Metal separator for fuel cell and method for producing the same
    2.
    发明授权
    Metal separator for fuel cell and method for producing the same 有权
    燃料电池用金属隔板及其制造方法

    公开(公告)号:US08241530B2

    公开(公告)日:2012-08-14

    申请号:US12299491

    申请日:2007-05-18

    IPC分类号: H01B1/04 C23C8/72 B05D5/12

    摘要: There is provided an electron conductive and corrosion-resistant material 3 containing titanium (Ti), boron (B) and nitrogen (N) in an atomic ratio satisfying 0.05≦[Ti]≦0.40, 0.20≦[B]≦0.40, and 0.35≦[N]≦0.55 (provided that [Ti]+[B]+[N]=1). Further, there is provided a method of manufacturing an electron conductive and corrosion-resistant material 3, wherein boron nitride powder adheres to the surface of a substrate 2 of which at least the surface is made of titanium or a titanium alloy, and is then heated. Furthermore, there is provided a method of manufacturing an electron conductive and corrosion-resistant material 3, wherein the surface of a substrate 2 of which at least the surface is made of titanium or a titanium alloy is borided and then heated. In addition, there is provided a method of manufacturing an electron conductive and corrosion-resistant material 3, wherein a TiB2 layer formed of TiB2 particles is formed by spraying TiB2 powder onto a metal substrate 2 and then nitriding the TiB2 layer.

    摘要翻译: 提供了含有钛(Ti),硼(B)和氮(N)的电子导电和耐腐蚀材料3,原子比满足0.05≦̸ [Ti]≦̸ 0.40,0.20< 1; [B]≦̸ 0.40和0.35≦̸ [N]≦̸ 0.55(条件是[Ti] + [B] + [N] = 1)。 此外,提供了一种制造电子传导和耐腐蚀材料3的方法,其中氮化硼粉末粘附到至少表面由钛或钛合金制成的基底2的表面,然后被加热 。 此外,提供一种制造电子传导和耐腐蚀材料3的方法,其中至少将表面由钛或钛合金制成的基板2的表面被硼化然后被加热。 此外,提供了一种制造电子传导和耐腐蚀材料3的方法,其中由TiB 2颗粒形成的TiB 2层通过将TiB 2粉末喷涂到金属基底2上然后氮化TiB 2层而形成。

    METAL SEPARATOR FOR FUEL CELL AND METHOD FOR PRODUCING THE SAME
    3.
    发明申请
    METAL SEPARATOR FOR FUEL CELL AND METHOD FOR PRODUCING THE SAME 有权
    用于燃料电池的金属分离器及其制造方法

    公开(公告)号:US20090202736A1

    公开(公告)日:2009-08-13

    申请号:US12299491

    申请日:2007-05-18

    IPC分类号: C23C4/06 H01B1/22 B05D5/12

    摘要: There is provided an electron conductive and corrosion-resistant material 3 containing titanium (Ti), boron (B) and nitrogen (N) in an atomic ratio satisfying 0.05≦[Ti]≦0.40, 0.20≦[B]≦0.40, and 0.35≦[N]≦0.55 (provided that [Ti]+[B]+[N]=1). Further, there is provided a method of manufacturing an electron conductive and corrosion-resistant material 3, wherein boron nitride powder adheres to the surface of a substrate 2 of which at least the surface is made of titanium or a titanium alloy, and is then heated. Furthermore, there is provided a method of manufacturing an electron conductive and corrosion-resistant material 3, wherein the surface of a substrate 2 of which at least the surface is made of titanium or a titanium alloy is borided and then heated. In addition, there is provided a method of manufacturing an electron conductive and corrosion-resistant material 3, wherein a TiB2 layer formed of TiB2 particles is formed by spraying TiB2 powder onto a metal substrate 2 and then nitriding the TiB2 layer.

