摘要:
The present invention relates to a positive bottom photoimageable antireflective coating composition which is capable of being developed in an aqueous alkaline developer, wherein the antireflective coating composition comprises a polymer comprising at least one recurring unit with a chromophore group and one recurring unit with a hydroxyl and/or a carboxyl group, a vinyl ether terminated crosslinking agent, and optionally, a photoacid generator and/or an acid and/or a thermal acid generator. The invention further relates to a process for using such a composition.
摘要:
The present invention relates to a positive bottom photoimageable antireflective coating composition which is capable of being developed in an aqueous alkaline developer, wherein the antireflective coating composition comprises a polymer comprising at least one recurring unit with a chromophore group and one recurring unit with a hydroxyl and/or a carboxyl group, a vinyl ether terminated crosslinking agent, and optionally, a photoacid generator and/or an acid and/or a thermal acid generator. The invention further relates to a process for using such a composition.
摘要:
The present invention relates to a positive bottom photoimageable antireflective coating composition which is capable of being developed in an aqueous alkaline developer, wherein the antireflective coating composition comprises a polymer comprising at least one recurring unit with a chromophore group and one recurring unit with a hydroxyl and/or a carboxyl group, a vinyl ether terminated crosslinking agent, and optionally, a photoacid generator and/or an acid and/or a thermal acid generator. The invention further relates to a process for using such a composition.
摘要:
Disclosed is a process for forming an image on a substrate, comprising the steps of: (a) coating on the substrate a first layer of a radiation sensitive, antireflective composition; (b) coating a second layer of a photoresist composition onto the first layer of the antireflective composition; (c) selectively exposing the coated substrate from step (b) to actinic radiation; and (d) developing the exposed coated substrate from step (c) to form an image; wherein both the photoresist composition and the antireflective composition are exposed in step (c); both are developed in step (d) using a single developer; wherein the antireflective composition of step (a) is a first minimum bottom antireflective coating (B.A.R.C.) composition, having a solids content of up to about 8% solids, and a maximum coating thickness of the coated substrate of λ/2n wherein λ is the wavelength of the actinic radiation of step (c) and n is the refractive index of the B.A.R.C. composition.
摘要:
The present invention relates to novel negative-working, photoimageable, and aqueous developable antireflective coating compositions and their use in image processing by forming a thin layer of the novel antireflective coating composition between a reflective substrate and a photoresist coating. The negative bottom photoimageable antireflective coating composition is capable of being developed in an alkaline developer and is coated below a negative photoresist.
摘要:
The present invention relates to a process for making a polyester where a dianhydride is reacted with a diol. The resulting polyester can be further reacted with a compound selected from aromatic oxides, aliphatic oxides, alkylene carbonates, alcohols, and mixtures thereof.
摘要:
The present invention relates to a novel polymeric composition comprising a novel polymer having two or more repeat units and a terminus having the structure (1): wherein R1 represents a C1-C20 substituted or unsubstituted alkyl group, w is a number from 1-8, X is oxygen (O) or nitrogen (N), and Rd is a reactive group. The invention also relates to a process for forming a pattern using the novel polymeric composition. The invention further relates to a process of making the novel polymer.
摘要:
The present invention relates to an antireflective coating composition comprising, (i) a thermal acid generator; (ii) a crosslinkable polymer comprising at least one aromatic group; and, (iii) a polymeric crosslinker comprising at least one unit of structure (6), where R11 to R13 is independently selected from H, (C1-C6) alkyl and aromatic group, R14 and R15 are independently (C1-C10) alkyl. The invention also relates to a process for imaging the antireflective coating composition of the present invention.
摘要:
The present invention relates to an antireflective coating composition comprising, (i) a thermal acid generator; (ii) a crosslinkable polymer comprising at least one aromatic group; and, (iii) a polymeric crosslinker comprising at least one unit of structure (6), where R11 to R13 is independently selected from H, (C1-C6) alkyl and aromatic group, R14 and R15 are independently (C1-C10) alkyl. The invention also relates to a process for imaging the antireflective coating composition of the present invention.
摘要:
The present invention relates to a method for treating a block copolymer solution, wherein the method comprises: providing a solution comprising a block copolymer in a non aqueous solvent; and, treating the solution to remove metals using an ion exchange resin. The invention also relates to a method of forming patterns using the treated block copolymer.