Method for producing nano-carbon materials
    1.
    发明申请
    Method for producing nano-carbon materials 失效
    生产纳米碳材料的方法

    公开(公告)号:US20050079119A1

    公开(公告)日:2005-04-14

    申请号:US10762343

    申请日:2004-01-23

    摘要: A method for producing nano-carbon materials, having a step wherein a starting material comprising one or more kinds of compounds selected from the group consisting saturated hydrocarbons, unsaturated hydrocarbons, saturated cyclic hydrocarbons, and alcohols whose atomic ratio of the component carbon to the component oxygen is more than 2.0 and a catalyst are together treated at a temperature in a range of from 100 to 800° C. while being compressed at a pressure in a range of from 0.2 to 60 MPa, where said starting material is converted into a supercritical fluid or a subcritical fluid while said supercritical fluid or said subcritical fluid being contacted with said catalyst, or a step wherein said starting material, said catalyst and a supplementary material capable of functioning as a reaction promotion medium are together treated at a temperature in a range of from 100 to 800° C. while being compressed at a pressure in a range of from 0.2 to 60 MPa, where at least said supplementary material is converted into a supercritical fluid or a subcritical fluid and said starting material is contacted with said supercritical fluid or said subcritical fluid formed from said supplementary material while being contacted with said catalyst.

    摘要翻译: 一种纳米碳材料的制造方法,其特征在于,具有含有一种或多种选自饱和烃,不饱和烃,饱和环状烃以及成分碳与成分的原子比的醇的原料的工序 氧气大于2.0,并且催化剂在100至800℃的温度下一起处理,同时在0.2至60MPa的压力下压缩,其中所述起始材料转化为超临界 流体或亚临界流体,同时所述超临界流体或所述亚临界流体与所述催化剂接触,或者其中所述起始材料,所述催化剂和能够用作反应促进介质的辅助材料的步骤一起在一定范围内的温度 在100至800℃的压力下进行压缩,同时在0.2至60MPa的压力下进行压缩,至少在所述补充物中 原料被转化为超临界流体或亚临界流体,并且所述原料在与所述催化剂接触的同时与所述超临界流体或由所述辅助材料形成的所述亚临界流体接触。