Method for manufacturing high magnetic flux denshy grain oriented electrical steel sheet based on low temperature slab heating method
    1.
    发明授权
    Method for manufacturing high magnetic flux denshy grain oriented electrical steel sheet based on low temperature slab heating method 有权
    基于低温板坯加热方法制造高磁通密度晶粒取向电工钢板的方法

    公开(公告)号:US06451128B1

    公开(公告)日:2002-09-17

    申请号:US09242865

    申请日:1999-02-25

    IPC分类号: H01F1147

    摘要: A method for manufacturing a high magnetic flux density grain oriented electrical steel sheet is disclosed. A silicon steel slab is heated and hot-rolled, and the steel sheet is annealed and cold-rolled and decarburized. An annealing separator is spread on the steel sheet, and a final high temperature annealing is carried out. The silicon steel contains in weight % 0.02-0.045% of C, 2.90-3.30% of Si, 0.05-0.30% of Mn, 0.005-0.019% of Al, 0.003-0.008% of N, 0.006% or less of S (the above being main ingredients), 0.001-0.012% of B, and a balance of Fe and unavoidable impurities; or the above main ingredients plus 0.30-0.70% of Cu, 0.03-0.07% of Ni, 0.03-0.07% of Cr, and a balance of Fe and unavoidable impurities; or the above main ingredients plus 0.001-0.012% of B, 0.30-0.70% of Cu, 0.03-0.07% of Ni, 0.03-0.07% of Cr, and a balance of Fe and unavoidable impurities.

    摘要翻译: 公开了一种制造高磁通密度晶粒取向电工钢板的方法。 对硅钢板进行加热热轧,对钢板进行退火冷轧,脱碳。 将退火分离器铺展在钢板上,进行最终的高温退火。 硅钢的重量%为C:0.02-0.045%,Si:2.90-3.30%,Mn:0.05-0.30%,Al:0.005-0.019%,N:0.003-0.008%,S:0.006% 以上为主要成分),0.001-0.012%B,余量为Fe和不可避免的杂质; 或上述主要成分加入Cu 0.30-0.70%,Ni 0.03-0.07%,Cr 0.03-0.07%,余量为Fe和不可避免的杂质; 或上述主要成分加上0.001-0.012%的B,0.30-0.70%的Cu,0.03-0.07%的Ni,0.03-0.07%的Cr,余量的Fe和不可避免的杂质。