Hermetically sealed glass package and method of fabrication
    1.
    发明授权
    Hermetically sealed glass package and method of fabrication 有权
    密封玻璃包装及其制造方法

    公开(公告)号:US08148179B2

    公开(公告)日:2012-04-03

    申请号:US12725648

    申请日:2010-03-17

    IPC分类号: H01L21/00

    摘要: A hermetically sealed glass package and method for manufacturing the hermetically sealed glass package are described herein using an OLED display as an example. In one embodiment, the hermetically sealed glass package is manufactured by providing a first substrate plate and a second substrate plate. The second substrate contains at least one transition or rare earth metal such as iron, copper, vanadium, manganese, cobalt, nickel, chromium, neodymium and/or cerium. A sensitive thin-film device that needs protection is deposited onto the first substrate plate. A laser is then used to heat the doped second substrate plate in a manner that causes a portion of it to swell and form a hermetic seal that connects the first substrate plate to the second substrate plate and also protects the thin film device. The second substrate plate is doped with at least one transition metal such that when the laser interacts with it there is an absorption of light from the laser in the second substrate plate, which leads to the formation of the hermetic seal while avoiding thermal damage to the thin-film device. Another embodiment of the hermetically sealed glass package and a method for manufacturing that hermetically sealed glass package are also described herein.

    摘要翻译: 这里使用OLED显示器作为示例来描述气密密封的玻璃封装和制造密封玻璃封装的方法。 在一个实施例中,通过提供第一基板和第二基板制造密封的玻璃封装。 第二基板包含至少一种过渡金属或稀土金属,例如铁,铜,钒,锰,钴,镍,铬,钕和/或铈。 需要保护的敏感薄膜器件沉积到第一衬底板上。 然后使用激光器以使其一部分膨胀并形成将第一衬底板连接到第二衬底板的气密密封件并且还保护薄膜器件的方式来加热掺杂的第二衬底板。 第二衬底板掺杂有至少一种过渡金属,使得当激光与其相互作用时,吸收来自第二衬底板中的激光的光,这导致气密密封的形成,同时避免对 薄膜装置。 本文还描述了密封玻璃封装的另一个实施例以及密封玻璃封装的制造方法。

    HERMETICALLY SEALED GLASS PACKAGE AND METHOD OF FABRICATION
    2.
    发明申请
    HERMETICALLY SEALED GLASS PACKAGE AND METHOD OF FABRICATION 有权
    密封玻璃包装和制造方法

    公开(公告)号:US20100186449A1

    公开(公告)日:2010-07-29

    申请号:US12725648

    申请日:2010-03-17

    IPC分类号: C03B29/00

    摘要: A hermetically sealed glass package and method for manufacturing the hermetically sealed glass package are described herein using an OLED display as an example. In one embodiment, the hermetically sealed glass package is manufactured by providing a first substrate plate and a second substrate plate. The second substrate contains at least one transition or rare earth metal such as iron, copper, vanadium, manganese, cobalt, nickel, chromium, neodymium and/or cerium. A sensitive thin-film device that needs protection is deposited onto the first substrate plate. A laser is then used to heat the doped second substrate plate in a manner that causes a portion of it to swell and form a hermetic seal that connects the first substrate plate to the second substrate plate and also protects the thin film device. The second substrate plate is doped with at least one transition metal such that when the laser interacts with it there is an absorption of light from the laser in the second substrate plate, which leads to the formation of the hermetic seal while avoiding thermal damage to the thin-film device. Another embodiment of the hermetically sealed glass package and a method for manufacturing that hermetically sealed glass package are also described herein.

    摘要翻译: 这里使用OLED显示器作为示例来描述气密密封的玻璃封装和制造密封玻璃封装的方法。 在一个实施例中,通过提供第一基板和第二基板制造密封的玻璃封装。 第二基板包含至少一种过渡金属或稀土金属,例如铁,铜,钒,锰,钴,镍,铬,钕和/或铈。 需要保护的敏感薄膜器件沉积到第一衬底板上。 然后使用激光器以使其一部分膨胀并形成将第一衬底板连接到第二衬底板的气密密封件并且还保护薄膜器件的方式来加热掺杂的第二衬底板。 第二衬底板掺杂有至少一种过渡金属,使得当激光与其相互作用时,吸收来自第二衬底板中的激光的光,这导致气密密封的形成,同时避免对 薄膜装置。 本文还描述了密封玻璃封装的另一个实施例以及密封玻璃封装的制造方法。

    Rare earth-doped, stabilized cadmium halide glasses
    4.
    发明授权
    Rare earth-doped, stabilized cadmium halide glasses 失效
    稀土掺杂,稳定的镉卤化物玻璃

