    发明授权
    Thermally stable oleophobic low adhesion coating for inkjet printhead face 有权
    用于喷墨打印头表面的热稳定的疏油性低粘附性涂层

    公开(公告)号:US08969487B2

    公开(公告)日:2015-03-03

    申请号:US13557466

    申请日:2012-07-25

    IPC分类号: C08L77/00 C08L79/08

    CPC分类号: B41J2/1606 B41J2/164

    摘要: A coating for an ink jet printhead front face, wherein the coating comprises an oleophobic low adhesion coating having high thermal stability as indicated by less than about 15 percent weight loss when heated to up to 300° C., and wherein a drop of ultra-violet (UV) gel ink or a drop of solid ink exhibits a contact angle of greater than about 45° and sliding angle of less than about 30° with a surface of the coating, wherein the coating maintains the contact angle and sliding angle after the coating has been exposed to a temperature of at least 200° C. for at least 30 minutes. In particular, the coating shows no oil on the coating surface after curing.

    摘要翻译: 一种用于喷墨打印头前面的涂层,其中所述涂层包含具有高热稳定性的疏油性低粘合性涂层,当加热至高达300℃时,其重量损失小于约15重量%,并且其中, 紫外线(UV)凝胶油墨或一滴固体油墨与涂层的表面呈现大于约45°的接触角和小于约30°的滑动角度,其中涂层保持接触角和滑动角度 已经将涂层暴露于至少200℃的温度至少30分钟。 特别地,涂层在固化后在涂层表面上不显示油。