Lubricant coated beverage container or conveyor therefor
    3.
    发明授权
    Lubricant coated beverage container or conveyor therefor 有权
    润滑涂层饮料容器或输送机

    公开(公告)号:US07067182B2

    公开(公告)日:2006-06-27

    申请号:US10260444

    申请日:2002-09-27

    IPC分类号: C08J7/04

    摘要: The passage of a container along a conveyor is lubricated by applying to the container or conveyor a lubricating coating that is thermally cured at less than 200° C. or radiation-cured. The mixture can be applied in relatively low amounts and with relatively low or no water content, to provide thin, substantially non-dripping, renewable lubricating films. In contrast to dilute aqueous lubricants, the lubricants of the invention provide dry lubrication of the conveyors and containers, a cleaner conveyor line and reduced lubricant usage, thereby reducing waste, cleanup and disposal problems.

    摘要翻译: 通过向容器或传送器施加在小于200℃下热固化或辐射固化的润滑涂层来润滑容器沿输送机的通道。 该混合物可以以相对低的量施用,相对较低或不含水量,以提供薄的,基本上不滴落的可再生润滑膜。 与稀释的含水润滑剂相反,本发明的润滑剂提供输送机和容器的干润滑,清洁的输送线和减少的润滑剂使用,从而减少浪费,清理和处理问题。

    Polyurethane coating cure enhancement using zinc carbonate initiators
    4.
    发明授权
    Polyurethane coating cure enhancement using zinc carbonate initiators 有权
    使用碳酸锌引发剂的聚氨酯涂层固化增强

    公开(公告)号:US07655718B2

    公开(公告)日:2010-02-02

    申请号:US10755976

    申请日:2004-01-12

    IPC分类号: B05D3/02 C08K3/00

    摘要: Zinc carbonates such as carbonic acid zinc salt, zinc carbonate hydroxide monohydrate, zinc bicarbonate, zinc tetraamine carbonate, zinc ammonium carbonate, carbamic acid zinc salt and zinc carbamate can initiate hardening of polyurethane coatings and decrease the coating tack-free time. The decreased tack-free times facilitate earlier application of additional polyurethane layers and earlier return of a coated article to service, and can provide improved floor finishes.

    摘要翻译: 碳酸锌如碳酸锌盐,碳酸氢氧化锌一水合物,碳酸氢锌,四胺碳酸锌,碳酸锌铵,氨基甲酸锌盐和氨基甲酸锌可以引发聚氨酯涂层的硬化,并降低涂层的无粘性时间。 降低的无粘性时间有利于更早地应用额外的聚氨酯层,并且早期使涂层制品返回使用,并且可以提供改进的地板饰面。

    Method for stripping floor finishes using composition that thickens upon dilution with water
    5.
    发明授权
    Method for stripping floor finishes using composition that thickens upon dilution with water 有权
    使用在用水稀释时增稠的组合物剥离地板表面处理的方法

    公开(公告)号:US07365046B2

    公开(公告)日:2008-04-29

    申请号:US11107307

    申请日:2005-04-15

    IPC分类号: C11D17/00

    摘要: A method for stripping a floor using a concentrate prepared by mixing a substantially nonchlorinated concentrate containing a floor finish solvent and an at least partially unactivated water thickener. The concentrate is diluted merely with water at an intended use location to activate the water thickener and noticeably increase within ten minutes or less the viscosity of the resulting mixture, then applied to a hardened floor finish atop a floor and allowed to soften or dissolve the floor finish so that the finish may be removed from the floor.

    摘要翻译: 一种使用通过混合含有地板涂料溶剂和至少部分未活化的水增稠剂的基本上非氯化浓缩物制备的浓缩物来剥离地板的方法。 浓缩物仅在预定的使用位置用水稀释,以激活水增稠剂,并且在10分钟内明显增加所得混合物的粘度,然后施加到地板顶部的硬化地板上并允许软化或溶解地板 完成,以便完成可以从地板上移除。

    Jobsite-renewable multilayer floor finish with enhanced hardening rate
    8.
    发明授权
    Jobsite-renewable multilayer floor finish with enhanced hardening rate 有权
    工作现场可再生多层地板,增强硬化率

    公开(公告)号:US07527861B2

    公开(公告)日:2009-05-05

    申请号:US10756119

    申请日:2004-01-12

    IPC分类号: B32B9/04 B35D1/38

    摘要: A jobsite-renewable multilayer floor finish system has an undercoat employing a first hardening system, an autohardenable (e.g., two-part) topcoat employing a second hardening system, and at least one initiator for the topcoat hardening system in at least the undercoat. The initiator increases the topcoat hardening rate while reducing the topcoat pot life to a lesser extent than would be the case if the initiator were included only in the topcoat. The increased topcoat hardening rate facilitates earlier application of additional topcoat layers, or earlier return of the floor to service.

    摘要翻译: 现场可再生的多层地板整理系统具有使用第一硬化系统的底层,使用第二硬化系统的可自动硬化(例如两部分)面漆,以及至少在底涂层中用于顶涂层硬化系统的至少一种引发剂。 如果引发剂仅包括在面漆中,引发剂会增加表面涂层硬化率,同时将面漆的适用期限降低到比较少的程度。 增加的表面涂层硬化率有助于更早地应用额外的顶涂层,或者更早地返回地板以服务。