Resin composition, and wire and cable using the same
    1.
    发明授权
    Resin composition, and wire and cable using the same 有权
    树脂组成,使用电线电缆

    公开(公告)号:US09127110B2

    公开(公告)日:2015-09-08

    申请号:US13474692

    申请日:2012-05-17

    Abstract: A resin composition includes a silane-crosslinked polyethylene as a main component provided by crosslinking a polyethylene in the presence of a silanol condensation catalyst and water, the polyethylene being graft-copolymerized with a silane compound by a free radical generating agent. The polyethylene has a density of 0.87 to 0.91 g/cm3. The silane compound is included not less than 2 parts by mass relative to 100 parts by mass of the polyethylene. The resin composition includes silicon detected by a fluorescence X-ray at a rate of not less than 0.3 mass % and has a gel fraction of not less than 70%. A mass ratio of the silane compound to the free radical generating agent is not less than 35 and not more than 150.

    Abstract translation: 树脂组合物包括硅烷交联聚乙烯作为主要组分,其通过在硅烷醇缩合催化剂和水的存在下交联聚乙烯,所述聚乙烯通过自由基生成剂与硅烷化合物接枝共聚。 聚乙烯的密度为0.87〜0.91g / cm 3。 相对于100质量份的聚乙烯,硅烷化合物的含量不得少于2质量份。 树脂组合物包含通过荧光X射线以不小于0.3质量%的速率检测并具有不小于70%的凝胶分数的硅。 硅烷化合物与自由基发生剂的质量比不小于35且不大于150。

    NON-HALOGEN FLAME-RESISTANT THERMOPLASTIC ELASTOMER COMPOSITION, MANUFACTURING METHOD THEREOF, AND ELECTRIC WIRE OR CABLE IN WHICH ITS ELASTOMER COMPOSITION IS USED
    2.
    发明申请
    NON-HALOGEN FLAME-RESISTANT THERMOPLASTIC ELASTOMER COMPOSITION, MANUFACTURING METHOD THEREOF, AND ELECTRIC WIRE OR CABLE IN WHICH ITS ELASTOMER COMPOSITION IS USED 审中-公开
    非卤化物耐火热塑性弹性体组合物及其制造方法,以及使用其弹性体组合物的电线或电缆

    公开(公告)号:US20080023680A1

    公开(公告)日:2008-01-31

    申请号:US11830232

    申请日:2007-07-30

    CPC classification number: C09K21/14 C09K21/02

    Abstract: Non-halogen flame-resistant thermoplastic elastomer composition, manufacturing method, and an electric wire or cable in which non-halogen flame-resistant thermoplastic elastomer composition is used for an insulator or a sheath are provided. Non-halogen flame-resistant thermoplastic elastomer composition includes (A) 40 to 80 parts by weight of ethylene-vinyl acetate copolymer, in which the content of vinyl acetate is 30 wt % or more; (B) 60 to 20 parts by weight of crystalline polyolefin resin; and (C) 40 to 250 parts by weight of metalhydroxide for 100 parts by weight in total of (A) and (B). Further, ethylene-vinyl acetate copolymer is cross-linked with silane.

    Abstract translation: 提供了非卤素阻燃热塑性弹性体组合物,制造方法以及其中使用非卤素阻燃热塑性弹性体组合物用于绝缘体或护套的电线或电缆。 无卤阻燃热塑性弹性体组合物包含(A)40〜80重量份乙烯 - 乙酸乙烯酯共聚物,其中乙酸乙烯酯的含量为30重量%以上; (B)60〜20重量份结晶聚烯烃树脂; 和(C)相对于(A)和(B)总计100重量份,为40〜250重量份的金属氢氧化物。 此外,乙烯 - 乙酸乙烯酯共聚物与硅烷交联。

    Method for producing &egr;-caprolactam and reactor for the method
    3.
    发明授权
    Method for producing &egr;-caprolactam and reactor for the method 失效
    用于该方法生产ε-己内酰胺和反应器的方法

    公开(公告)号:US06531595B2

    公开(公告)日:2003-03-11

    申请号:US09963603

    申请日:2001-09-27

    CPC classification number: C07D201/04

    Abstract: A method is provided for producing &egr;-caprolactam from cyclohexanone oxime by using a zeolite or non-zeolitic material as a catalyst under gas phase reaction conditions. The method comprises a reaction step converting cyclohexanone oxime into &egr;-caprolactam in the presence of the zeolite or non-zeolitic material; and a regeneration step of treating the zeolite or non-zeolitic material with a non-oxidizing gas at a temperature of from about 100°C. to about 600° C.

