公开(公告)号:US4116882A
公开(公告)日:1978-09-26
申请号:US860369
申请日:1977-12-14
CPC分类号: C01F7/46 , B01J21/04 , B01J21/14 , B01J35/08 , B01J37/00 , C01F7/36 , C01P2004/32 , C01P2006/14 , C01P2006/16 , Y10S502/503
摘要: Alumina spheres are formed by peptizing alumina slurries, centrifugates, and filtercakes, aging and dropping the peptized material through a hydrocarbon filled column. The improved method avoids the drying and reslurrying of alumina powders currently used and provides a method whereby harmful ions such as chloride and sulfates can be excluded from the alumina.
摘要翻译: 通过将氧化铝浆料,离心液和滤饼胶化,通过填充烃的柱来老化和滴加胶溶材料来形成氧化铝球体。 改进的方法避免了目前使用的氧化铝粉末的干燥和再浆化,并且提供了可以从氧化铝中排除有害离子如氯化物和硫酸盐的方法。