Thermoplastic resin composition and process for preparing the same
    2.
    发明授权
    Thermoplastic resin composition and process for preparing the same 失效
    热塑性树脂组合物及其制备方法

    公开(公告)号:US5496885A

    公开(公告)日:1996-03-05

    申请号:US67816

    申请日:1993-05-27

    摘要: There are disclosed a thermoplastic resin composition which comprises(a) 4 to 95% by weight of a polyphenylene ether,(b) 95 to 4% by weight of a saturated polyester,(c) 0.5 to 40% by weight of an impact modifier and(d) 0.01 to 50% by weight of a compatibilizer and(e) 0.1 to 3 parts by weight of a polycarbonate based on 100 parts by weight of the above (a) to (d) in total; and a process for preparing a thermoplastic resin composition which comprises the steps of melting and kneading(a) 50 to 95% by weight of a polyphenylene ether,(e) 0.1 to 5% by weight of a polycarbonate, and(d) 5 to 50% by weight of a compatibilizer and(c) 0 to 35 parts by weight of an impact modifier based on 100 parts by weight of the above (a), (e) and (d) in total to obtain an intermediate composition (A), and then, melting and kneading 10 to 80% by weight of the intermediate composition (A) and (b) 90 to 20% by weight of a saturated polyester in a kneader equipped with vent ports each having a vacuum device while maintaining each vent port at a reduced pressure of 200 mmHg or less to prepare a thermoplastic resin composition.

    摘要翻译: 公开了一种热塑性树脂组合物,其包含(a)4〜95重量%的聚苯醚,(b)95〜4重量%的饱和聚酯,(c)0.5〜40重量%的抗冲改性剂 和(d)0.01〜50重量%的增容剂和(e)基于100重量份上述(a)〜(d)的总计0.1〜3重量份的聚碳酸酯; 以及制备热塑性树脂组合物的方法,其包括以下步骤:(a)将50至95重量%的聚苯醚,(e)0.1-5重量%的聚碳酸酯,和(d)5至 50重量%的增容剂和(c)0至35重量份的基于100重量份上述(a),(e)和(d)的抗冲改性剂以获得中间体组合物(A ),然后在具有各自具有真空装置的排气口的捏合机中熔融捏合10至80重量%的中间体组合物(A)和(b)90至20重量%的饱和聚酯,同时保持每个 通气口处于200mmHg以下的减压下,制备热塑性树脂组合物。