LIQUID CRYSTAL POLYESTER RESIN COMPOSITION
    2.
    发明申请
    LIQUID CRYSTAL POLYESTER RESIN COMPOSITION 有权
    液晶聚酯树脂组合物

    公开(公告)号:US20120235092A1

    公开(公告)日:2012-09-20

    申请号:US13410344

    申请日:2012-03-02

    IPC分类号: C09K19/20

    摘要: An object is to provide a liquid crystal polyester resin composition capable of producing a molding in which the generation amount of particles is sufficiently reduced.The present invention provides a liquid crystal polyester resin composition including (1) a liquid crystal polyester, and (2) a fiber-shaped filler having a fiber diameter of 5 to 15 μm and a number average fiber length of 30 to 200 μm, wherein the content of a fiber having a fiber length of more than 200 μm is 10% by mass or less based on 100% by mass of the amount of the fiber-shaped filler.

    摘要翻译: 本发明的目的是提供一种液晶聚酯树脂组合物,其能够制造其中颗粒的产生量充分降低的成型体。 本发明提供一种液晶聚酯树脂组合物,其包括(1)液晶聚酯,和(2)纤维直径为5〜15μm,数均纤维长为30〜200μm的纤维状填料,其中, 纤维长度大于200μm的纤维的含量相对于纤维状填料的100质量%为10质量%以下。

    LIQUID CRYSTAL POLYESTER COMPOSITION AND PROCESS FOR PRODUCING THE SAME
    3.
    发明申请
    LIQUID CRYSTAL POLYESTER COMPOSITION AND PROCESS FOR PRODUCING THE SAME 有权
    液晶聚酯组合物及其制造方法

    公开(公告)号:US20120217678A1

    公开(公告)日:2012-08-30

    申请号:US13368525

    申请日:2012-02-08

    IPC分类号: C09K19/20 B29C45/00

    摘要: The present invention provides a liquid crystal polyester composition, comprising (i) 100 parts by weight of a liquid crystal polyester, and (ii) 65 to 100 parts by weight of a combination of a fibrous filler with a plate-like filler, wherein the fibrous filler has a number-average fiber diameter of 5 to 15 μm, and a number-average aspect ratio of 20 to 40, and a content ratio by weight of the fibrous filler to the plate-like filler is more than 1.0 and 1.6 or less; and a process for producing the liquid crystal polyester composition comprising a step of melt-kneading the above respective components with one another.

    摘要翻译: 本发明提供一种液晶聚酯组合物,其包含(i)100重量份的液晶聚酯,和(ii)65至100重量份的纤维填料与板状填料的组合,其中 纤维状填料的数均纤维直径为5〜15μm,数均分子比为20〜40,纤维状填料与板状填料的重量比为1.0以上1.6以下 减; 以及一种制备液晶聚酯组合物的方法,包括将上述各组分彼此熔融捏合的步骤。

    LIQUID-CRYSTALLINE POLYMER COMPOSITION AND MOLDED ARTICLE THEREOF
    4.
    发明申请
    LIQUID-CRYSTALLINE POLYMER COMPOSITION AND MOLDED ARTICLE THEREOF 审中-公开
    液晶聚合物组合物及其成型品

    公开(公告)号:US20110210290A1

    公开(公告)日:2011-09-01

    申请号:US13034049

    申请日:2011-02-24

    IPC分类号: C09K19/06 C09K19/00

    摘要: The present invention provides a liquid-crystalline polymer composition comprising:a liquid-crystalline polymer and an aromatic polysulfone resin having oxygen-containing groups selected from among hydroxyl groups and oxyanion groups in an amount of 6×10−5 or more in number per 1 g of the polysulfone resin. The composition can suppress rise of specific gravity and reduction of heat resistance and can stably provide a molded article having excellent mechanical characteristics.

