Negative electrode material for lithium secondary batteries
    1.
    发明授权
    Negative electrode material for lithium secondary batteries 失效
    锂二次电池用负极材料

    公开(公告)号:US5958622A

    公开(公告)日:1999-09-28

    申请号:US824294

    申请日:1997-03-26

    IPC分类号: H01M4/02 H01M4/58 H01M4/587

    摘要: A negative electrode material capable of absorbing and desorbing lithium is comprised of a mixture of coke and graphite. The amount of graphite in the mixture is near to that which induces percolation transition. Preferably, the amount of graphite in the mixture is 2 to 37 wt % relative to the total amount of the coke and graphite. The coke may be prepared by heating raw coke from oil or coal at 500 to 900.degree. C. The coke may be 0.06 or more in the atomic ratio of hydrogen to carbon and 0.003 or more in the atomic ratio of oxygen to carbon. The graphite may be 0.5 .mu.m to 30 .mu.m in a mean particle size. Lithium secondary batteries comprising the negative electrodes have a large discharge capacity.

    摘要翻译: 能够吸收和解吸锂的负极材料由焦炭和石墨的混合物构成。 混合物中石墨的量接近于引起渗透转变的石墨。 优选地,混合物中石墨的量相对于焦炭和石墨的总量为2〜37重量%。 焦炭可以通过在500〜900℃下从油或煤中加热原焦炭来制备。焦炭可以以氢与碳的原子比为0.06以上,氧与碳的原子比为0.003以上。 石墨的平均粒径可以为0.5〜30μm。 包括负极的锂二次电池具有大的放电容量。

    BLADE AND LAMINATED PROTECTIVE SHEET FOR THE BLADE
    3.
    发明申请
    BLADE AND LAMINATED PROTECTIVE SHEET FOR THE BLADE 有权
    叶片的叶片和层压保护片

    公开(公告)号:US20130101426A1

    公开(公告)日:2013-04-25

    申请号:US13807127

    申请日:2012-01-25

    IPC分类号: F03D1/06

    摘要: A scratch-resistant blade such as an FRP wind turbine blade and a blade protective sheet which can be easily repaired when scratched. A blade is provided with a laminated protective sheet bonded to at least part of a leading edge of an FRP blade body of said blade, wherein the laminated protective sheet comprises an adhesive layer, a intermediate fabric layer and a durable surface layer, in that order from the blade body.

    摘要翻译: FRP风力涡轮机叶片等刮伤刀片和刮伤时易于维修的刀片保护片。 叶片设置有粘合到所述叶片的FRP叶片体的前缘的至少一部分的层压保护片,其中所述层压保护片按顺序包括粘合剂层,中间织物层和耐用的表面层 从刀片体。

    Network control device and control method
    4.
    发明授权
    Network control device and control method 有权
    网络控制装置及控制方法

    公开(公告)号:US07843953B2

    公开(公告)日:2010-11-30

    申请号:US11641682

    申请日:2006-12-20

    IPC分类号: H04L12/28 G06F1/26 G06F1/32

    CPC分类号: H04L12/4625 G03G15/5004

    摘要: A network control device that has a packet filtering unit for implementing packet filtering based on prescribed information in a header of a received packet, which includes: a position designating unit that designates a prescribed comparison position in a higher level protocol header to the header of the received packet; and an additional determination unit that implements pattern matching filtering by comparing data at the comparison position designated by the position designating unit with preset data.

    摘要翻译: 一种网络控制装置,具有:基于接收到的分组的报头中的规定信息进行分组过滤的分组过滤单元,其包括:位置指定单元,其将上位协议报头中的规定比较位置指定到 收到包; 以及附加确定单元,其通过将由位置指定单元指定的比较位置处的数据与预设数据进行比较来实现模式匹配滤波。

    Conductive film, corrosion-resistant conduction film, corrosion-resistant conduction Material and process for producing the same
    5.
    发明申请
    Conductive film, corrosion-resistant conduction film, corrosion-resistant conduction Material and process for producing the same 有权
    导电膜,耐腐蚀导电膜,耐腐蚀导电材料及其制造方法

    公开(公告)号:US20100200120A1

    公开(公告)日:2010-08-12

    申请号:US12656459

    申请日:2010-01-29

    IPC分类号: C23C8/24 B32B9/00 H01B1/02

    摘要: A conductive film comprises a phosphide particle coated film formed by attaching raw material particles including phosphide particles comprising a compound of Ti and/or Fe, and P to a surface of a substrate material. This conductive film exhibits good corrosion resistant conductivity, and can be easily formed at low costs because of comprising the phosphide particle coated film. A corrosion-resistant conduction film comprises an iron-containing titanium phosphide layer containing Ti, Fe and P as essential basic elements. A corrosion-resistant conduction material having this corrosion-resistant conduction film on a surface of a substrate exhibits good corrosion resistance or conductivity. This corrosion-resistant conduction material can be obtained, for example, by a process comprising a plating step of forming an Ni plating layer on a surface of a Ti-based material substrate and a nitriding step of applying nitriding treatment to the Ti-based material substrate after the plating step at not more than 880 deg. C.

