Vanadium phosphorus oxide catalyst having a thermally conductive support
    1.
    发明授权
    Vanadium phosphorus oxide catalyst having a thermally conductive support 失效
    具有导热性载体的氧化钒催化剂

    公开(公告)号:US06660681B1

    公开(公告)日:2003-12-09

    申请号:US09958584

    申请日:2001-10-09

    IPC分类号: B01J27198

    摘要: A catalyst comprising vanadium phosphorus oxide combined with a thermally conductive material is particularly useful for the selective hydrocarbon oxidations (e.g., butane to maleic anhydride) and can be prepared by forming a suspension comprising a vanadium (IV) phosphate compound in a liquid medium (via hydrochloric acid digestion of V2O5 and H3PO4 in an aqueous solvent or via heating vanadium pentoxide with at least one substantially anhydrous unsubstituted alcohol having 1-10 carbon atoms, 1-3 hydroxyl groups free from olefinic double bonds to form a feed of vanadium pentoxide reduced to a valence between 4 and 4.6, and then contacting the feed with a solution of orthophosphoric acid and at least one unsubstituted alcohol), adding a thermally conductive material to the suspension under agitation at moderated temperature between 40° C. and 120° C., followed by drying, optionally but preferably washing and calcining (either in situ or ex situ) the material thus formed.

    摘要翻译: 包含与导热材料结合的钒磷氧化物的催化剂对于选择性烃氧化(例如,丁烷至马来酸酐)特别有用,并且可以通过在液体介质中形成包含磷酸钒(IV)化合物的悬浮液(通过 在水溶剂中盐酸消化V2O5和H3PO4,或通过加热五氧化二钒与至少一种具有1-10个碳原子的基本上无水的未取代的醇,1-3个不含烯属双键的羟基,形成还原成五氧化二钒的进料 价格在4和4.6之间,然后使进料与正磷酸和至少一种未取代的醇的溶液接触),在40℃至120℃的温和温度下在搅拌下向悬浮液中加入导热材料, 随后干燥,任选地,但优选洗涤和煅烧(原位或非原位)所形成的材料。