    摘要翻译: 提供了含有钛(Ti),硼(B)和氮(N)的电子导电耐腐蚀材料3,原子比满足0.05 <= [Ti] <= 0.40,0.20 [= [B] 0.40和0.35 <= [N] <= 0.55(条件是[Ti] + [B] + [N] = 1)。 此外,提供了一种制造电子传导和耐腐蚀材料3的方法,其中氮化硼粉末粘附到至少表面由钛或钛合金制成的基底2的表面,然后被加热 。 此外,提供一种制造电子传导和耐腐蚀材料3的方法,其中至少将表面由钛或钛合金制成的基板2的表面被硼化然后被加热。 此外,提供了一种制造电子传导和耐腐蚀材料3的方法,其中由TiB 2颗粒形成的TiB 2层通过将TiB 2粉末喷涂到金属基底2上然后氮化TiB 2层而形成。

    Aluminum alloys for casting, aluminum alloy castings and manufacturing method thereof
    4.
    发明申请
    Aluminum alloys for casting, aluminum alloy castings and manufacturing method thereof 有权
    铸铝用合金,铝合金铸件及其制造方法

    公开(公告)号:US20050100473A1

    公开(公告)日:2005-05-12

    申请号:US10965293

    申请日:2004-10-14

    CPC分类号: C22C21/02 C22F1/043

    摘要: Aluminum alloys and castings are provided that have excellent practical fatigue resistances. The alloy includes, based upon 100 mass %, 4-12 mass % of Si, less than 0.2 mass % of Cu, 0.1-0.5 mass % of Mg, 0.2-3.0 mass % of Ni, 0.1-0.7 mass % of Fe, 0.15-0.3 mass % of Ti, and the balance of aluminum (Al) and impurities. The alloy has a metallographic structure, which includes a matrix phase primarily of α-Al and a skeleton phase crystallizing around the matrix phase in a network shape. The matrix phase is strengthened by precipitates containing Mg. Because of the strengthened matrix phase, and the skeleton phase that surrounds it, the castings have high strength, high fatigue strength, and high thermo-mechanical fatigue resistance.

    摘要翻译: 提供具有优异的实际耐疲劳性的铝合金和铸件。 合金的含量为100质量%,Si:4〜12质量%,Cu:0.2质量%以下,Mg:0.1〜0.5质量%,Ni:0.2〜3.0质量%,Fe:0.1-0.7质量% 0.15-0.3质量%的Ti,余量为铝(Al)和杂质。 该合金具有金相结构,其包括主要为α-Al的基体相和以网状形式围绕基体相结晶的骨架相。 通过含有Mg的析出物强化了基体相。 由于强化的基体相以及其周围的骨架相,铸件具有高强度,高疲劳强度和高耐机械疲劳性能。

    Aluminum alloys for casting and aluminum alloy castings
    6.
    发明授权
    Aluminum alloys for casting and aluminum alloy castings 有权
    铝合金铸造和铝合金铸件

    公开(公告)号:US07959856B2

    公开(公告)日:2011-06-14

    申请号:US10965293

    申请日:2004-10-14

    IPC分类号: C22C21/04

    CPC分类号: C22C21/02 C22F1/043

    摘要: Aluminum alloys and castings are provided that have excellent practical fatigue resistances. The alloy includes, based upon 100 mass %, 4-12 mass % of Si, less than 0.2 mass % of Cu, 0.1-0.5 mass % of Mg, 0.2-3.0 mass % of Ni, 0.1-0.7 mass % of Fe, 0.15-0.3 mass % of Ti, and the balance of aluminum (Al) and impurities. The alloy has a metallographic structure, which includes a matrix phase primarily of α-Al and a skeleton phase crystallizing around the matrix phase in a network shape. The matrix phase is strengthened by precipitates containing Mg. Because of the strengthened matrix phase, and the skeleton phase that surrounds it, the castings have high strength, high fatigue strength, and high thermo-mechanical fatigue resistance.

