公开(公告)号:US5392375A
公开(公告)日:1995-02-21
申请号:US103130
申请日:1993-08-09
申请人: Naoyuki Kitamura , Kenichi Kinugawa , Jun Matsuoka , Kohei Fukumi , Isao Kondoh , Saburo Kose , Hiroshi Yamashita , Makoto Kinoshita
发明人: Naoyuki Kitamura , Kenichi Kinugawa , Jun Matsuoka , Kohei Fukumi , Isao Kondoh , Saburo Kose , Hiroshi Yamashita , Makoto Kinoshita
IPC分类号: C03B19/06 , C03B32/00 , C03B37/012 , G02B6/18
CPC分类号: C03B37/012 , C03B19/06 , C03B32/00
摘要: A process for producing a glass having a rod refractive index distribution, which includes pressing a glass at a temperature below the glass transition temperature to form a glass having a density increased towards the surface layer thereof, or alternatively includes heating a glass at a temperature around the transition temperature at the lowest to prepare glass having a uniformly enhanced density and heating the treated glass under a pressure lower than the applied pressure at a temperature below the glass transition temperature of the glass to prepare a rod glass having a density increased towards the central portion.
摘要翻译: 一种制造具有棒折射率分布的玻璃的方法,其包括在低于玻璃化转变温度的温度下压制玻璃以形成具有朝其表面层增加的密度的玻璃,或者可选地包括在周围的温度下加热玻璃 转变温度最低以制备具有均匀增强密度的玻璃,并且在低于玻璃化转变温度的温度的压力下,在低于施加压力的压力下加热处理过的玻璃,以制备密度朝向中心的密度增加的棒状玻璃 一部分。
-
2.
公开(公告)号:US5261938A
公开(公告)日:1993-11-16
申请号:US13554
申请日:1992-12-16
申请人: Naoyuki Kitamura , Kenichi Kinugawa , Jun Matsuoka , Kohei Fukumi , Isao Kondoh , Saburo Kose , Hiroshi Yamashita , Makoto Kinoshita
发明人: Naoyuki Kitamura , Kenichi Kinugawa , Jun Matsuoka , Kohei Fukumi , Isao Kondoh , Saburo Kose , Hiroshi Yamashita , Makoto Kinoshita
IPC分类号: C03B19/06 , C03B32/00 , C03B37/012 , C03B37/075
CPC分类号: C03B37/012 , C03B19/06 , C03B32/00
摘要: A process for producing a rod glass having a refractive index distribution, which includes pressing a glass at a temperature below the glass transition temperature to form a glass having a density increased towards the surface layer thereof, or alternatively includes heating a glass at a temperature around the transition temperature at the lowest to prepare glass having a uniformly enhanced density and heating the treated glass under a pressure lower than the applied pressure at a temperature below the glass transition temperature of the glass to prepare a glass having a density increased towards the central portion.
摘要翻译: 一种制造具有折射率分布的棒状玻璃的方法,其包括在低于玻璃化转变温度的温度下压制玻璃以形成具有朝向其表面层增加的密度的玻璃,或者可选地包括在周围的温度下加热玻璃 过渡温度最低以制备具有均匀增强密度的玻璃,并且在低于玻璃化转变温度的温度的压力下,在低于施加压力的压力下加热处理的玻璃,以制备密度朝向中心部分增加的玻璃 。
-
公开(公告)号:US5139899A
公开(公告)日:1992-08-18
申请号:US654109
申请日:1991-02-12
摘要: The present invention discloses a lithium ion conductive glass electrolyte including a cationic component and an anionic component, the cationic component including (A) a lithium ion, (B) alkaline earth metal ions and (C) alkali metal ions other than lithium in a percentage composition falling within a region enclosed by the straight lines formed by connecting, in an ionic ratio diagram, points of A(60, 10, 30), B(70, 0, 30), C(40, 0, 60) and D(40, 10, 50) in order, the anionic component being at least one halide ion selected from among chloride, bromide and iodide ions.
摘要翻译: 本发明公开了一种阳离子成分和阴离子成分的锂离子传导性玻璃电解质,所述阳离子成分包含(A)锂离子,(B)碱土类金属离子和(C)除锂以外的碱金属离子, A(60,10,30),B(70,0,30),C(40,0,60)和D(60)的点连接形成的直线形成的区域内的成分 (40,10,50),阴离子组分为选自氯离子,溴化物和碘离子中的至少一种卤离子。
-
-