公开(公告)号:US10519598B2
公开(公告)日:2019-12-31
申请号:US14651975
申请日:2013-12-26
发明人: Satoshi Wada , Yuko Okusa , Chigusa Taguchi , Yukio Abe , Michiyasu Yamazaki
摘要: Provided are a pitch-formation suppressor and the like which can be widely applied independently of the substance that causes a pitch and of the situation to generate a pitch in a paper manufacturing process, and which can effectively suppress and prevent the troubles due to the pitch, such as foreign spots and defects in a paper, breakage of a paper, and lowering of workability. This pitch-formation suppressor comprises an alkaline solution in which a phenol resin and/or a modified phenol resin is dissolved, or an acid solution in which a phenol resin and/or a modified phenol resin is dissolved.
-
公开(公告)号:US20040197558A1
公开(公告)日:2004-10-07
申请号:US10816538
申请日:2004-03-31
IPC分类号: B22C009/00
CPC分类号: B22C1/22 , B33Y70/00 , Y10T428/2993 , Y10T428/2998
摘要: The resin-coated sand is produced by coating the surface of a refractory granular aggregate with a thermosetting resin and a thermoplastic resin. When using this resin-coated sand, a mold with a less rough surface can be produced by a RP molding apparatus. When using this mold made of the resin-coated sand, a casting with fewer gas defects can be produced.
摘要翻译: 通过用热固性树脂和热塑性树脂涂覆耐火颗粒状聚集体的表面来制备树脂涂覆的砂。 当使用该树脂涂覆的砂时,可以通过RP成型装置来制造表面粗糙的模具。 当使用由树脂涂覆的砂制成的模具时,可以产生具有较少气体缺陷的铸件。
-
公开(公告)号:US5929191A
公开(公告)日:1999-07-27
申请号:US863583
申请日:1997-05-27
摘要: One of the objects of the present invention is to offer novolak type phenolic resins which use phenols and aldehydes as raw materials and give narrow molecular weight distributions.The novolak type phenolic resins of the present invention are those obtained by condensation reaction of phenols with aldehydes in the presence of an oxycarboxylic acid having carboxyl groups, --COOH, and alcoholic hydroxyl groups, --OH, in one molecule. Thus, obtained novolak type phenolic resins show narrow molecular weight distributions, lower viscosity in molten state and, as a consequence, uniformity in curing time.
摘要翻译: 本发明的目的之一是提供酚醛树脂型酚醛树脂,它们以苯酚和醛为原料,分子量分布窄。 本发明的酚醛清漆型酚醛树脂是通过在一分子中在具有羧基-COOH和醇羟基-OH的羟基羧酸存在下酚与醛的缩合反应得到的酚醛清漆型酚醛树脂。 因此,获得的酚醛清漆型酚醛树脂显示出窄的分子量分布,熔融状态下的粘度较低,因此固化时间的均匀性。
-
公开(公告)号:US2111446A
公开(公告)日:1938-03-15
申请号:US75330434
申请日:1934-11-16
发明人: GLOOR WALTER E
IPC分类号: C09D101/14
CPC分类号: C09D101/14
-
公开(公告)号:US07019045B2
公开(公告)日:2006-03-28
申请号:US11125950
申请日:2005-05-09
CPC分类号: G03F7/023 , C07C215/74 , C07C217/80 , C07C229/52 , C08G73/10 , G03F7/033 , G03F7/0388
摘要: An object of the present invention is to provide a material which resolves the drawbacks associated with polyimide polymers, and yet retains the advantages offered by conventional polyimide polymers.An amino group containing phenol derivative of the present invention is represented by a general formula (1) show below, and the present invention also provides a polyimide precursor produced using such an amino group containing phenol derivative. (wherein, R1, R2 and R3, which may be the same or different, each represent an alkyl group of 1 to 9 carbon atoms, an alkoxy group of 1 to 10 carbon atoms, a COOR group (in which R represents an alkyl group of 1 to 6 carbon atoms) or a hydrogen atom; R4 and R5, which may be the same or different, each represent an alkyl group of 1 to 9 carbon atoms or a hydrogen atom; X represents —O—, —S—, —SO2—, —C(CH3)2—, —CH2—, —C(CH3)(C2H5)—, or —C(CF3)2—; and n represents an integer of 1 or greater).
