯轴,以及从芯心轴上去除涂层。

    Surface treatment method without external power source
    47.
    发明授权
    Surface treatment method without external power source 失效
    无外部电源的表面处理方法

    公开(公告)号:US6048657A

    公开(公告)日:2000-04-11

    申请号:US238286

    申请日:1999-01-28

    IPC分类号: G03G5/047 G03G5/10

    CPC分类号: G03G5/102 G03G5/047

    摘要: There is disclosed a process for forming a photosensitive imaging member including positioning a substrate and an electrode in an electrolytic solution to form a galvanic cell and electrochemically graining the substrate surface in the absence of an external power source to provide a substrate surface roughness sufficient to substantially suppress the formation of a pattern of light and dark interference fringes upon exposure of the photosensitive imaging member to a light source.

    摘要翻译: 公开了一种用于形成感光成像构件的方法,包括将基底和电极定位在电解溶液中以形成原电池,并且在不存在外部电源的情况下对基底表面进行电化学研磨以提供足以基本上 抑制在将光敏成像构件暴露于光源时形成光和黑色干涉条纹的图案。