公开(公告)号:US10329189B2
公开(公告)日:2019-06-25
申请号:US15739110
申请日:2016-06-16
Applicant: JUSHI GROUP CO., LTD.
Inventor: Yuqiang Zhang , Guorong Cao , Lin Zhang , Wenzhong Xing , Guijiang Gu
Abstract: A high-modulus glass fiber composition, and a glass fiber and a composite material therefrom. The glass fiber composition comprises the following components in weight percentage: SiO2 55.7 to 58.9%, Al2O3 15 to 19.9%, Y2O3 0.1 to 4.3%, La2O3 less than or equal to 1.5%, CeO2 less than or equal to 1.2%, CaO 6 to 10%, MgO 9.05 to 9.95%, SrO less than or equal to 2%, Li2O+Na2O+K2O less than or equal to 0.99%, Li2O less than or equal to 0.65%, Fe2O3 less than 1%, TiO2 0.1 to 1.5%; wherein, the range of the weight percentage ratio C1=Y2O3/(Y2O3+La2O3+CeO2) is greater than 0.6. The composition can greatly improve the elastic modulus of glass, significantly reduce liquidus temperature and forming temperature of the glass, greatly reduce the crystallization rate of molten glass and bubble amount under the same conditions, and therefore is more suitable for large-scale tank furnace production of high-modulus fiberglass with low bubble amount.
-
公开(公告)号:US10590027B2
公开(公告)日:2020-03-17
申请号:US16081350
申请日:2016-03-21
Applicant: JUSHI GROUP CO., LTD.
Inventor: Yuqiang Zhang , Guorong Cao , Lin Zhang , Wenzhong Xing , Guijiang Gu
Abstract: Provided are a high performance glass fiber composition, and a glass fiber and a composite material thereof. The content, given in weight percentage, of each component of the glass fiber composition is as follows: 52-67% of SiO2, 12-24% of Al2O3, 0.05-4.5% of Sm2O3+Gd2O3, less than 2% of Li2O+Na2O+K2O, 10-24% of CaO+MgO+SrO, less than 16% of CaO, less than 13% of MgO, less than 3% of TiO2, and less than 1.5% of Fe2O3. The composition significantly improves the mechanical properties and the thermal stability of glass, significantly reduces the liquidus temperature and forming temperature of glass, and under equal conditions, significantly reduces the crystallisation rate of glass. The composition is particularly suitable for the tank furnace production of a high performance glass fiber having excellent thermal stability.
-
公开(公告)号:US10287206B2
公开(公告)日:2019-05-14
申请号:US15851759
申请日:2017-12-22
Applicant: JUSHI GROUP CO., LTD.
Inventor: Guorong Cao , Lin Zhang , Wenzhong Xing , Guijiang Gu
Abstract: A composition of matter, including the following components expressed as percentage by weight: SiO2, 58-60.4%; Al2O3, 14-16.5%; CaO, 14.1-16.5%; MgO, 6-8.2%; Li2O, 0.01-0.4%; Na2O+K2O, less than 1.15%; K2O, greater than 0.5%; TiO2, less than 1.5%; and Fe2O3, less than 1%. The range of the weight percentage ratio CaO/MgO is greater than 2 and less than or equal to 2.4. A glass fiber prepared from the composition is also provided.
-
4.
公开(公告)号:US10207949B2
公开(公告)日:2019-02-19
申请号:US15821710
申请日:2017-11-22
Applicant: JUSHI GROUP CO., LTD.
Inventor: Lin Zhang , Wenzhong Xing , Guorong Cao , Guijiang Gu
Abstract: A composition for producing a glass fiber, including the following components with corresponding percentage amounts by weight: SiO2: 57.1-61.4%; Al2O3: 17.1-21%; MgO: 10.1-14.5%; Y2O3: 1.1-4.3%; CaO:
-
公开(公告)号:US09758423B2
公开(公告)日:2017-09-12
申请号:US15122127
申请日:2015-01-20
Applicant: JUSHI GROUP CO., LTD.
Inventor: Guorong Cao , Wenzhong Xing , Lin Zhang , Guijiang Gu
Abstract: The present invention provides a glass fiber composition, a glass fiber and a composite material therefrom. The glass fiber composition comprises the following components expressed as percentage by weight: 58-64% SiO2, 14-19% Al203, ≧8.8% and
-
公开(公告)号:US11078109B2
公开(公告)日:2021-08-03
申请号:US16309611
申请日:2018-08-24
Applicant: JUSHI GROUP CO., LTD.