摘要翻译: 本发明的目的是提供一种解决与聚酰亚胺聚合物有关的缺点的材料,并且仍然保留了常规聚酰亚胺聚合物所提供的优点。 本发明的含氨基的苯酚衍生物由下述通式(1)表示,本发明还提供使用含氨基的苯酚衍生物制造的聚酰亚胺前体。 (其中R 1,R 2,R 3和R 3)可相同或不同,分别表示1〜9的烷基 碳原子,碳原子数1〜10的烷氧基,COOR基(其中,R表示碳原子数为1〜6的烷基)或氢原子; R 4,R 4, 5个可以相同或不同,各自表示1至9个碳原子的烷基或氢原子; X表示-O - , - S - , - SO 2 - , - C(CH 3)2 - , - CH 2 - , - C(CH 3) (C 2 H 5) - 或-C(CF 3)2 - ;且n表示 1或更大的整数)。
-
公开(公告)号:US5859168A
公开(公告)日:1999-01-12
申请号:US753304
申请日:1996-11-22
摘要: One of the objects of the present invention is to offer novolak type phenolic resins which use phenols and aldehydes as raw materials and give narrow molecular weight distributions.The novolak type phenolic resins of the present invention are those obtained by condensation reaction of phenols with aldehydes in the presence of an oxycarboxylic acid having carboxyl groups, --COOH, and alcoholic hydroxyl groups, --OH, in one molecule. Thus obtained novolak type phenolic resins show narrow molecular weight distributions, lower viscosity in molten state and, as a consequence, uniformity in curing time.
摘要翻译: 本发明的目的之一是提供酚醛树脂型酚醛树脂,它们以苯酚和醛为原料,分子量分布窄。 本发明的酚醛清漆型酚醛树脂是通过在一分子中在具有羧基-COOH和醇羟基-OH的羟基羧酸存在下酚与醛的缩合反应得到的酚醛清漆型酚醛树脂。 由此获得的酚醛清漆型酚醛树脂显示出窄的分子量分布,熔融状态下的粘度较低,因此固化时间的均匀性。
-
公开(公告)号:US5230960A
公开(公告)日:1993-07-27
申请号:US653544
申请日:1991-01-07
申请人: Toshi Iizuka
发明人: Toshi Iizuka
CPC分类号: D01F9/24 , D01F9/15 , D01F9/155 , D01F9/21 , Y10S428/902 , Y10T428/2918 , Y10T428/30
摘要: An activated and heat-treated product of a pitch fiber (A) is combined with an activated and heat-treated product of a precursor fiber of carbon fiber (B) having a larger elongation and a larger shrinkage during activation treatment thereof than those of the pitch fiber (A) to provide an activated carbon fiber structure. The activated carbon fiber structure is produced by subjecting the pitch fiber (A) and the precursor fiber of carbon fiber (B) to an activation treatment before or after the fibers (A) and (B) are formed into a configuration corresponding to a fiber structure through mixing or laminating.
-
公开(公告)号:US20060284346A1
公开(公告)日:2006-12-21
申请号:US11502868
申请日:2006-08-11
CPC分类号: B22C1/22 , B33Y70/00 , Y10T428/2993 , Y10T428/2998
摘要: The resin-coated sand is produced by coating the surface of a refractory granular aggregate with a thermosetting resin and a thermoplastic resin. When using this resin-coated sand, a mold with a less rough surface can be produced by a RP molding apparatus. When using this mold made of the resin-coated sand, a casting with fewer gas defects can be produced.
