    摘要: For high track density recording, tighter reader and writer track width control are essential. This has been achieved by using a plated NiPd write gap which is self-aligned with a plated 23 KG pole material. Heat dissipation by the writer is thus improved since alumina has been replaced with nonmagnetic metal materials, such as Ru, leading to less pole tip protrusion which in turn leads to better writer track width control

    摘要翻译: 对于高轨道密度记录,更紧密的读写器轨道宽度控制是至关重要的。 这已经通过使用与电镀的23KG极材料自对准的镀NiPd写入间隙来实现。 因此,由于氧化铝被诸如Ru之类的非磁性金属材料所代替,导致作者的散热得到改善,导致较少的极尖突起,这又导致更好的写入器轨道宽度控制

    Pole piece for high track density recording
    2.
    发明申请
    Pole piece for high track density recording 失效
    用于高轨道密度记录的极片

    公开(公告)号:US20050180049A1

    公开(公告)日:2005-08-18

    申请号:US10780514

    申请日:2004-02-17

    IPC分类号: G11B5/147 G11B5/31

    摘要: For high track density recording, tighter reader and writer track width control are essential. This has been achieved by using a plated NiPd write gap which is self-aligned with a plated 23 KG pole material. Heat dissipation by the writer is thus improved since alumina has been replaced with nonmagnetic metal materials, such as Ru, leading to less pole tip protrusion which in turn leads to better writer track width control

    摘要翻译: 对于高轨道密度记录,更紧密的读写器轨道宽度控制是至关重要的。 这已经通过使用与电镀的23KG极材料自对准的镀NiPd写入间隙来实现。 因此,由于氧化铝被诸如Ru之类的非磁性金属材料所代替,导致作者的散热得到改善,导致较少的极尖突起,这又导致更好的写入器轨道宽度控制

    ABS through aggressive stitching
    3.
    发明申请
    ABS through aggressive stitching 失效
    ABS通过积极的拼接

    公开(公告)号:US20070266551A1

    公开(公告)日:2007-11-22

    申请号:US11881316

    申请日:2007-07-26

    IPC分类号: G11B5/127 H04R31/00

    摘要: Aggressive (i.e. tight tolerance) stitching offers several advantages for magnetic write heads but at the cost of some losses during pole trimming. This problem has been overcome by replacing the alumina filler layer, that is used to protect the stitched pole during trimming, with a layer of electroplated material. Because of the superior step coverage associated with the plating method of deposition, pole trimming can then proceed without the introduction of stresses to the stitched pole while it is being trimmed.

    摘要翻译: 积极(即紧公差)缝合为磁性写入头提供了几个优点,但是在极修整期间以一些损失为代价。 通过用一层电镀材料替换用于在修整期间保护缝合极的氧化铝填料层已经克服了这个问题。 由于与沉积电镀方法相关的优越的台阶覆盖,因此可以进行极细修剪,而不会在缝合极被修剪时引入应力。

    ABS through aggressive stitching
    5.
    发明授权
    ABS through aggressive stitching 失效
    ABS通过积极的拼接

    公开(公告)号:US07251102B2

    公开(公告)日:2007-07-31

    申请号:US10782496

    申请日:2004-02-19

    IPC分类号: G11B5/127

    摘要: Aggressive (i.e. tight tolerance) stitching offers several advantages for magnetic write heads but at the cost of some losses during pole trimming. This problem has been overcome by replacing the alumina filler layer, that is used to protect the stitched pole during trimming, with a layer of electro-plated material. Because of the superior step coverage associated with the plating method of deposition, pole trimming can then proceed without the introduction of stresses to the stitched pole while it is being trimmed.

    摘要翻译: 积极(即紧公差)缝合为磁性写入头提供了几个优点,但是在极修整期间以一些损失为代价。 通过用一层电镀材料代替在修整期间用于保护缝合极的氧化铝填料层已经克服了这个问题。 由于与沉积电镀方法相关的优越的台阶覆盖,因此可以进行极细修剪,而不会在缝合极被修剪时引入应力。

    Abs through aggressive stitching
    6.
    发明授权
    Abs through aggressive stitching 失效
    通过积极的缝合

    公开(公告)号:US07751146B2

    公开(公告)日:2010-07-06

    申请号:US11881350

    申请日:2007-07-26

    IPC分类号: G11B5/187 G11B5/127

    摘要: Aggressive (i.e. tight tolerance) stitching offers several advantages for magnetic write heads but at the cost of some losses during pole trimming. This problem has been overcome by replacing the alumina filler layer, that is used to protect the stitched pole during trimming, with a layer of electro-plated material. Because of the superior step coverage associated with the plating method of deposition, pole trimming can then proceed without the introduction of stresses to the stitched pole while it is being trimmed.

    摘要翻译: 积极(即紧公差)缝合为磁性写入头提供了几个优点,但是在极修整期间以一些损失为代价。 通过用一层电镀材料代替在修整期间用于保护缝合极的氧化铝填料层已经克服了这个问题。 由于与沉积电镀方法相关的优越的台阶覆盖,因此可以进行极细修剪,而不会在缝合极被修剪时引入应力。

    Process to form an ABS through aggressive stitching
    7.
    发明授权
    Process to form an ABS through aggressive stitching 失效
    通过积极缝合形成ABS的过程

    公开(公告)号:US07631418B2

    公开(公告)日:2009-12-15

    申请号:US11881316

    申请日:2007-07-26

    IPC分类号: G11B5/187

    摘要: A manufacturing process is provided where aggressive (i.e. tight tolerance) stitching offers several advantages for magnetic write heads but at the cost of some losses during pole trimming. This problem has been overcome by replacing the alumina filler layer, that is used to protect the stitched pole during trimming, with a layer of electroplated material. Because of the superior step coverage associated with the plating method of deposition, pole trimming can then proceed without the introduction of stresses to the stitched pole while it is being trimmed.

    摘要翻译: 提供了一种制造工艺,其中积极(即紧密公差)缝合为磁性写头提供了几个优点,但是在极修整期间以一些损失为代价。 通过用一层电镀材料替换用于在修整期间保护缝合极的氧化铝填料层已经克服了这个问题。 由于与沉积电镀方法相关的优越的台阶覆盖,因此可以进行极细修剪,而不会在缝合极被修剪时引入应力。

    Abs through aggressive stitching
    8.
    发明申请
    Abs through aggressive stitching 失效
    通过积极的缝合

    公开(公告)号:US20070268628A1

    公开(公告)日:2007-11-22

    申请号:US11881350

    申请日:2007-07-26

    IPC分类号: G11B5/147

    摘要: Aggressive (i.e. tight tolerance) stitching offers several advantages for magnetic write heads but at the cost of some losses during pole trimming. This problem has been overcome by replacing the alumina filler layer, that is used to protect the stitched pole during trimming, with a layer of electro-plated material. Because of the superior step coverage associated with the plating method of deposition, pole trimming can then proceed without the introduction of stresses to the stitched pole while it is being trimmed.