    摘要翻译: 本发明提供一种液晶聚合物组合物,其包含:液晶聚合物和芳族聚砜树脂,其具有选自羟基和氧阴离子基团中的含氧基团,数量为每1个6×10-5或更多 g的聚砜树脂。 该组合物可以抑制比重的升高和耐热性的降低,并且可以稳定地提供具有优异的机械特性的成型体。

    WATER DISPERSION OF AROMATIC POLYSULFONE RESIN PARTICLES
    5.
    发明申请
    WATER DISPERSION OF AROMATIC POLYSULFONE RESIN PARTICLES 审中-公开
    芳香聚苯乙烯树脂颗粒的水分散

    公开(公告)号:US20110054120A1

    公开(公告)日:2011-03-03

    申请号:US12871207

    申请日:2010-08-30

    IPC分类号: C09D181/06

    CPC分类号: C09D181/06

    摘要: The present invention provides a dispersion in which aromatic polysulfone resin particles are dispersed in water. The aromatic polysulfone resin particles comprises a aromatic polysulfone resin having oxygen-containing groups selected from among hydroxyl groups and oxyanion groups in an amount of 1.6 or more groups relative to 100 repeating units forming the aromatic polysulfone resin; and have the volume average particle diameter of 50 μm or less. The dispersion is less likely to cause settlement of the aromatic polysulfone particles and is suited for use as an aqueous coating material.

    摘要翻译: 本发明提供了将芳香族聚砜树脂粒子分散在水中的分散液。 相对于形成芳香族聚砜树脂的100个重复单元,芳香族聚砜树脂粒子含有选自羟基和氧阴离子基中的含氧基团的芳族聚砜树脂的量为1.6以上; 体积平均粒径为50μm以下。 分散体不太可能引起芳族聚砜颗粒的沉降,并且适合用作水性涂料。

    NI-BASED SINGLE CRYSTAL SUPER ALLOY
    7.
    发明申请
    NI-BASED SINGLE CRYSTAL SUPER ALLOY 有权
    基于NI的单晶超级合金

    公开(公告)号:US20110171057A1

    公开(公告)日:2011-07-14

    申请号:US12900896

    申请日:2010-10-08

    IPC分类号: C22C19/05

    CPC分类号: C22C19/057 C30B29/52

    摘要: The object of the present invention is to provide an Ni-based single crystal super alloy capable of improving strength by preventing precipitation of a TCP phase at high temperatures. This object is achieved by an Ni-based single crystal super alloy having a composition comprising 5.0-7.0 wt % of Al, 4.0-10.0 wt % of Ta, 1.1-4.5 wt % of Mo, 4.0-10.0 wt % of W, 3.1-8.0 wt % of Re, 0-0.50 wt % of Hf, 2.0-5.0 wt % of Cr, 0-9.9 wt % of Co and 4.1-14.0 wt % of Ru in terms of its weight ratio, with the remainder consisting of Ni and unavoidable impurities. Furthermore, in this Ni-based single crystal super alloy, when lattice constant of matrix is taken to be a1 and lattice constant of precipitation phase is taken to be a2, a2≦0.999a1.

    摘要翻译: 本发明的目的是提供一种能够通过防止TCP相在高温下析出而提高强度的Ni系单晶超合金。 该目的通过一种Ni基单晶超级合金来实现,该Ni基单晶超合金的组成包括5.0-7.0重量%的Al,4.0-10.0重量%的Ta,1.1-4.5重量%的Mo,4.0-10.0重量%的W,3.1 -8.0重量%的Re,0-0.50重量%的Hf,2.0-5.0重量%的Cr,0-9.9重量%的Co和4.1-14.0重量%的Ru,以其重量比计,其余由 Ni和不可避免的杂质。 此外,在该Ni基单晶超合金中,当将晶格的晶格常数设为a1,析出相的晶格常数取为a2时,a2≦̸ 0.999a1。

