MELT ADHESIVE BASED ON METALLOCENE CATALYZED OLEFIN-A-OLEFIN COPOLYMERS
    1.
    发明申请
    MELT ADHESIVE BASED ON METALLOCENE CATALYZED OLEFIN-A-OLEFIN COPOLYMERS 有权
    基于金属催化的烯烃-α-烯烃共聚物的熔融粘合剂

    公开(公告)号:US20110213067A1

    公开(公告)日:2011-09-01

    申请号:US13040405

    申请日:2011-03-04

    CPC classification number: C09J123/0815 C08L2314/06 C08L2666/02 C09J153/00

    Abstract: Melt adhesive containing 5 to 40 wt.-% of at least one ethylene-based copolymer and at least one C3 to C20 -α-olefin obtained through metallocene-catalyzed polymerization, 10 to 65 wt.-% of at least one tackifying resin, 0 to 35 wt.-% of a plasticizer, 0.01 to 30 wt.-% additives and additional ingredients selected from stabilizers, adhesion promoters, fillers or pigments, waxes and/or other polymers, wherein the total should amount to 100%, characterized in that copolymer A is a block copolymer that exhibits a substantially even elastic behavior in the range of 0° C. to 25° C., measured as the ratio of the storage modulus E′ according to (E′0C−E′25C)/E′25C

    Abstract translation: 含有5〜40重量%的至少一种乙烯类共聚物和至少一种通过金属茂催化聚合得到的C3〜C20-α-烯烃的熔融粘合剂,10〜65重量%的至少一种增粘树脂, 0至35重量%的增塑剂,0.01至30重量%的添加剂和选自稳定剂,粘合促进剂,填料或颜料,蜡和/或其它聚合物的其它成分,其中总量应为100% 在该共聚物A中,嵌段共聚物在0℃〜25℃的范围内显示出基本上均匀的弹性,根据(E'C-E'25℃)的储能模量E' /E'25C<1.5。

    Method for Performing a Phase Conversion
    3.
    发明申请
    Method for Performing a Phase Conversion 审中-公开
    执行相位转换的方法

    公开(公告)号:US20120199577A1

    公开(公告)日:2012-08-09

    申请号:US13451955

    申请日:2012-04-20

    Abstract: A method for performing a phase transition, in particular a melting process, by heating a carrier medium containing or constituting a phase change material in a reactor, the carrier medium being brought into contact with a solid heating medium that can be heated by electromagnetic induction and that is contained in the reactor and is surrounded by the carrier medium, and heating the heating medium by electromagnetic induction by means of an inductor, the phase change material undergoing a phase transition and the carrier medium being separated from the heating medium after the phase transition. This preferably takes place in a continuous-flow reactor. The inductor preferably generates an alternating field having a frequency in the range from 1 to 100 kHz.

    Abstract translation: 通过在反应器中加热含有或构成相变材料的载体介质进行相变,特别是熔融过程的方法,使载体介质与可通过电磁感应加热的固体加热介质接触, 其被包含在反应器中并被载体介质包围,并且通过电感器的电磁感应来加热加热介质,所述相变材料经历相变,并且载体介质在相变之后与加热介质分离 。 这优选在连续流动反应器中进行。 电感器优选地产生频率在1至100kHz范围内的交变场。

    SOFT CROSSLINKABLE POLYURETHANE MATERIALS
    4.
    发明申请
    SOFT CROSSLINKABLE POLYURETHANE MATERIALS 审中-公开
    软交联聚氨酯材料

    公开(公告)号:US20090039551A1

    公开(公告)日:2009-02-12

    申请号:US12186612

    申请日:2008-08-06

    Abstract: The invention relates to crosslinking compositions for polyurethane elastomers, made up of a polyol component containing: 30 to 80 wt % polyether diols and/or polyester diols; 10 to 40 wt % polyols comprising at least three OH groups; and to 50 wt % of a monofunctional compound that comprises an isocyanate-reactive group, and an isocyanate component containing an at least trifunctional isocyanate, such that the NCO/OH ratio is intended to be between 0.9 to 1.2. Use of the corresponding crosslinked polyurethane elastomers as molded elements is also described.

    Abstract translation: 本发明涉及用于聚氨酯弹性体的交联组合物,其由多元醇组分组成,所述多元醇组分含有:30至80重量%的聚醚二醇和/或聚酯二醇; 10至40重量%的包含至少三个OH基团的多元醇; 和50重量%的包含异氰酸酯反应性基团的单官能化合物和含有至少三官能异氰酸酯的异氰酸酯组分,使得NCO / OH比旨在在0.9至1.2之间。 还描述了使用相应的交联聚氨酯弹性体作为模制元件。

    Melt adhesive based on metallocene catalyzed olefin-α-olefin copolymers
    6.
    发明授权
    Melt adhesive based on metallocene catalyzed olefin-α-olefin copolymers 有权
    基于金属茂催化的烯烃-α-烯烃共聚物的熔融粘合剂

    公开(公告)号:US08163833B2

    公开(公告)日:2012-04-24

    申请号:US13040405

    申请日:2011-03-04

    CPC classification number: C09J123/0815 C08L2314/06 C08L2666/02 C09J153/00

    Abstract: Melt adhesive containing 5 to 40 wt.-% of at least one ethylene-based copolymer and at least one C3 to C20-α-olefin obtained through metallocene-catalyzed polymerization, 10 to 65 wt.-% of at least one tackifying resin, 0 to 35 wt.-% of a plasticizer, 0.01 to 30 wt.-% additives and additional ingredients selected from stabilizers, adhesion promoters, fillers or pigments, waxes and/or other polymers, wherein the total should amount to 100%, characterized in that copolymer A is a block copolymer that exhibits a substantially even elastic behavior in the range of 0° C. to 25° C., measured as the ratio of the storage modulus E′ according to (E′0C−E′25C)/E′25C

    Abstract translation: 含有5〜40重量%的至少一种乙烯类共聚物和至少一种通过金属茂催化聚合得到的C3〜C20-α-烯烃的熔融粘合剂,10〜65重量%的至少一种增粘树脂, 0至35重量%的增塑剂,0.01至30重量%的添加剂和选自稳定剂,粘合促进剂,填料或颜料,蜡和/或其它聚合物的其它成分,其中总量应为100% 在该共聚物A中,嵌段共聚物在0℃〜25℃的范围内显示出基本上均匀的弹性,根据(E'C-E'25℃)的储能模量E' /E'25C<1.5。