Low metal loaded, catalyst compositions including acidic mixed metal oxide as support
    1.
    发明授权
    Low metal loaded, catalyst compositions including acidic mixed metal oxide as support 有权
    低金属负载的催化剂组合物,包括作为载体的酸性混合金属氧化物

    公开(公告)号:US08492592B2

    公开(公告)日:2013-07-23

    申请号:US13456444

    申请日:2012-04-26

    摘要: The invention provides a method of transaminating a reactant with a catalyst composition comprising support and catalyst portions. The support includes an acidic mixed metal oxide including a transitional alumina and a second metal oxide. The transitional alumina can comprise delta or theta alumina, in combination with other transitional phases, or an alpha or gamma alumina. The second metal oxide has a weight percentage less than the weight percentage of alumina. The catalyst portion is 25 weight percent or less of the catalyst composition and is composed of nickel and rhenium. The catalyst portion includes nickel in an amount in the range of 2 to 20 weight percent, based upon total catalyst composition weight, and there is no boron in the catalyst portion. The method provides high activity and selectivity for reactant transamination to a desired product while minimizing the formation of unwanted cyclic products.

    摘要翻译: 本发明提供了一种用包含载体和催化剂部分的催化剂组合物将反应物转氨的方法。 载体包括含有过渡氧化铝和第二金属氧化物的酸性混合金属氧化物。 过渡氧化铝可以包含与其它过渡相结合的δ或θ氧化铝,或α或γ氧化铝。 第二金属氧化物的重量百分比小于氧化铝的重量百分数。 催化剂部分为催化剂组合物的25重量%以下,由镍和铼构成。 催化剂部分包括基于总催化剂组合物重量的2-20重量%范围内的量的镍,并且在催化剂部分中不存在硼。 该方法提供了对期望产物的反应物转氨酸的高活性和选择性,同时使不期望的环状产物的形成最小化。

    LOW METAL LOADED, CATALYST COMPOSITIONS INCLUDING ACIDIC MIXED METAL OXIDE AS SUPPORT
    2.
    发明申请
    LOW METAL LOADED, CATALYST COMPOSITIONS INCLUDING ACIDIC MIXED METAL OXIDE AS SUPPORT 有权
    低金属负载,催化剂组合物,包括酸性混合金属氧化物作为支持

    公开(公告)号:US20120238780A1

    公开(公告)日:2012-09-20

    申请号:US13456444

    申请日:2012-04-26

    IPC分类号: C07C209/02

    摘要: The invention provides a method of transaminating a reactant with a catalyst composition comprising support and catalyst portions. The support includes an acidic mixed metal oxide including a transitional alumina and a second metal oxide. The transitional alumina can comprise delta or theta alumina, in combination with other transitional phases, or an alpha or gamma alumina. The second metal oxide has a weight percentage less than the weight percentage of alumina. The catalyst portion is 25 weight percent or less of the catalyst composition and is composed of nickel and rhenium. The catalyst portion includes nickel in an amount in the range of 2 to 20 weight percent, based upon total catalyst composition weight, and there is no boron in the catalyst portion. The method provides high activity and selectivity for reactant transamination to a desired product while minimizing the formation of unwanted cyclic products.

    摘要翻译: 本发明提供了一种用包含载体和催化剂部分的催化剂组合物将反应物转氨的方法。 载体包括含有过渡氧化铝和第二金属氧化物的酸性混合金属氧化物。 过渡氧化铝可以包含与其它过渡相结合的δ或θ氧化铝,或α或γ氧化铝。 第二金属氧化物的重量百分比小于氧化铝的重量百分数。 催化剂部分为催化剂组合物的25重量%以下,由镍和铼构成。 催化剂部分包括基于总催化剂组合物重量的2-20重量%范围内的量的镍,并且在催化剂部分中不存在硼。 该方法提供了对期望产物的反应物转氨酸的高活性和选择性,同时使不期望的环状产物的形成最小化。

    Low metal loaded, catalyst compositions including acidic mixed metal oxide as support
    3.
    发明授权
    Low metal loaded, catalyst compositions including acidic mixed metal oxide as support 有权
    低金属负载,催化剂组合物包括作为载体的酸性混合金属氧化物

    公开(公告)号:US08187997B2

    公开(公告)日:2012-05-29

    申请号:US12587351

    申请日:2009-10-06

    IPC分类号: B01J23/00 B01J21/00 B01J20/00

    摘要: The invention provides a catalyst composition composed of a support portion and a catalyst portion. The support portion includes an acidic mixed metal oxide including a transitional alumina and a second metal oxide. The transitional alumina can comprise delta or theta alumina, in combination with other transitional phases, or an alpha or gamma alumina. The second metal oxide has a weight percentage that is less than the weight percentage of alumina. The catalyst portion is 25 weight percent or less of the catalyst composition and is composed of nickel and rhenium. The catalyst portion includes nickel in an amount in the range of 2 to 20 weight percent, based upon total catalyst composition weight, and there is no boron in the catalyst portion.

    摘要翻译: 本发明提供一种由支撑部分和催化剂部分组成的催化剂组合物。 支撑部分包括包含过渡氧化铝和第二金属氧化物的酸性混合金属氧化物。 过渡氧化铝可以包含与其它过渡相结合的δ或θ氧化铝,或α或γ氧化铝。 第二金属氧化物的重量百分比小于氧化铝的重量百分数。 催化剂部分为催化剂组合物的25重量%以下,由镍和铼构成。 催化剂部分包括基于总催化剂组合物重量的2-20重量%范围内的量的镍,并且在催化剂部分中不存在硼。

    Wood preservative composition
    4.
    发明授权
    Wood preservative composition 有权
    木材防腐剂组成

    公开(公告)号:US07740692B2

    公开(公告)日:2010-06-22

    申请号:US11922173

    申请日:2006-06-07

    摘要: A wood preservative composition resulting from admixing components comprising: at least one preservative metal; a quaternary ammonium compound; at least 2 amine compounds; a pH reducing agent, and water, wherein the pH of the composition is from about 7.1 to less than 8.5. Surprisingly, this combination of materials results in a stable solution that can contain a moldicide yet have a commercially acceptable shelf life.

    摘要翻译: 由混合组分得到的木材防腐剂组合物,包括:至少一种防腐金属; 季铵化合物; 至少2种胺化合物; pH降低剂和水,其中组合物的pH为约7.1至小于8.5。 令人惊讶的是,这种材料的组合产生可以含有杀菌剂但具有商业上可接受的保质期的稳定溶液。