    Abstract translation: 提供了一种通过在气相反应条件下使用沸石或非沸石材料作为催化剂从环己酮肟生产ε-己内酰胺的方法。 该方法包括在沸石或非沸石材料存在下将环己酮肟转化成ε-己内酰胺的反应步骤; 以及在约100℃的温度下用非氧化性气体处理沸石或非沸石材料的再生步骤。 至约600℃

    Method for producing cycloalkanol and/or cycloalkanone
    4.
    发明授权
    Method for producing cycloalkanol and/or cycloalkanone 失效
    环烷醇和/或环烷酮的制备方法

    公开(公告)号:US07910777B2

    公开(公告)日:2011-03-22

    申请号:US12560788

    申请日:2009-09-16

    Abstract: The present invention provides a method for producing cycloalkanol and/or cycloalkanone, which comprises reacting cycloalkane with molecular oxygen in the presence of mesoporous silica, (1) the mesoporous silica containing at least one transition metal; (2) the mesoporous silica having such pore distribution that the ratio of a total pore volume of mesoporous silica particles having a pore size of 3 to 50 nm to a total pore volume of mesoporous silica particles having a pore size of 2 to 50 nm is 50% or more; and (3) the mesoporous silica being modified by an organic silicon compound.

    Abstract translation: 本发明提供一种制备环烷醇和/或环烷酮的方法,其包括在介孔二氧化硅存在下使环烷烃与分子氧反应,(1)含有至少一种过渡金属的介孔二氧化硅; (2)具有孔分布的孔隙二氧化硅,孔径为3〜50nm的介孔二氧化硅粒子的总细孔容积与孔径为2〜50nm的介孔二氧化硅粒子的总孔体积的比为 50%以上; 和(3)介孔二氧化硅被有机硅化合物改性。

    Method for manufacturing zeolite and method for manufacturing ε-caprolactam
    5.
    发明授权
    Method for manufacturing zeolite and method for manufacturing ε-caprolactam 失效
    沸石的制造方法及ε-己内酰胺的制造方法

    公开(公告)号:US07060645B2

    公开(公告)日:2006-06-13

    申请号:US11165538

    申请日:2005-06-24

    Abstract: The present invention provides a method for manufacturing a zeolite comprising following steps of: (1): calcining crystals obtained by hydrothermal synthesis reaction of a silicon compound; (2): contact treating a calcined product obtained by the step (1) with an aqueous solution including an amine and/or a quaternary ammonium compound; (3): calcining a treated product obtained by the step (2); and (4): contact treating the calcined product obtained by the step (3) with an aqueous solution including ammonia and/or an ammonium salt. According to the present invention, a method is also provided wherein ε-caprolactam is manufactured by Beckmann rearrangement reaction of cyclohexanone oxime in a gaseous phase in the presence of the zeolite manufactured by the above-described method.

    Abstract translation: 本发明提供一种制造沸石的方法,包括以下步骤:(1):煅烧通过硅化合物的水热合成反应获得的晶体; (2):用包含胺和/或季铵化合物的水溶液接触步骤(1)得到的煅烧产物; (3):煅烧通过工序(2)得到的处理物; 和(4):用包含氨和/或铵盐的水溶液接触处理由步骤(3)获得的煅烧产物。 根据本发明,还提供了一种方法,其中ε-己内酰胺通过在通过上述方法制造的沸石存在下,在气相中通过环己酮肟的贝克曼重排反应制造。

    Method for producing ε-caprolactam and method for reactivating catalyst for production of ε-caprolactam
    6.
    发明授权
    Method for producing ε-caprolactam and method for reactivating catalyst for production of ε-caprolactam 失效
    ε-己内酰胺的制造方法以及催化剂再生催化剂生产ε-己内酰胺的方法

