Production of polyurethane foams
    2.
    发明授权
    Production of polyurethane foams 失效
    生产聚氨酯泡沫

    公开(公告)号:US6031013A

    公开(公告)日:2000-02-29

    申请号:US176423

    申请日:1998-10-21

    摘要: In a process for producing foams based on polyisocyanate polyaddition products by reacting isocyanates with compounds which are reactive toward isocyanates and have a molecular weight of from 400 to 8000 in the presence of blowing agents, catalysts and, if desired, chain extenders and/or crosslinkers having a molecular weight of 40.degree. C.

    摘要翻译: 在通过使异氰酸酯与对异氰酸酯具有反应性并且在发泡剂,催化剂和如果需要的情况下,扩链剂和/或交联剂存在下分子量为400-8000的化合物反应生产基于多异氰酸酯加聚产物的泡沫的方法 具有分子量<400的助剂和/或添加剂,使用具有异氰脲酸酯和/或缩二脲结构的异氰酸酯,至少一种对异氰酸酯具有反应性的化合物,其分子量为400至8000并且至少包含 50%的伯羟基,作为催化剂的至少一种叔胺和至少一种金属盐加上0.5-5.3重量%的水,基于对异氰酸酯具有反应性且分子量为400的化合物的重量 至8000℃,反应在> 40℃下进行。

    Radiation-sensitive material containing a multilayer support material
    3.
    发明授权
    Radiation-sensitive material containing a multilayer support material 失效
    含有多层载体材料的辐射敏感材料

    公开(公告)号:US6074798A

    公开(公告)日:2000-06-13

    申请号:US196742

    申请日:1998-11-20

    CPC分类号: G03F3/102 G03F7/34

    摘要: The invention relates to a radiation-sensitive material comprising A) a multilayer support material, B) a colored photopolymerizable layer, and C) an adhesive layer. The multilayer support material consists of at least two sheet-form materials, which are bonded to one another in such a way that the adhesion between the two sheet-form materials is less than the adhesion between the radiation-sensitive layer and the adjacent support material. The invention furthermore relates to a process in which a colored image, in particular a multicolored image comprising a plurality of primary-color images, is produced on an image-receiving material. The color images are produced by laminating a colored photopolymerizable layer onto the image-receiving material, exposing the material under the relevant master, in particular a color separation, developing the image by peeling-off the support film from the photopolymerizable layer together with the non-image areas, and, if desired, repeating the same steps with a photopolymerizable layer in a different color.

    摘要翻译: 本发明涉及一种辐射敏感材料,其包括A)多层载体材料,B)着色的可光聚合层,和C)粘合剂层。 多层载体材料由至少两种片状材料组成,这两种片状材料彼此粘合,使两个片状材料之间的粘合力小于辐射敏感层和相邻载体材料之间的粘合性 。 本发明还涉及在图像接收材料上产生彩色图像,特别是包括多个原色图像的多色图像的过程。 彩色图像是通过将着色的可光聚合层层压到图像接收材料上,将相关母版下的材料曝光,特别是颜色分离,通过从支持膜与可光聚合层一起剥离来显影图像而产生的, 图像区域,如果需要,用不同颜色的可光聚合层重复相同的步骤。

    Method for producing a positive as well as a negative multicolor
color-proof image
    6.
    发明授权
    Method for producing a positive as well as a negative multicolor color-proof image 失效
    用于产生正面以及负面的多色防色图像的方法

    公开(公告)号:US5972558A

    公开(公告)日:1999-10-26

    申请号:US104365

    申请日:1998-06-25

    CPC分类号: G03F3/102

    摘要: A method for producing a positive as well as a negative multicolor color-proof image.The invention relates to a color proofing process in which a multicolor image is produced from a plurality of single-color images in register with the aid of a colored, photosensitive, photopolymerizable material on an image-receiving material. Depending on the processing variant, both positive and negative film masters can be processed, even simultaneously on a single receiving material, and it is not necessary for the emission spectrum of the light source to be variable.

    摘要翻译: 一种产生正面和负面的多色防色图像的方法。 本发明涉及一种彩色打样工艺,其中通过借助于图像接收材料上的着色感光的可光聚合材料,从多个单色图像中产生多色图像。 取决于处理方式,即使在单个接收材料上也可以同时处理正面和负面胶片主体,并且不需要光源的发射光谱是可变的。

    Fully aromatic mesomorphic polyesters and their preparation
    9.
    发明授权
    Fully aromatic mesomorphic polyesters and their preparation 失效
    全芳族介晶聚酯及其制备

    公开(公告)号:US4749769A

    公开(公告)日:1988-06-07

    申请号:US64700

    申请日:1987-06-22

    CPC分类号: C08G63/605

    摘要: Fully aromatic mesomorphic polyesters which give a liquid crystalline filament-forming melt below 300.degree. C. consist of(a) from 5 to 25 mol % of repeating units of the formula I ##STR1## (b) from 5 to 25 mol % of repeating units of the formula II ##STR2## (c) from 10 to 50 mol % of repeating units of the formula III ##STR3## and (d) not less than 10 mol % of repeating units of the formula IV ##STR4## the sum of the molar amounts of components (a), (b), (c) and (d) being 100 mol %, and the molar ratio of components (a) and (b) to component (c) being from 0.9:1 to 1.1:1.