    摘要翻译: 提供具有优异的实际耐疲劳性的铝合金和铸件。 合金的含量为100质量%,Si:4〜12质量%,Cu:0.2质量%以下,Mg:0.1〜0.5质量%,Ni:0.2〜3.0质量%,Fe:0.1-0.7质量% 0.15-0.3质量%的Ti,余量为铝(Al)和杂质。 该合金具有金相结构,其包括主要为α-Al的基体相和以网状形式围绕基体相结晶的骨架相。 通过含有Mg的析出物强化了基体相。 由于强化的基体相以及其周围的骨架相,铸件具有高强度,高疲劳强度和高耐机械疲劳性能。

    CAST ALUMINUM ALLOY EXCELLENT IN RELAXATION RESISTANCE PROPERTY AND METHOD OF HEAT-TREATING THE SAME
    7.
    发明申请
    CAST ALUMINUM ALLOY EXCELLENT IN RELAXATION RESISTANCE PROPERTY AND METHOD OF HEAT-TREATING THE SAME 审中-公开
    耐蚀铝合金优良耐热性能及其加热方法

    公开(公告)号:US20080000561A1

    公开(公告)日:2008-01-03

    申请号:US11769290

    申请日:2007-06-27

    IPC分类号: C22F1/043 C22C21/04

    CPC分类号: C22C21/04

    摘要: A cast aluminum alloy excellent in the relaxation resistance property, comprising 9 to 17% by mass of Si, 3 to 6% by mass of Cu, 0.2 to 1.2% by mass of Mg, 0.2 to 1.5% by mass of Fe, 0.1 to 1% by mass of Mn, a balance consists of Al and unavoidable impurities, wherein a Ni content is not more than 0.5% by mass. The average hardness is adjusted to HV130 to HV160 by performing, after casting, solution heating by retaining the alloy at a treatment temperature of 450 to 510° C. for 0.5 hour or longer, performing water quenching and, thereafter, performing aging treatment by retaining the alloy at a treatment temperature of 170 to 230° C. for 1 to 24 hours.

    摘要翻译: 耐弛豫性优异的铸铝合金,含有9〜17质量%的Si,3〜6质量%的Cu,0.2〜1.2质量%的Mg,0.2〜1.5质量%的Fe,0.1〜 1质量%的Mn,余量由Al和不可避免的杂质组成,其中Ni含量不超过0.5质量%。 通过在450〜510℃的处理温度下保持合金0.5小时以上进行浇铸后的溶液加热,将平均硬度调整为HV130〜HV160,进行水淬,然后通过保持 该合金在处理温度为170〜230℃下进行1〜24小时。

    Compressor
    8.
    发明申请
    Compressor 审中-公开
    压缩机

    公开(公告)号:US20080006149A1

    公开(公告)日:2008-01-10

    申请号:US11824858

    申请日:2007-07-03

    IPC分类号: F02F7/00

    摘要: A compressor having a housing formed by a plurality of housing members that are connected together is disclosed. The compressor is configured in such a manner that refrigerant is compressed in the housing and discharged to the exterior. Each of the housing members contains 9 to 17 percent by mass of Si, 3.5 to 6 percent by mass of Cu, 0.2 to 1.2 percent by mass of Mg, 0.2 to 1.5 percent by mass of Fe, 0 to 1 percent by mass of Mn, 0.5 percent by mass or less of Ni, and a remaining portion containing Al and unavoidable impurities. It is preferred that the average hardness of each housing member is adjusted to HV130 to HV170 through solution heating in which the housing member is maintained at the treatment temperature of 450° C. to 510° C. for 0.5 hours or longer, followed by water quenching, and then by aging treatment in which the housing member is maintained at the treatment temperature of 170° C. to 230° C. for one to twenty-four hours after the c housing member is cast.

    摘要翻译: 公开了一种压缩机,其具有由连接在一起的多个壳体构件形成的壳体。 压缩机构造成使得制冷剂在壳体中被压缩并排放到外部。 每个壳体中含有9〜17质量%的Si,3.5〜6质量%的Cu,0.2〜1.2质量%的Mg,0.2〜1.5质量%的Fe,0〜1质量%的Mn ,0.5质量%以下的Ni,剩余部分含有Al和不可避免的杂质。 优选地,通过溶液加热将每个壳体构件的平均硬度调节至HV130至HV170,其中壳体构件在450℃至510℃的处理温度下保持0.5小时或更长时间,然后是水 淬火,然后通过老化处理,其中壳体构件被保持在处理温度为170℃至230℃,在c壳体构件被铸造之后一到二十四小时。