摘要:
Provided is a Nd-based two-phase separation amorphous alloy by adding an element having a big difference in heat of mixing in a Nd-based alloy with a superior amorphous formability through an inherent characteristic of compositional elements and consideration of thermodynamics, at the time of forming amorphous phase, to thereby enable two-phase separation amorphous alloy during solidification. The Nd-based two-phase separation amorphous alloy is represented as a general equation Nd100-a-b(TM)a(D)b wherein TM is a combination selected from A-B, A-C and B—C when an element group of A consists of Y, Ti, Zr, La, Pr, Gd and Hf, an element group of B consists of Fe and Mn, and an element group of C consists of Co, Ni, Cu and Ag, wherein the content of the element group which constitutes the combination is 5 atomic weight % or greater, and the element selected from each of the element group is at least one element, and the content of one element selected from each of the element group does not exceed 50 atomic weight %, wherein the content of the element group of B is less than that of the element group of C when TM is a B—C combination, and wherein D is at least one selected from the group consisting of Al, B, Si and P, and a and b have the range of 20≦a≦70, 5≦b≦30, and a+b≧40 in terms of atomic weight %.
摘要翻译:提供了一种Nd基二相分离非晶合金,通过在Nd基合金中通过组成元素的固有特性和热力学的考虑,在Nd基合金中添加具有大的混合热差的元素和优异的非晶形成性 形成非晶相,从而使固化期间的两相分离非晶态合金。 Nd基二相分离非晶态合金表示为一般方程式Nd100-ab(a)(D)b其中,当A的元素组由Y,Ti组成时,TM是选自AB,AC和BC的组合 ,Zr,La,Pr,Gd和Hf中的一种元素组,由Fe和Mn组成,C元素组由Co,Ni,Cu和Ag组成,其中构成组合的元素基团的含量为 5原子%以上,从元素组中选择的元素为至少一种元素,从元素组中选择的一种元素的含量不超过50原子%,其中元素的含量 当TM是BC组合时,B的组小于C的元素组,并且其中D是选自Al,B,Si和P中的至少一种,a和b的范围为20 <= a <= 70,5 <= b <= 30,a + b> = 40。
摘要:
Provided is a Nd-based two-phase separation amorphous alloy by adding an element having a big difference in heat of mixing in a Nd-based alloy with a superior amorphous formability through an inherent characteristic of compositional elements and consideration of thermodynamics, at the time of forming amorphous phase, to thereby enable two-phase separation amorphous alloy during solidification. The Nd-based two-phase separation amorphous alloy which is represented as a general equation Nd100-a-b(TM)a(D)b wherein TM is a transition metal which is a combination of respective one selected from A-B, A-C and B-C when a group of A consists of Y, Ti, Zr, La, Pr, Gd, and Hf, a group of B consists of Fe, and Mn, and a group of C consists of Co, Ni, Cu, and Ag, wherein the content of the element group which constitutes each combination is 5 atomic weight % or greater, and the element selected from each element group is at least one, and wherein D is at least one selected from the group consisting of Al, B, Si and P, and a and b have the range of 20≦a≦80, and 5≦b≦30, respectively, in terms of atomic weight %.
摘要翻译:提供了一种Nd基二相分离非晶合金,通过在Nd基合金中通过组成元素的固有特性和热力学的考虑,在Nd基合金中添加具有大的混合热差的元素和优异的非晶形成性 形成非晶相,从而使固化期间的两相分离非晶态合金。 以通常方程式表示的基于Nd的两相分离非晶态合金(D)B(B) 其中当A组由Y,Ti,Zr,La,Pr,Gd和Hf组成时,TM是一种选自AB,AC和BC的各自的组合的过渡金属,B组由Fe组成, 和Mn,C组由Co,Ni,Cu和Ag组成,其中构成每个组合的元素基团的含量为5原子%或更大,并且每个元素基团中的元素为至少一个 ,其中D是选自Al,B,Si和P中的至少一种,a和b分别具有20 <= a <= 80和5 <= b <30的范围 原子量%。
摘要:
Provided is a Nd-based two-phase separation amorphous alloy by adding an element having a big difference in heat of mixing in a Nd-based alloy with a superior amorphous formability through an inherent characteristic of compositional elements and consideration of thermodynamics, at the time of forming amorphous phase, to thereby enable two-phase separation amorphous alloy during solidification. The Nd-based two-phase separation amorphous alloy is represented as a general equation Nd100-a-b(TM)a(D)b wherein TM is a combination selected from A-B, A-C and B—C when an element group of A consists of Y, Ti, Zr, La, Pr, Gd and Hf, an element group of B consists of Fe and Mn, and an element group of C consists of Co, Ni, Cu and Ag, wherein the content of the element group which constitutes the combination is 5 atomic weight % or greater, and the element selected from each of the element group is at least one element, and the content of one element selected from each of the element group does not exceed 50 atomic weight %, wherein the content of the element group of B is less than that of the element group of C when TM is a B—C combination, and wherein D is at least one selected from the group consisting of Al, B, Si and P, and a and b have the range of 20≦a≦70, 5≦b≦30, and a+b≧40 in terms of atomic weight %.
摘要:
Disclosed is a single-phase amorphous alloy having an enhanced ductility. The single-phase amorphous alloy has a composition range of A100-a-bBaCb where a and b are respectively 0
摘要:
Disclosed is a magnesium based amorphous alloy having a good glass forming ability and ductility. The Mg based amorphous alloy has a composition range of Mg100-x-yAxBy where x and y are respectively 2.5≦x≦30, 2.5≦y≦20 in atomic percent. Here, A includes at least one element selected from the group consisting of Cu, Ni, Zn, Al, Ag, and Pd, and B includes at least one element selected from the group consisting of Gd, Y, Ca, and Nd.