    摘要翻译: 导电膜包括通过将包含Ti和/或Fe化合物的磷化物颗粒和P的原料颗粒附着到基材的表面而形成的磷化物颗粒涂布膜。 该导电膜表现出良好的耐腐蚀性导电性,并且由于包含磷化物粒子涂布膜,可以以低成本容易地形成。 耐腐蚀导电膜包括含有Ti,Fe和P作为必需碱性元素的含铁磷化钛层。 在基板表面具有这种耐腐蚀导电膜的耐腐蚀导电材料表现出良好的耐腐蚀性或导电性。 该耐腐蚀导电材料可以通过例如在Ti基材料基板的表面上形成Ni镀层的镀覆工序和对Ti系材料进行氮化处理的氮化工序 电镀步骤后的基板不大于880度。 C。

    Method of forming polycrystalline semiconductor thin film
    8.
    发明授权
    Method of forming polycrystalline semiconductor thin film 失效
    多晶半导体薄膜的形成方法

    公开(公告)号:US6025217A

    公开(公告)日:2000-02-15

    申请号:US561246

    申请日:1995-11-21

    CPC分类号: H01L29/66757 H01L21/2026

    摘要: Method of forming a uniform polycrystalline semiconductor thin film by laser annealing. The method is started with preparing a substrate having an insulating layer which has a relatively low thermal conductivity and a thickness of more than 20 nm. Then, an amorphous silicon thin film having a relatively high thermal conductivity is formed to a thickness of less than 35 nm on the insulating layer. Thereafter, the amorphous silicon thin film is irradiated with laser beam to impart thermal energy to the film. In this way, the amorphous film is converted into a polysilicon thin film. Since the thickness of the amorphous silicon film is less than 35 nm, polysilicons having uniform grain diameters can be grown.

    摘要翻译: 通过激光退火形成均匀多晶半导体薄膜的方法。 该方法开始于制备具有绝热层的基板,该绝缘层具有相对较低的热导率和大于20nm的厚度。 然后,在绝缘层上形成厚度小于35nm的导热率较高的非晶硅薄膜。 此后,用激光束照射非晶硅薄膜,以赋予薄膜热能。 以这种方式,将非晶膜转变为多晶硅薄膜。 由于非晶硅膜的厚度小于35nm,因此可以生长具有均匀粒径的多晶硅。

    Electronic watch
    9.
    发明授权
    Electronic watch 有权
    电子手表

    公开(公告)号:US08841875B2

    公开(公告)日:2014-09-23

    申请号:US13500829

    申请日:2010-10-06

    IPC分类号: H02P8/00 G04C3/14 H02P8/02

    CPC分类号: G04C3/143 H02P8/02

    摘要: Provided is an electronic watch capable of, even if an indicating hand having a large moment of inertia is used, accurately determining success and failure of rotation. The electronic watch detects rotation by using a first detection mode determination circuit (12) and a second detection mode determination circuit (13). In the electronic watch, a timing counter (14) for measuring a time after an output of a normal drive pulse is followed by a detection pulse selection circuit (151) provided as changing means for changing a width or a frequency of a detection pulse in accordance with an output time of the detection pulse. The detection pulse detects the rotation and simultaneously serves as an electromagnetic brake for a rotor (10). The electromagnetic brake for the rotor (10) is controlled by changing the width or the frequency of the detection pulse in a predetermined period, thereby achieving an accurate rotation detection. Alternatively, the setting of the width or the frequency of the detection pulse may be changed in accordance with a determination result in a first detection mode, an output voltage of a power supply, and a driving power of the normal drive pulse, instead of the output timing of the detection pulse.

    摘要翻译: 提供一种能够即使具有大惯性矩的指示手也能够精确地确定旋转成功和失败的电子手表。 电子表通过使用第一检测模式确定电路(12)和第二检测模式确定电路(13)检测旋转。 在电子表中,用于测量正常驱动脉冲输出之后的时间的定时计数器(14)后面是检测脉冲选择电路(151),该检测脉冲选择电路(151)被设置为改变装置,用于改变检测脉冲的宽度或频率 根据检测脉冲的输出时间。 检测脉冲检测旋转,同时用作转子(10)的电磁制动器。 用于转子(10)的电磁制动器通过在预定时间段内改变检测脉冲的宽度或频率来控制,从而实现精确的旋转检测。 或者,可以根据第一检测模式,电源的输出电压和正常驱动脉冲的驱动功率的确定结果来改变检测脉冲的宽度或频率的设置,而不是 检测脉冲的输出定时。

    Blade and laminated protective sheet for the blade
    10.
    发明授权
    Blade and laminated protective sheet for the blade 有权
    刀片和刀片的层压保护片

    公开(公告)号:US08770942B2

    公开(公告)日:2014-07-08

    申请号:US13807127

    申请日:2012-01-25

    IPC分类号: F01D5/28 F03D11/00

    摘要: A scratch-resistant blade such as an FRP wind turbine blade and a blade protective sheet which can be easily repaired when scratched. A blade is provided with a laminated protective sheet bonded to at least part of a leading edge of an FRP blade body of said blade, wherein the laminated protective sheet comprises an adhesive layer, a intermediate fabric layer and a durable surface layer, in that order from the blade body.

    摘要翻译: FRP风力涡轮机叶片等刮伤刀片和刮伤时易于维修的刀片保护片。 叶片设置有粘合到所述叶片的FRP叶片体的前缘的至少一部分的层压保护片,其中所述层压保护片按顺序包括粘合剂层,中间织物层和耐用的表面层 从刀片体。