公开(公告)号:US20060285990A1
公开(公告)日:2006-12-21
申请号:US11510238
申请日:2006-08-25
Applicant: Pascal Jehanno , Martin Heilmaier , Heinrich Kestler
Inventor: Pascal Jehanno , Martin Heilmaier , Heinrich Kestler
IPC: B22F3/12
CPC classification number: C22C1/045 , B22F3/156 , B22F3/162 , B22F2003/248 , B22F2009/041 , B22F2998/00 , B22F2998/10 , B22F2999/00 , C22C27/04 , C22F1/18 , B22F3/1208 , B22F3/15 , B22F3/20 , B22F9/04 , B22F3/14 , B22F3/16 , B22F3/24 , B22F2009/042 , B22F2201/013
Abstract: Semi-finished or finished parts are made from a molybdenum alloy with intermetallic phases, preferably molybdenum-silicide, molybdenum-boron-silicide, optionally also molybdenum-boride phases. Starting from mechanically alloyed powder, hot compacted material exhibits superplastic forming behavior. It is thus possible to lower the forming temperature by at least 300° C., thus permitting processing on conventional plants.
Abstract translation: 半成品或成品部分由具有金属间相的钼合金制成,优选硅化钼,钼 - 硼硅化物,任选地还包括硼化钼相。 从机械合金粉末开始,热压成型材料具有超塑性成形特性。 因此,可以将成形温度降低至少300℃,从而允许对常规设备进行加工。
-
公开(公告)号:US07767138B2
公开(公告)日:2010-08-03
申请号:US11510238
申请日:2006-08-25
Applicant: Pascal Jehanno , Martin Heilmaier , Heinrich Kestler
Inventor: Pascal Jehanno , Martin Heilmaier , Heinrich Kestler
IPC: B22F3/24
CPC classification number: C22C1/045 , B22F3/156 , B22F3/162 , B22F2003/248 , B22F2009/041 , B22F2998/00 , B22F2998/10 , B22F2999/00 , C22C27/04 , C22F1/18 , B22F3/1208 , B22F3/15 , B22F3/20 , B22F9/04 , B22F3/14 , B22F3/16 , B22F3/24 , B22F2009/042 , B22F2201/013
Abstract: Semi-finished or finished parts are made from a molybdenum alloy with intermetallic phases, preferably molybdenum-silicide, molybdenum-boron-silicide, optionally also molybdenum-boride phases. Starting from mechanically alloyed powder, hot compacted material exhibits superplastic forming behavior. It is thus possible to lower the forming temperature by at least 300° C., thus permitting processing on conventional plants.
Abstract translation: 半成品或成品部分由具有金属间相的钼合金制成,优选硅化钼,钼 - 硼硅化物,任选地还包括硼化钼相。 从机械合金粉末开始,热压成型材料具有超塑性成形特性。 因此,可以将成形温度降低至少300℃,从而允许对常规设备进行加工。
-
公开(公告)号:US20060169369A1
公开(公告)日:2006-08-03
申请号:US11384631
申请日:2006-03-20
Applicant: Pascal Jehanno
Inventor: Pascal Jehanno
IPC: C22C27/04
CPC classification number: C22C27/04 , B22F2998/10 , B22F2999/00 , C22C29/18 , C22C37/04 , B22F9/04 , B22F3/14 , C22C1/1084
Abstract: A Mo—Si—B alloy has a matrix of Mo or a Mo solid solution, wherein 25% by volume to 90% by volume of molybdenum silicide and molybdenum boron silicide, optionally together with molybdenum boride, are incorporated. The alloy also contains 0.1-5% by volume of one or more oxides or mixed oxides with a vapor pressure at 1500° C. of
Abstract translation: Mo-Si-B合金具有Mo或Mo固溶体的基体,其中加入25体积%至90体积%的硅化钼和硼硅化钼,任选与硼化钼一起加入。 该合金还含有0.1-5体积%的一种或多种氧化物或混合氧化物,其蒸气压在1500℃,细分散形式为<5×10 -2 -2巴。 氧化物添加不仅提高了热强度,而且大大提高了延展性。
-
公开(公告)号:US07806995B2
公开(公告)日:2010-10-05
申请号:US11384631
申请日:2006-03-20
Applicant: Pascal Jehanno
Inventor: Pascal Jehanno
IPC: C22C27/04
CPC classification number: C22C27/04 , B22F2998/10 , B22F2999/00 , C22C29/18 , C22C37/04 , B22F9/04 , B22F3/14 , C22C1/1084
Abstract: A Mo—Si—B alloy has a matrix of Mo or a Mo solid solution, wherein 25% by volume to 90% by volume of molybdenum silicide and molybdenum boron silicide, optionally together with molybdenum boride, are incorporated. The alloy also contains 0.1-5% by volume of one or more oxides or mixed oxides with a vapor pressure at 1500° C. of
Abstract translation: Mo-Si-B合金具有Mo或Mo固溶体的基体,其中加入25体积%至90体积%的硅化钼和硼硅化钼,任选与硼化钼一起加入。 该合金还含有0.1-5体积%的一种或多种氧化物或混合氧化物,其蒸气压在1500℃,细分散形式为<5×10-2巴。 氧化物添加不仅提高了热强度,而且大大提高了延展性。
-
-
-