Propylene-based polymer composition, use thereof, and method for producing thermoplastic polymer composition
    1.
    发明授权
    Propylene-based polymer composition, use thereof, and method for producing thermoplastic polymer composition 有权
    丙烯系聚合物组合物,其用途,热塑性聚合物组合物的制造方法

    公开(公告)号:US08802779B2

    公开(公告)日:2014-08-12

    申请号:US11643944

    申请日:2006-12-22

    IPC分类号: C08L23/00 C08L23/04

    摘要: The propylene-based polymer composition of the present invention includes 41 to 95 parts by weight of a propylene-based polymer (A) having a Tm measured by DSC of not less than 120° C. and not more than 170° C., and 59 to 5 parts by weight (provided that the total of (A) and (B) is 100 parts by weight) of a propylene/ethylene/α-olefin copolymer (B) that contains 84.0 to 60.0 mol % of constitutional units derived from propylene, 15.0 to 30.0 mol % of constitutional units derived from ethylene, and 1.0 to 10.0 mol % of constitutional units derived from an α-olefin having 4 to 20 carbon atoms and has a B-value of not less than 0.9 and not more than 1.5. This polymer composition is excellent in transparency, low-temperature impact resistance, and mechanical properties (flexibility or rigidity, etc.) and also excellent in heat resistance.

    摘要翻译: 本发明的丙烯类聚合物组合物包含41〜95重量份的通过DSC测定的Tm为120℃以上且170℃以下的丙烯系聚合物(A), 59〜5重量份(式(A)和(B)为100重量份)的丙烯/乙烯/α-烯烃共聚物(B)的含量为84.0〜60.0摩尔% 丙烯,来自乙烯的结构单元为15.0〜30.0摩尔%,来自碳原子数4〜20的α-烯烃的结构单元为1.0〜10.0摩尔%,B值为0.9以上且不大于 1.5。 该聚合物组合物的透明性,耐低温冲击性,机械特性(柔软性,刚性等)优异,耐热性优异。

    Propylene-based polymer composition, use thereof, and method for producing thermpolastic polymer composition
    2.
    发明申请
    Propylene-based polymer composition, use thereof, and method for producing thermpolastic polymer composition 有权
    丙烯类聚合物组合物,其用途,以及制备热弹性聚合物组合物的方法

    公开(公告)号:US20080085977A1

    公开(公告)日:2008-04-10

    申请号:US11643944

    申请日:2006-12-22

    IPC分类号: C08L23/12

    摘要: The propylene-based polymer composition of the present invention includes 41 to 95 parts by weight of a propylene-based polymer (A) having a Tm measured by DSC of not less than 120° C. and not more than 170° C., and 59 to 5 parts by weight (provided that the total of (A) and (B) is 100 parts by weight) of a propylene/ethylene/α-olefin copolymer (B) that contains 84.0 to 60.0 mol % of constitutional units derived from propylene, 15.0 to 30.0 mol % of constitutional units derived from ethylene, and 1.0 to 10.0 mol % of constitutional units derived from an α-olefin having 4 to 20 carbon atoms and has a B-value of not less than 0.9 and not more than 1.5. This polymer composition is excellent in transparency, low-temperature impact resistance, and mechanical properties (flexibility or rigidity, etc.) and also excellent in heat resistance.

    摘要翻译: 本发明的丙烯类聚合物组合物包含41〜95重量份的通过DSC测定的Tm为120℃以上且170℃以下的丙烯系聚合物(A), 59〜5重量份(条件是(A)和(B)的总和为100重量份)的丙烯/乙烯/α-烯烃共聚物(B)的含量为84.0〜60.0摩尔% 丙烯,来自乙烯的结构单元为15.0〜30.0摩尔%,衍生自碳原子数4〜20的α-烯烃的结构单元为1.0〜10.0摩尔%,B值为0.9以上且不大于 1.5。 该聚合物组合物的透明性,耐低温冲击性,机械特性(柔软性,刚性等)优异,耐热性优异。

    α-olefin-based polymer composition, molded product formed from the composition, and novel polymer
    3.
    发明授权
    α-olefin-based polymer composition, molded product formed from the composition, and novel polymer 有权
    基于α-烯烃的聚合物组合物,由该组合物形成的模塑产品和新型聚合物