摘要翻译: 通过用热固性树脂和热塑性树脂涂覆耐火颗粒状聚集体的表面来制备树脂涂覆的砂。 当使用该树脂涂覆的砂时,可以通过RP成型装置制造具有较小粗糙表面的模具。 当使用由树脂涂覆的砂制成的模具时,可以产生具有较少气体缺陷的铸件。
-
公开(公告)号:US20050197482A1
公开(公告)日:2005-09-08
申请号:US11125950
申请日:2005-05-09
IPC分类号: C08L79/08 , C07C215/74 , C07C217/80 , C07C229/52 , C08F2/46 , C08G8/28 , C08G73/10 , C08L83/04 , G03F7/023 , G03F7/033 , G03F7/038 , C08G8/02
CPC分类号: G03F7/023 , C07C215/74 , C07C217/80 , C07C229/52 , C08G73/10 , G03F7/033 , G03F7/0388
摘要: An object of the present invention is to provide a material which resolves the drawbacks associated with polyimide polymers, and yet retains the advantages offered by conventional polyimide polymers. An amino group containing phenol derivative of the present invention is represented by a general formula (1) show below, and the present invention also provides a polyimide precursor produced using such an amino group containing phenol derivative. (wherein, R1, R2 and R3, which may be the same or different, each represent an alkyl group of 1 to 9 carbon atoms, an alkoxy group of 1 to 10 carbon atoms, a COOR group (in which R represents an alkyl group of 1 to 6 carbon atoms) or a hydrogen atom; R4 and R5, which may be the same or different, each represent an alkyl group of 1 to 9 carbon atoms or a hydrogen atom; X represents —O—, —S—, —SO2—, —C(CH3)2—, —CH2—, —C(CH3)(C2H5)—, or —C(CF3)2—; and n represents an integer of 1 or greater).
摘要翻译: 本发明的目的是提供一种解决与聚酰亚胺聚合物有关的缺点的材料,并且仍然保留了传统聚酰亚胺聚合物所提供的优点。 本发明的含氨基的苯酚衍生物由下述通式(1)表示,本发明还提供使用含氨基的苯酚衍生物制造的聚酰亚胺前体。 (其中R 1,R 2,R 3和R 3)可相同或不同,分别表示1〜9的烷基 碳原子,碳原子数1〜10的烷氧基,COOR基(其中,R表示碳原子数为1〜6的烷基)或氢原子; R 4,R 4, 5个可以相同或不同,各自表示1至9个碳原子的烷基或氢原子; X表示-O - , - S - , - SO 2 - , - C(CH 3)2 - , - CH 2 - , - C(CH 3) (C 2 H 5) - 或-C(CF 3)2 - ;且n表示 1或更大的整数)。
-
10.
公开(公告)号:US6124420A
公开(公告)日:2000-09-26
申请号:US930892
申请日:1997-12-05
申请人: Kenichi Kuboki , Yoshio Shimamura , Ryoichi Hasegawa , Yoshiaki Kurimoto , Akiyuki Kojima , Yukio Abe
发明人: Kenichi Kuboki , Yoshio Shimamura , Ryoichi Hasegawa , Yoshiaki Kurimoto , Akiyuki Kojima , Yukio Abe
CPC分类号: C08G59/688 , C08G59/08 , C08G59/18 , C08G59/3218 , C08L63/04
摘要: This invention provides a novolak type epoxy resin which has low melt viscosity but shows high heat resistance when hardened. Particularly, it relates to a novolak type epoxy resin in which the relationship between the total % by weight of 3 to 6 nucleus bodies and the melt viscosity measured by a cone plate method at 150.degree. C. satisfies specified conditions, an epoxy resin composition containing the same and hardened products thereof.
摘要翻译: PCT No.PCT / JP97 / 00331 Sec。 371 1997年12月5日第 102(e)日期1997年12月5日PCT提交1997年2月7日PCT公布。 出版物WO97 / 29144 日期:1997年8月14日本发明提供了一种酚醛清漆型环氧树脂,其具有低熔体粘度,但在硬化时显示出高耐热性。 特别涉及一种酚醛清漆型环氧树脂,其中3〜6个核体的总重量%与锥板法在150℃下测定的熔融粘度之间的关系满足规定的条件,含有 其相同和硬化的产品。
-
-
-
-
-
-
-
-
-