摘要:
Thermoplastic molding materials containA) from 40 to 99.69% by weight of a polyoxymethylene homo- or copolymer,B) from 0.1 to 2% by weight of at least one stabilizer selected from the group consisting of benzotriazole derivatives or benzophenone derivatives or aromatic benzoate derivatives,C) from 0.1 to 2% by weight of at least one sterically hindered amino compound,D) from 0.005 to 2% by weight of a polyamide,E) from 0 to 2% by weight of an epoxy-containing compound,F) from 0 to 50% by weight of a toughened polymer andG) from 0 to 50% by weight of a fibrous or particulate filler or of a mixture thereof.
摘要:
A flameproofed black thermoplastic molding material containingA) from 5 to 98.9% by weight of a thermoplastic polyamide,B) from 1 to 20% by weight of red phosphorusC) from 0.1 to 5% by weight of a colorant complementary with red phosphorus to produce blackened polyamide,D) from 0 to 30% by weight of an elastomeric polymer,E) from 0 to 50% by weight of a fibrous or particulate filler or of a mixture thereof,F) from 0 to 70% by weight of a polyphenylene ether andG) from 0 to 30% by weight of conventional additives and processing assistants,the percentages by weight of components A to G being 100% in each case.
摘要:
Polyoxymethylene molding materials having improved heat stability and consisting of(A) one or more polyoxymethylene homopolymers and/or copolymers and(B) one or more antioxidants having a sterically hindered phenolic structure,(C) with or without additives, contain(D) as an additive, one or more alkaline earth metal silicates and/or alkaline earth metal glycerophosphates, advantageously in an amount of from 0.002 to 2.0% by weight, based on the weight of component (A),for improving the heat stability, reducing the tendency to discoloration and minimizing the free formaldehyde content.To prepare the novel polyoxymethylene molding materials, the components are advantageously melted in an extruder at from 150.degree. to 260.degree. C.The polyoxymethylene molding materials are useful for the production of films or, preferably, moldings, which are used, for example, in the automotive, electrical appliances and electronics industries.
摘要:
Molding materials of(A) one or more polyoxymethylene homopolymers and/or copolymers and(B) one or more thermoplastic polyurethane elastomers,(C) with or without additives, contain, as an additive,(D) one or more alkaline earth metal silicates, advantageously in an amount of from 0.005 to 2% by weight, based on the weight of the components (A) and (B), for improving the heat stability, reducing the tendency to discoloration and minimizing the free formaldehyde content.To prepare the molding materials, the components (A), (B), (D) and, if required (C) are advantageously melted together in an extruder at from 150.degree. to 260.degree. C.The molding materials are useful for the production of films or moldings, which are used, for example, in the automotive, electrical appliances and electronics industries.
摘要:
Styrene copolymer compositions, especially ASA compositions, exhibit improved weatherability and color retention performance when processed according to the invention. Disclosed herein is a method of improving the weatherability and color retention performance of styrene copolymer compositions and exterior siding incorporating such styrene copolymer compositions. More specifically, a method is disclosed comprising improving the weatherability and color retention of styrene copolymer compositions, especially ASA compositions, which is advantageous with respect to cost and ease of manufacturing. Composite articles are also disclosed incorporating the foregoing improved styrene copolymer compositions as an exterior layer.
摘要:
Reinforced polyoxymethylene materials containing(A) one or more polyoxymethylene homopolymers and/or copolymers and(B) wollastonite, advantageously in a weight ratio of components (A) to (B) of from 95:50 to5:50, with or without(C) additives in effective amounts, the wollastonite crystals (B) have a mean thickness equal to or smaller than 5 .mu.m and a mean length/thickness ratio equal to or greater than 5. The molding materials are prepared by introducing the wollastonite crystals (B) into the melt of component (A) at from 180.degree. to 260.degree. C., advantageously by means of an extruder.
摘要:
Impact-resistant polyoxymethylene molding materials containing(A) from 30 to 95% by weight of one or more polyoxymethylenes and(B) from 5 to 70% by weight of one or more elastomeric graft polymers which are prepared by emulsion polymerization, are dispersed in component A, have a mean particle diameter of from 0.08 to 2 .mu.m and are composed of1. from 60 to 90% by weight of a grafting base of crosslinked polybutadiene in which not more than 30% by weight of the butadiene may be replaced with isoprene, 2,3-dimethylbutadiene, styrene, p-methylstyrene, .alpha.-methylstyrene and/or (meth)acrylonitrile, and2. from 10 to 40% by weight of one or more grafted shells consisting of polymers of styrene and/or methyl methacrylate, in which not more than 15% by weight of the said monomers 2 may be replaced with acrylonitrile or a C.sub.1 -C.sub.8 -alkyl acrylate,the percentages A and B and the percentages 1 and 2 summing to 100, with or without(C) effective amounts of assistants,and a process for their preparation.