OPTICAL ELEMENT, MOLD, AND OPTICAL DEVICE
    1.
    发明申请
    OPTICAL ELEMENT, MOLD, AND OPTICAL DEVICE 有权
    光学元件,模具和光学器件

    公开(公告)号:US20140211302A1

    公开(公告)日:2014-07-31

    申请号:US14163224

    申请日:2014-01-24

    IPC分类号: G02B1/11 G02B13/14

    CPC分类号: G02B1/118 G02B13/14

    摘要: An optical element having an antireflection effect includes an incident plane and an emission plane and a conical microstructure formed on at least one plane of the incident plane and the emission plane. The conical microstructure includes a first structure formed of a plurality of conical microprojections with an average height H1 and a second structure formed of a plurality of conical microrecesses with an average height H2. The average height H1 satisfies an inequality H1≦1/3*λ/n and the average height H2 satisfies an inequality H2≦1/3*λ/n. An average pitch P between the first structure and the second structure satisfies following conditions: H1/2≦P≦1/3*λ/n, and H2/2≦P≦1/3*λ/n, in which the use wavelength is defined as X and the refractive index relative to the use wavelength is n.

    摘要翻译: 具有防反射效果的光学元件包括在入射面和发射面的至少一个平面上形成的入射面和发射面以及圆锥形微结构。 圆锥形微结构包括由具有平均高度H1的多个锥形微喷射体形成的第一结构和由具有平均高度H2的多个锥形微过程形成的第二结构。 平均高度H1满足不等式H1< nlE; 1/3 *λ/ n,平均高度H2满足不等式H2≦̸ 1/3 *λ/ n。 第一结构和第二结构之间的平均间距P满足以下条件:H1 / 2≦̸ P≦̸ 1/3 *λ/ n和H2 / 2≦̸ P≦̸ 1/3 *λ/ 被定义为X,相对于使用波长的折射率为n。

    METHOD FOR PRODUCING DUST CORE
    2.
    发明申请
    METHOD FOR PRODUCING DUST CORE 有权
    生产粉芯的方法

    公开(公告)号:US20110274576A1

    公开(公告)日:2011-11-10

    申请号:US13188638

    申请日:2011-07-22

    IPC分类号: B22F3/12

    摘要: An object of the present invention is to provide a method for producing a dust core wherein generation of iron oxide at grain boundaries in the dust core is unlikely to take place upon annealing of the dust core subjected to compaction, thus allowing excellent electromagnetic characteristics to be realized. Also, the following is provided: a method for producing a dust core, which comprises: a step of molding a magnetic powder comprising a powder for a dust core formed with an iron-based magnetic powder coated with a silicone resin into a dust core via compaction; and a step of annealing the dust core via heating so as to cause the silicone resin contained in the dust core to be partially formed into a silicate compound, wherein annealing of the dust core is carried out at a dew point of an inert gas of −40° C. or lower in an inert gas atmosphere in the annealing step.

    摘要翻译: 本发明的目的在于提供一种粉尘芯的制造方法,其特征在于,在经过压实的压粉芯退火后,在粉尘芯中产生铁氧化物不容易发生,从而使电磁特性优异 实现了 另外,提供以下内容:一种压粉芯的制造方法,其特征在于,包括以下步骤:将形成有由硅酮树脂涂覆的铁基磁性粉末形成的粉尘的粉末的磁性粉末成型为粉尘芯, 压实 以及通过加热对所述防尘芯体进行退火以使所述防尘芯体中包含的硅酮树脂部分地形成为硅酸盐化合物的步骤,其中所述防尘芯的退火在所述惰性气体的露点处进行, 在退火步骤中的惰性气体气氛中为40℃以下。