    LIQUID CRYSTALLINE POLYESTER RESIN COMPOSITION, MOLDED ARTICLE AND HOLDER FOR OPTICAL PICKUP LENSES
    8.
    发明申请
    LIQUID CRYSTALLINE POLYESTER RESIN COMPOSITION, MOLDED ARTICLE AND HOLDER FOR OPTICAL PICKUP LENSES 失效
    液晶聚酯树脂组合物,用于光学皮肤镜片的模制品和保持器

    公开(公告)号:US20110073807A1

    公开(公告)日:2011-03-31

    申请号:US12890844

    申请日:2010-09-27

    IPC分类号: C09K19/06

    摘要: A liquid crystalline polyester resin composition is provided, by which a molded article with an enhanced specific modulus can be produced. The liquid crystalline polyester resin composition comprises mica fillers in an amount of 15 to 30 parts by mass and carbon fibers with specific volume resistance of 108 Ωcm or more in an amount of 5 to 20 parts by mass with respect to 100 parts by mass of the liquid crystalline polyester.

    摘要翻译: 提供了一种液晶聚酯树脂组合物,通过该液晶聚酯树脂组合物可以制备具有增强的比模量的模制品。 液晶聚酯树脂组合物含有15〜30质量份的云母填充剂,相对于100质量份为5〜20质量份,比容积电阻为108〜OHgr·cm以上的碳纤维 的液晶聚酯。

    CAMERA MODULE CAPABLE OF FIXING LENS HELD IN LENS BARREL AFTER THE LENS IS ADJUSTED IN OPTICAL AXIS DIRECTION
    9.
    发明申请
    CAMERA MODULE CAPABLE OF FIXING LENS HELD IN LENS BARREL AFTER THE LENS IS ADJUSTED IN OPTICAL AXIS DIRECTION 审中-公开
    相机镜头固定镜头固定在镜头后,镜头被调整在光轴方向

    公开(公告)号:US20080112066A1

    公开(公告)日:2008-05-15

    申请号:US11869712

    申请日:2007-10-09

    IPC分类号: G02B7/02

    CPC分类号: G02B7/04

    摘要: A camera module includes a lens barrel 4 for holding a lens 6 and a base 3 having a housing part 11 for housing the lens barrel 4. The lens barrel 4 comes in contact with an inner circumference surface of the housing part 11 of the base 3 on an outer circumference surface and can move in an optical axis direction of the lens 6. The housing part 11 of the base 3 has openings 14 on the circumference surface, and the outer circumference surface of the lens barrel 4 has welding parts 22 for welding with respect to rim parts of the openings 14.

    摘要翻译: 相机模块包括用于保持透镜6的镜筒4和具有用于容纳镜筒4的壳体部分11的底座3。 镜筒4在外周面与底座3的外壳部11的内周面抵接,能够在透镜6的光轴方向上移动。 基座3的外壳部11在圆周面上具有开口14,透镜筒4的外周面具有焊接部22,用于相对于开口14的边缘部进行焊接。

    LIQUID CRYSTAL POLYMER MOLDING AND METHOD FOR PRODUCING THE SAME
    10.
    发明申请
    LIQUID CRYSTAL POLYMER MOLDING AND METHOD FOR PRODUCING THE SAME 审中-公开
    液晶聚合物成型及其制造方法

    公开(公告)号:US20120252955A1

    公开(公告)日:2012-10-04

    申请号:US13425527

    申请日:2012-03-21

    IPC分类号: C08K3/40 B29C45/72 B29C45/00

    摘要: Provided is a liquid crystal polymer molding in which a weld portion has high strength and also surface properties are satisfactory. A method for producing a liquid crystal polymer molding including a weld portion by injection-molding a liquid crystal polymer composition containing a spherical filler, wherein the spherical filler has a center particle diameter of 60 μm or less, the method including molding so as to satisfy a relation: 20≦[thickness of the weld portion/center particle diameter of the spherical filler]≦55; and a liquid crystal polymer molding obtained by such a method.