    公开(公告)号:US07026474B2

    公开(公告)日:2006-04-11

    申请号:US11055101

    申请日:2005-02-11

    Abstract: A method for producing ε-caprolactam and a method for reactivating a zeolite catalyst for the production are provided. In the reactivation step, a zeolite catalyst is allowed to contact a gas containing a carboxylic acid, water and a compound selected from ammonia and amines. In accordance with the present invention, the catalytic activities of a zeolite catalyst used for the Beckmann rearrangement reaction of cyclohexanone oxime can be effectively restored. Consequently, ε-caprolactam may be produced with a high production yield for a long period of time by reusing the catalyst by the method described above.

    Abstract translation: 提供了制备ε-己内酰胺的方法和用于再生催化剂的方法。 在再活化步骤中,使沸石催化剂与含有羧酸,水和选自氨和胺的化合物的气体接触。 根据本发明,可以有效地恢复用于环己酮肟的贝克曼重排反应的沸石催化剂的催化活性。 因此,通过上述方法重新使用催化剂,可以长期生产ε-己内酰胺。

    Process for producing ε-caprolactam and catalyst for the production
    7.
    发明授权
    Process for producing ε-caprolactam and catalyst for the production 有权
    生产ε-己内酰胺和催化剂的方法

    公开(公告)号:US06946553B2

    公开(公告)日:2005-09-20

    申请号:US10367701

    申请日:2003-02-19

    CPC classification number: B01J29/90 B01J29/035 B01J38/66

    Abstract: Improved processes for producing an ε-caprolactam using a solid catalyst and for producing a catalyst which can be used in the production of ε-caprolactam are provided. In the present invention, a solid catalyst such as a zeolite is treated with an aqueous solution containing an ammonia and at least one compound selected from the group consisting of quaternary ammonium compounds and lower alkylamines. In accordance with the present invention, a zeolite having a high catalyst activity and a long lifetime is produced, and a solid catalyst which has been used in the production of ε-caprolactam can be re-activated. In the present invention, by using the thus obtained zeolite and/or the thus activated solid catalyst, an ε-caprolactam is produced in a high yield over the long period of time.

    Abstract translation: 提供了使用固体催化剂生产ε-己内酰胺和用于生产可用于生产ε-己内酰胺的催化剂的改进方法。 在本发明中,使用含有氨和至少一种选自季铵化合物和低级烷基胺的化合物的水溶液处理沸石等固体催化剂。 根据本发明,产生具有高催化剂活性和长寿命的沸石,并且可以重新活化用于生产ε-己内酰胺的固体催化剂。 在本发明中,通过使用由此获得的沸石和/或由此活化的固体催化剂,可以长时间以高产率生产ε-己内酰胺。

    Process for producing a high purity caprolactam
    8.
    发明授权
    Process for producing a high purity caprolactam 失效
    生产高纯度己内酰胺的方法

    公开(公告)号:US5459261A

    公开(公告)日:1995-10-17

    申请号:US289577

    申请日:1994-08-15

    CPC classification number: C07D201/16

    Abstract: A process for producing a high purity caprolactam is disclosed in which a crude caprolactam obtained by a catalytic rearrangement of cyclohexanone oxime is subjected(1) to mixing, while stirring, with at least one hydrocarbon selected from the group consisting of aliphatic hydrocarbons and alicyclic hydrocarbons to form a liquid-liquid, two-layer liquid mixture, and then crystallizing caprolactam out of the liquid mixture;(2) to mixing with both at least one hydrocarbon selected from the group consisting of aliphatic hydrocarbons and alicyclic hydrocarbons, and water to form a liquid mixture, separating the liquid mixture into a hydrocarbon layer and a water layer, and then recovering caprolactam from the water layer; or(3) to distillation in the co-presence of at least one aliphatic saturated hydrocarbon of 10 to 18 carbon atoms.

