CROSSLINKED ELASTOMER AND METHOD OF PRODUCING SAME

    公开(公告)号:US20240327547A1

    公开(公告)日:2024-10-03

    申请号:US18574149

    申请日:2022-06-30

    CPC classification number: C08C19/00

    Abstract: Provided is a crosslinked elastomer that can easily be decrosslinked. The crosslinked elastomer is obtained through crosslinking of a diene elastomer that has a vinyl bond content of 30 mass % or less and a weight-average molecular weight of 1,000 or more. The crosslinked elastomer includes a diboronic acid ester skeleton unit represented by a specific general formula (1) at a crosslinking site.

    Production method of modified diene-based polymer

    公开(公告)号:US11787879B2

    公开(公告)日:2023-10-17

    申请号:US17711208

    申请日:2022-04-01

    CPC classification number: C08F8/34 C08F10/08

    Abstract: An object of the present invention is to provide a production method of a diene-based polymer that can control the crosslinking morphology. The present invention provides a method for producing a modified diene-based polymer having a structure represented by the formula (1), comprising a first step of mixing a diene-based polymer and a dithioester compound to prepare a mixture; and a second step of irradiating a ray to the mixture under an inert atmosphere.




    [In the formula (1), R1 and R2 represent an alkyl group having 1 or more carbon atoms, an aryl group having 6 or more carbon atoms, an aralkyl group having 6 or more carbon atoms, a hydrogen atom, or a halogen atom; and Z is an organic group, an organic group where a part of hydrogen atom of the above organic group is substituted, a hydrogen atom, or a halogen atom.]

    Functionalized polymer, rubber composition and pneumatic tire

    公开(公告)号:US11492426B2

    公开(公告)日:2022-11-08

    申请号:US16987521

    申请日:2020-08-07

    Abstract: A functionalized elastomer comprising the reaction product of a living elastomeric polymer and a polymerization terminator of formula I [R1]n—B—[X—R2]m  I where B is boron; X is oxygen or nitrogen; R1 is independently vinyl, oxiranyl, phenyl, 1-alkenyl of 2 to 8 carbon atoms, alkyl of 1 to 8 carbon atoms including at least one halogen atom, 1-alkenyl of 2 to 8 carbon atoms including at least one halogen or one hydrogen; R2 is independently C1 to C8 alkyl, C8 to C14 aryl; or when m>1 R2 may be taken together to form a substituted or unsubstituted cyclic structure comprising 2 to 16 carbon atoms where the cyclic structure may be heterocyclic or non-heterocyclic; n is 1 or 2, m is 1 or 2, and n+m=3.

    CONJUGATED DIENE GRAFT POLYMER AND METHOD FOR PRODUCING THE SAME

    公开(公告)号:US20220289872A1

    公开(公告)日:2022-09-15

    申请号:US17761384

    申请日:2020-09-18

    Abstract: To provide a conjugated diene graft polymer having high transparency, heat resistance and weather resistance, and a method for producing the conjugated diene graft polymer. A method for producing a conjugated diene graft polymer in which a side chain (b) including a polymer including at least one monomer unit selected from the group consisting of a conjugated diene unit and an aromatic vinyl compound unit is bonded to a main chain (a) including a polymer including a conjugated diene unit, via a hetero atom Z serving as a branching point and having a valence of not less than 3, the method including a step of reacting a specific active end polymer and a specific functional group-modified conjugated diene polymer having a functional group in a side chain to thereby produce a conjugated diene graft polymer; and a step of recovering the conjugated diene graft polymer obtained.

    CURABLE LOW SULFUR LIQUID RUBBER COMPOSITIONS

    公开(公告)号:US20200339786A1

    公开(公告)日:2020-10-29

    申请号:US16393493

    申请日:2019-04-24

    Abstract: A curable low sulfur liquid rubber composition including at least one polymer which contains, in polymerized form, at least one monomer having a carbon chain of four and a peroxide system which includes at least one organic peroxide and at least one coagent. The polymer has a vinyl content of 1% to 90% and a number average molecular weight of 800 g/mol to 70,000 g/mol. The curable low sulfur liquid rubber composition has a sulfur content of 0 to 1%, by weight, and is curable at a temperature of 100° C. to 190° C.