    公开(公告)号:US5346865A

    公开(公告)日:1994-09-13

    申请号:US86048

    申请日:1993-07-06

    摘要: This invention is directed to the production of transparent glasses exhibiting transmission far into the infrared regime of the radiation spectrum. The glasses consist essentially, in mole percent, of 42-55% CdF.sub.2 and/or CdCl.sub.2, 30-40% NaF and/or NaCl, 2-20% total of BaF.sub.2 and/or BaCl.sub.2 +KF and/or KCl, consisting of 0-15% BaF.sub.2 and/or BaCl.sub.2 and 0-7% KF and/or KCl, 1-12% total of at least one stabilizing metal halide selected from the group LiX, BeX.sub.2, MgX.sub.2, MnX.sub.2, PbX.sub.2, TlX, COX.sub.2, and ZnX.sub.2, and 0,005-0.5% REX.sub.3, wherein Re is at least one rare earth metal selected from the lanthanide series of rare earth metals and X is at least one halide selected from the group consisting of fluoride, chloride, and bromide. The preferred glasses contain at least 2% each of BaF.sub.2 and/or BaCl.sub.2 and KF and/or KCl.

    摘要翻译: 本发明涉及透明玻璃的生产,该透明玻璃显示出远离辐射光谱的红外区域的传播。 玻璃基本上以摩尔百分数计含42-55%的CdF2和/或CdCl2,30-40%的NaF和/或NaCl,2-20%的BaF 2和/或BaCl 2 + KF和/或KCl,由 0-15%BaF 2和/或BaCl 2和0-7%KF和/或KCl,1-12%的至少一种选自LiX,BeX2,MgX2,MnX2,PbX2,TlX,COX2, 和ZnX2和0.005-0.5%的REX3,其中Re是选自镧系稀土金属中的至少一种稀土金属,X是选自氟化物,氯化物和溴化物中的至少一种卤化物。 优选的玻璃含有至少2%的BaF 2和/或BaCl 2和KF和/或KCl。

    Alkali metal lanthanum gallate glasses
    6.
    发明授权
    Alkali metal lanthanum gallate glasses 失效
    碱金属镧镓酸盐玻璃

    公开(公告)号:US5232879A

    公开(公告)日:1993-08-03

    申请号:US925105

    申请日:1992-08-06

    IPC分类号: C03C3/12 C03C4/10

    CPC分类号: C03C4/10 C03C3/12 Y10S501/904

    摘要: This invention is directed to glasses exhibiting annealing points above 625.degree. C., strain points above 600.degree. C., linear coefficients of thermal expansion (25.degree.-300.degree. C.) below 90.times.10.sup.-7 /.degree. C., refractive indices below 1.8, and, in thicknesses of 2 mm, infrared transmissions of at least 50% to wavelengths longer than 6 .mu.m, consisting essentially expressed in terms of cation % on the oxide basis, of 5-40% KO.sub.0.5, 4-22% LaO.sub.1.5, 50-76% GaO.sub.1.5, and up to 15% total of at least one additional component in the indicated properties selected from the group consisting of______________________________________ BaO 0-5 NaO.sub.0.5 0-5 CaO 0-5 PbO 0-5 CsO.sub.0.5 0-10 ZnO 0-5 ReO.sub.1.5 0-5 Cl 0-5. ______________________________________

    摘要翻译: 本发明涉及显示退火点高于625℃,应变点高于600℃,线性热膨胀系数(25-300℃)低于90×10 -7 /℃,折射率低于1.8的玻璃 ,并且在厚度为2mm的情况下,基于以氧化物为基准的阳离子%表示的至少50%的长于6μm的波长的红外线透射率为5-40%KO0.5,4-22% LaO 1.5,50-76%GaO 1.5,以及至多一种额定组分的至少15%,所述特性选自-BaO 0-5 NaO0.5-0-5CaO0-5 PbO 0-5 -CsO0.5 0-10 ZnO 0-5 -ReO1.5 0-5 Cl 0-5。 -

    Alkali bismuth gallate glasses
    9.
    发明授权
    Alkali bismuth gallate glasses 失效
    枸橼酸铋玻璃

    公开(公告)号:US5114884A

    公开(公告)日:1992-05-19

    申请号:US691843

    申请日:1991-04-26

    IPC分类号: C03C3/12 C03C3/23 C03C4/10

    摘要: This invention relates to the preparation of thermally stable, chemically durable, heavy metal oxide glasses exhibiting good transmission of infrared radiation to wavelengths of about 7 microns consisting essentially, in weight percent, of 7.5-25% Ga.sub.2 O.sub.3, 70-92% Bi.sub.2 O.sub.3, and 0.25-12% R.sub.2 O, wherein R.sub.2 O consists of at least one alkali metal oxide selected from the group consisting of Na.sub.2 O and K.sub.2 O.