Abstract:
A method of forming an asphalt mixture can include mixing a bio-source material and a bitumen source to form a bitumen mixture. The bitumen mixture can be mixed with a catalyst to form the asphalt mixture. Particles can be added to the asphalt mixture to form a roofing-grade asphalt mixture. In an embodiment, the bitumen source material can have a softening point of at least approximately 93° C. and a penetration distance no greater than approximately 25 dmm. In another embodiment, the roofing-grade asphalt mixture can have a softening point of at least approximately 104° C., a penetration distance no greater than approximately 12 dmm, a viscosity of at least approximately 3000 cps at a temperature of 204° C., or any combination thereof. The asphalt mixture can be applied to a base material to form a roofing product. The asphalt mixture can be applied as a pavement product.
Abstract:
A method of forming an asphalt mixture can include mixing a bio-source material and a bitumen source to form a bitumen mixture. The bitumen mixture can be mixed with a catalyst to form the asphalt mixture. Particles can be added to the asphalt mixture to form a roofing-grade asphalt mixture. In an embodiment, the bitumen source material can have a softening point of at least approximately 93° C. and a penetration distance no greater than approximately 25 dmm. In another embodiment, the roofing-grade asphalt mixture can have a softening point of at least approximately 104° C., a penetration distance no greater than approximately 12 dmm, a viscosity of at least approximately 3000 cps at a temperature of 204° C., or any combination thereof. The asphalt mixture can be applied to a base material to form a roofing product. The asphalt mixture can be applied as a pavement product.
Abstract:
A composition and method for making a faced insulation product having an asphalt adhesive layer is provided. The faced insulation product includes a facing layer laminated to a fibrous insulation layer by a waterless asphalt adhesive.
Abstract:
A roofing membrane that includes a blend of thermoplastic polyurethane and petroleum liquid so as to improve the UV stability of the blend without adversely affecting the flexibility of the dried and/or cured blend.
Abstract:
A process for manufacturing fiberboard by preparing a fiber slurry mixture including containing cellulose fibers and water then atomizing a liquid bituminous material, such as asphalt. The liquid bituminous material is atomized by mixing it with a pressurized gas, such as compressed air, forming a mist comprising droplets of bituminous material having a diameter between 20 microns and 50 microns. A water spray solidifies the bituminous material droplets thereby forming bituminous particles which fall into the fiber slurry within the spray chamber. From there the slurry is sheared, dewatered, and dried, forming a finished fiberboard.
Abstract:
A process for manufacturing fiberboard by preparing a fiber slurry mixture including containing cellulose fibers and water then atomizing a liquid bituminous material, such as asphalt. The liquid bituminous material is atomized by mixing it with a pressurized gas, such as compressed air, forming a mist comprising droplets of bituminous material having a diameter between 20 microns and 50 microns. A water spray solidifies the bituminous material droplets thereby forming bituminous particles which fall into the fiber slurry within the spray chamber. From there the slurry is sheared, dewatered, and dried, forming a finished fiberboard.
Abstract:
A process for manufacturing fiberboard by preparing a fiber slurry mixture including containing cellulose fibers and water then atomizing a liquid bituminous material, such as asphalt. The liquid bituminous material is atomized by mixing it with a pressurized gas, such as compressed air, forming a mist comprising droplets of bituminous material having a diameter between 20 microns and 50 microns. A water spray solidifies the bituminous material droplets thereby forming bituminous particles which fall into the fiber slurry within the spray chamber. From there the slurry is sheared, dewatered, and dried, forming a finished fiberboard.
Abstract:
The present invention provides a polymeric composition that includes a coupled block copolymer having a plurality of arms comprising at least two blocks of a monovinylaromatic hydrocarbon that are located on at least two of the plurality of arms, and at least one block of a conjugated diene located on at least one of the plurality of arms, and optionally one or more block copolymers comprising at least one block of monovinylaromatic hydrocarbon and at least one block of a conjugated diene, the block copolymer may be selected from linear copolymers, linear triblock copolymers, multiarm coupled block copolymers, and mixtures thereof. The molecular weight of the polymeric composition is in the range from about 100 kg/mol to about 400 kg/mol.