    Abstract translation: 公开了一种制备高纯度己内酰胺的方法,其中通过环己酮肟的催化重排获得的粗己内酰胺在搅拌下与至少一种选自脂族烃和脂环族烃的烃进行混合 形成液 - 液两层液体混合物,然后从该液体混合物中结晶己内酰胺; (2)与选自脂族烃和脂环烃的至少一种烃和水混合以形成液体混合物,将液体混合物分离成烃层和水层,然后从其中回收己内酰胺 水层; 或(3)在至少一种10至18个碳原子的脂族饱和烃的共存下进行蒸馏。

    Process for producing a high purity caprolactam
    9.
    发明授权
    Process for producing a high purity caprolactam 失效
    生产高纯度己内酰胺的方法

    公开(公告)号:US5362870A

    公开(公告)日:1994-11-08

    申请号:US46146

    申请日:1993-04-15

    CPC classification number: C07D201/16

    Abstract: A process for producing a high purity caprolactam is disclosed in which a crude caprolactam obtained by a catalytic rearrangement of cyclohexanone oxime is subjected(1) to mixing, while stirring, with at least one hydrocarbon selected from the group consisting of aliphatic hydrocarbons and alicyclic hydrocarbons to form a liquid-liquid, two-layer liquid mixture, and then crystallizing caprolactam out of the liquid mixture;(2) to mixing with both at least one hydrocarbon selected from the group consisting of aliphatic hydrocarbons and alicyclic hydrocarbons, and water to form a liquid mixture, separating the liquid mixture into a hydrocarbon layer and a water layer, and then recovering caprolactam from the water layer; or(3) to distillation in the co-presence of at least one aliphatic saturated hydrocarbon of 10 to 18 carbon atoms.

    Abstract translation: 公开了一种制备高纯度己内酰胺的方法,其中通过环己酮肟的催化重排获得的粗己内酰胺在搅拌下与至少一种选自脂族烃和脂环族烃的烃进行混合 形成液 - 液两层液体混合物,然后从该液体混合物中结晶己内酰胺; (2)与选自脂族烃和脂环烃的至少一种烃和水混合以形成液体混合物,将液体混合物分离成烃层和水层,然后从其中回收己内酰胺 水层; 或(3)在至少一种10至18个碳原子的脂族饱和烃的共存下进行蒸馏。

    Process for producing pentacyl-type crystalline zeolites and a process for producing &egr;-caprolactam using the same
    10.
    发明授权
    Process for producing pentacyl-type crystalline zeolites and a process for producing &egr;-caprolactam using the same 有权
    制备戊酰基型结晶沸石的方法和使用该方法制备ε-己内酰胺的方法

    公开(公告)号:US06303099B1

    公开(公告)日:2001-10-16

    申请号:US09605473

    申请日:2000-06-28

    Abstract: A process for producing a pentacyl-type crystalline zeolite is provided which comprises the steps of (i) preparing a mixture of a silicon compound, water and tetrapropyl ammonium hydroxide, (ii) conducting a hydrothermal reaction of the mixture to obtain a reaction mixture containing zeolite crystals, (iii) separating zeolite crystals from the reaction mixture to collect a remaining solution, (iv) calcinating the resulting zeolite crystals, (v) treating the calcinated zeolite crystals with a solution such as ammonia water and (vi) recycling the solution collected in step (iii) to step (i), wherein in the mixture prepared in step (i) a molar ratio of hydroxide ion to silicon is from about 0.1 to about 0.4 and a molar ratio of potassium to silicon is about 0.1 or less. With this process, a zeolite catalyst having good performance can be produced with good reproducibility.

    Abstract translation: 提供了一种制备五酰基型结晶沸石的方法,其包括以下步骤:(i)制备硅化合物,水和四丙基氢氧化铵的混合物,(ii)进行混合物的水热反应,得到含有 沸石晶体,(iii)从反应混合物中分离沸石晶体以收集剩余溶液,(iv)煅烧所得沸石晶体,(v)用溶液如氨水处理煅烧的沸石晶体,和(vi)回收溶液 在步骤(iii)至步骤(i)中收集,其中在步骤(i)中制备的混合物中,氢氧根离子与硅的摩尔比为约0.1至约0.4,并且钾与硅的摩尔比为约0.1或更小 。 通过该方法,可以以良好的再现性制造具有良好性能的沸石催化剂。

Patent Agency Ranking