Inventor: Guorong Cao , Wenzhong Xing , Lin Zhang , Guijiang Gu
IPC: C03C13/00 , C03C3/087 , C03C3/112 , C03B37/01 , C03B37/022
Abstract: A composition for producing a glass fiber, including the following components with corresponding percentage amounts by weight: 54.2-64% SiO2, 11-18% Al2O3, 20-25.5% CaO, 0.3-3.9% MgO, 0.1-2% of Na2O+K2O, 0.1-1.5% TiO2, and 0.1-1% total iron oxides including ferrous oxide (calculated as FeO). The weight percentage ratio C1=FeO/(iron oxides−FeO) is greater than or equal to 0.53. The total content of the above components in the composition is greater than 97%. The invention also provides a glass fiber produced using the composition and a composite material including the glass fiber.
-
公开(公告)号:US10399889B2
公开(公告)日:2019-09-03
申请号:US15565412
申请日:2016-04-06
Applicant: JUSHI GROUP CO., LTD.
Inventor: Lin Zhang , Guorong Cao , Wenzhong Xing , Guijiang Gu , Xiucheng Hong
IPC: C03C3/087
Abstract: The present invention provides a glass fiber composition, glass fiber and composite material therefrom. The glass fiber composition comprises the following components expressed as percentage by weight: 58.5-62.5% SiO2, 14.5-17% Al2O3, 10.5-14.5% CaO, 8-10% MgO, 0.5%
-
公开(公告)号:US10351465B2
公开(公告)日:2019-07-16
申请号:US15511585
申请日:2014-12-29
Applicant: JUSHI GROUP CO., LTD.
Inventor: Guorong Cao , Wenzhong Xing , Lin Zhang , Guijiang Gu
Abstract: The present invention provides a glass fiber composition, glass fiber and composite material therefrom. The glass fiber composition comprises the following components expressed as percentage by weight: 58-63% SiO2, 13-17% Al2O3, 6-11.8% CaO, 7-11% MgO, 3.05-8% SrO, 0.1-2% Na2O+K2O+Li2O, 0.1-1% Fe2O3, 0-1% CeO2 and 0-2% TiO2, wherein a weight percentage ratio C1=(MgO+SrO)/CaO is greater than 1. Said composition greatly improves the refractive index of glass, significantly shields against harmful rays for humans and further reduces glass crystallization risk and production costs, thereby making it more suitable for large-scale production with refractory-lined furnaces.
-
9.
公开(公告)号:US10189742B2
公开(公告)日:2019-01-29
申请号:US15805159
申请日:2017-11-07
Applicant: JUSHI GROUP CO., LTD.
Inventor: Lin Zhang , Guorong Cao , Wenzhong Xing , Guijiang Gu
Abstract: A composition for producing a glass fiber, including the following components with the corresponding percentage amounts by weight: SiO2: 58-62%; Al2O3: 14-18%; CaO+MgO: 20-24.5%; CaO: greater than 14%; Li2O: 0.01-0.5%; Na2O+K2O: less than 2%; TiO2: less than 3.5%; Fe2O3: less than 1%; and F2: less than 1%. The weight percentage ratio of CaO/MgO is greater than 2 and less than or equal to 2.6; and the weight percentage ratio SiO2/CaO is between 3.3 and 4.3. The invention also provides a glass fiber produced using the composition and a composite material including the glass fiber.
-
10.
公开(公告)号:US10377662B2
公开(公告)日:2019-08-13
申请号:US15739081
申请日:2016-03-21
Applicant: JUSHI GROUP CO., LTD.
Inventor: Yuqiang Zhang , Guorong Cao , Lin Zhang , Wenzhong Xing , Guijiang Gu
Abstract: The present invention provides a glass fiber composition, a glass fiber and a composite material therefrom. The glass fiber composition comprises the following components expressed as percentage by weight: 53-64% SiO2, greater than 19% and lower than 25% Al2O3, 0.05-7% Y2O3+La2O3+Gd2O3, not greater than 1% Li2O+Na2O+K2O, 10-24% CaO+MgO+SrO, 1.5-12% CaO, lower than 2% TiO2, lower than 1.5% Fe2O3. Said composition can not only significantly improve the elastic modulus and chemical stability of the glass, but also overcome the technical problems in the manufacture of traditional high-performance glasses including high risk of crystallization, fining difficulty of molten glass and production efficiency difficulty with refractory-lined furnaces, significantly reduce the liquidus and forming temperatures and greatly reduce the crystallization rate under the same conditions, thus making it particularly suitable for production of high-performance glass fiber with excellent chemical stability in refractory-lined furnaces.
-
-
-
-
-
-
-
-
-