Abstract:
A sol comprising a precipitated component in an amount of less than 10 mass% based on the total solid content of the sol and comprising titanium oxide comprising a transition metal compound. When the sol is mixed with a binder which can be hardened at ambient temperature, the mixture readily forms a thin film having high photocatalytic performance on a substrate of poor heat resistance such as plastics or paper. The titanium oxide sol can readily forms titanium oxide thin film on surfaces of a variety of substrate materials such as ceramics, glass, metal, plastics, wood, or paper. Articles to which photocatalytic performance or hydrophilicity is imparted include building materials, fluorescent lamps, glass panes, machinery, vehicles, glass products, household electrical appliances, water purifying apparatuses, agricultural materials, electronic apparatus, tools, tableware, bath products, toiletry products, furniture, clothing, cloth products, fibers, leather products, paper products, sporting goods, beauty-related instruments, health improvement instruments, medical goods, futon, containers, eyeglasses, signboards, piping, wiring, brackets, sanitary materials, and automobile parts as well as environmental purification apparatuses/units.
Abstract:
A metal oxide dispersion comprising metal oxide particles with a necking structure, and a solvent, wherein the liquid droplet contact angle of the metal oxide dispersion to an ITO film (Indium-Tin Oxide type film) formed is from 0 to 60°. A metal oxide dispersion for the production of a dye-sensitized solar cell electrode, comprising Metal Oxide Particle Group F having a necking structure formed by m connected particles, Metal Oxide Particle Group G having only 0.2m or less connected particles, and a solvent, and being formable into a film at 200°C or less. A metal oxide electrode comprising an electrically conducting substrate having thereon a metal oxide layer comprising metal oxide particles bound by a binder, wherein the binder content is from 0.005 to 5 mass% based on the metal oxide film and the metal oxide layer has a pencil scratch strength of H or more according to JIS5600.