    公开(公告)号:US07847040B2

    公开(公告)日:2010-12-07

    申请号:US11578972

    申请日:2005-04-08

    IPC分类号: C08F4/48

    摘要: A composition having excellent transparency, flexibility, rubber elasticity, thermal resistance, impact resistance, abrasion resistance and the like, a composition having excellent rigidity and impact resistance as well as excellently balanced in whitening resistance, abrasion resistance and heat sealability, and a composition having excellent rubbery properties, thermal resistance, abrasion resistance and flexibility are provided.A composition comprising a specific propylene•α-olefin copolymer for which, in a signal chart measured by 13C-NMR and predetermined such that the peak present at the highest magnetic field among the signals originating from CH (methine) of the constituent unit derived from an α-olefin having 4 to 20 carbon atoms is to be at 34.4 ppm, an absorption intensity A at about 22.0 to 20.9 ppm and an absorption intensity B at about 19.0 to 20.6 ppm satisfy the following relational expressions (i) and (ii) with respect to an absorption intensity C at about 19.0 to 22.0 ppm, which is assignable to propylene methyl: (A/C)×100≦8  (i), and (B/C)×100≧60  (ii), a molded product thereof, and the α-olefin-based copolymer are provided.

    摘要翻译: 具有优异的透明性,柔软性,橡胶弹性,耐热性,耐冲击性,耐磨性等的组合物,具有优异的刚性和耐冲击性以及优异的耐白度,耐磨性和热封性均衡的组合物和具有 提供优异的橡胶性能,耐热性,耐磨性和柔韧性。 一种包含特定丙烯-α-烯烃共聚物的组合物,其以13 C-NMR测量的信号图表示,并且预先确定来自源自该构成单元的CH(次甲基)的CH(次甲基)的信号中的最高磁场存在的峰 具有4至20个碳原子的α-烯烃应为34.4ppm,约22.0至20.9ppm的吸收强度A和约19.0至20.6ppm的吸收强度B满足以下关系式(i)和(ii) (A / C)×100≦̸ 8(i)和(B / C)×100≥60(ii))中的约19.0〜22.0ppm的吸收强度C, 其产物和α-烯烃基共聚物。

    Alpha-Olefin-Based Polymer Composition, Molded Product Formed From the Composition, and Novel Polymer
    5.
    发明申请
    Alpha-Olefin-Based Polymer Composition, Molded Product Formed From the Composition, and Novel Polymer 有权
    基于α-烯烃的聚合物组合物,由组合物形成的成型产品和新型聚合物

    公开(公告)号:US20070225431A1

    公开(公告)日:2007-09-27

    申请号:US11578972

    申请日:2005-04-08

    IPC分类号: C08L23/16 C08F4/64 C08L23/00

    摘要: A composition having excellent transparency, flexibility, rubber elasticity, thermal resistance, impact resistance, abrasion resistance and the like, a composition having excellent rigidity and impact resistance as well as excellently balanced in whitening resistance, abrasion resistance and heat sealability, and a composition having excellent rubbery properties, thermal resistance, abrasion resistance and flexibility are provided. A composition comprising a specific propylene•α-olefin copolymer for which, in a signal chart measured by 13C-NMR and predetermined such that the peak present at the highest magnetic field among the signals originating from CH (methine) of the constituent unit derived from an α-olefin having 4 to 20 carbon atoms is to be at 34.4 ppm, an absorption intensity A at about 22.0 to 20.9 ppm and an absorption intensity B at about 19.0 to 20.6 ppm satisfy the following relational expressions (i) and (ii) with respect to an absorption intensity C at about 19.0 to 22.0 ppm, which is assignable to propylene methyl: (A/C)×100≦8  (i), and (B/C)×100≧60  (ii), a molded product thereof, and the α-olefin-based copolymer are provided.

    摘要翻译: 具有优异的透明性,柔软性,橡胶弹性,耐热性,耐冲击性,耐磨性等的组合物,具有优异的刚性和耐冲击性以及优异的耐白度,耐磨性和热封性均衡的组合物和具有 提供优异的橡胶性能,耐热性,耐磨性和柔韧性。 一种包含特定丙烯-α-烯烃共聚物的组合物,其在通过13 C-NMR测量的信号图中预定使得在来自CH的信号中存在于最高磁场的峰( 来自具有4〜20个碳原子的α-烯烃的构成单元的重量比为34.4ppm,约22.0〜20.9ppm的吸收强度A和约19.0〜20.6ppm的吸收强度B满足以下关系式 表示(i)和(ii)关于在约19.0至22.0ppm处的吸收强度C,其可分配给丙烯甲基:<?在线公式描述=“在线公式”end =“lead”? >(A / C)x100 <= 8(i)和<?在线公式描述=“在线公式”end =“tail”?> <?in-line-formula description =“In-line 公式“end =”lead“?>(B / C)x100> = 60(ii),<?in-line-formula description =”In-line Formulas“end =”tail“?>其成型产品, 提供了α-烯烃基共聚物。