摘要:
Disclosed is a quasicrystalline phase-reinforced Mg-based metallic alloy with high warm and hot formability, and making method thereof. The metallic alloy comprises a composition of Mg—1˜10 at % Zn—0.1˜3 at % Y, in which a two-phase region consisting of a quascrystalline phase and a magnesium-based solid solution phase exists. Constituting a matrix structure, the Mg-based solid solution phase (&agr;—Mg) is formed as a primary solid phase upon solidification. The quasicrystalline phase serves as a second phase and forms, together with the Mg-based solid solution phase, a eutectic phase, thereby reinforcing the matrix. The materials obtained through the hot rolling or extrusion of the cast alloy have an increased volume % of the second phase and thus show significantly increased strength.
摘要:
A ductile particle-reinforced amorphous matrix composite characterized in that ductile powder is dispersed into amorphous matrix and the mixture is plastically worked to be consolidated and a method for manufacturing the same are provided. The amorphous powder includes any alloy, which can be produced in the form of amorphous structure and which is selected from the group consisting of Ni-, Ti-, Zr-, Al-, Fe-, La-, Cu- and Mg-based alloys. The method for manufacturing a ductile particle-reinforced amorphous matrix composite, the method comprising steps of preparing a mixture consisting of amorphous powder and ductile powder, obtaining a billet by compacting the mixture in a hermetically sealing condition, and plastic working the mixture by processing the billet at the temperature in the super-cooled liquid region of the amorphous alloy.
摘要:
Disclosed are nickel-based amorphous alloy compositions, and particularly quaternary nickel-based amorphous alloy compositions containing nickel, zirconium and titanium as main constituent elements and additive Si or P, the quaternary nickel-zirconium-titanium-silicon alloy compositions comprising nickel in the range of 45 to 63 atomic %, zirconium plus titanium in the range of 32 to 48 atomic % and silicon in the range of 1 to 11 atomic %, and being represented by the general formula: Nia(Zr1−xTix)bSic. Also, at least one kind of element selected from the group consisting of V, Cr, Mn, Cu, Co, W, Sn, Mo, Y, C, B, P, Al can be added to the alloy compositions in the range of content of 2 to 15 atomic %. The quaternary nickel-zirconium-titanium-phosphorus alloy compositions comprising nickel in the range of 50 to 62 atomic %, zirconium plus titanium in the range of 33 to 46 atomic % and phosphorus in the range of 3 to 8 atomic %, and being represented by the general formula: Nid(Zr1−yTiy)ePf. The nickel-based amorphous alloy compositions have a superior amorphous phase-forming ability to produce the bulk amorphous alloy having a thickness of 1 mm by general casting methods.
摘要:
In Cu-based bulk amorphous matrix composite materials, comprising a Cu-based amorphous alloy containing high fusion point element(s) selected from a group of Ta, W or combination thereof, wherein the high fusion point element(s) has(have) a shape of crystalline grain and is(are) dispersed around a Cu-based amorphous matrix. Cu-based bulk amorphous matrix composite materials have the composition expressed as the following Chemical formula 1; CuaZrbTicRd [Chemical formula 1] where R is Ta, W or combination thereof, a, b, c and d are atomic weight ratio, a+b+c+d equals 100, a, b, c, and d have the range of 45≦a≦65, 10≦b≦35, 5≦c≦30, and 5≦d≦10, respectively.
摘要翻译:在包含选自Ta,W或其组合的高熔点元素的Cu基非晶态合金的Cu基块状无定形基质复合材料中,其中高熔点元素具有(具有) 晶体形状并分散在Cu基非晶基体周围。 Cu基块状无定形基质复合材料具有如下化学式1所示的组成: <?in-line-formula description =“In-line Formulas”end =“lead”?> CuaZrbTicRd [化学式1] <?in-line-formula description =“In-line Formulas”end =“tail”?> 其中R是Ta,W或其组合,a,b,c和d是原子重量比,a + b + c + d等于100,a,b,c和d的范围为45 <= a < 65,10 <= b <= 35,5 <= c <= 30,5 <= d <= 10。
摘要:
In Cu-based bulk amorphous matrix composite materials, comprising a Cu-based amorphous alloy containing high fusion point element(s) selected from a group of Ta, W or combination thereof, wherein the high fusion point element(s) has(have) a shape of crystalline grain and is(are) dispersed around a Cu-based amorphous matrix. Cu-based bulk amorphous matrix composite materials have the composition expressed as the following Chemical formula 1; [Chemical formula 1]CuaZrbTicRd where R is Ta, W or combination thereof, a, b, c and d are atomic weight ratio, a+b+c+d equals 100, a, b, c, and d have the range of 45≦a≦65, 10≦b≦35, 5≦c≦30, and 5≦d≦10, respectively.
摘要翻译:在包含选自Ta,W或其组合的高熔点元素的Cu基非晶态合金的Cu基块状无定形基质复合材料中,其中高熔点元素具有(具有) 晶体形状并分散在Cu基非晶基体周围。 Cu基块状无定形基质复合材料具有如下化学式1所示的组成: [化学式1]其中R是Ta,W或其组合的一种或多种其中R a, a,b,c和d是原子重量比,a + b + c + d等于100,a,b,c和d的范围为45 <= a <= 65,10 <= b <= 35 ,5 <= c <= 30,5 <= d <= 10。