发明授权
- 专利标题: MIXED FIBER SPUNBOND NON-WOVEN FABRIC AND METHOD FOR PRODUCTION AND APPLICATION OF THE SAME
- 专利标题(中): 混合纤维纺织非织造和方法进行生产及其用途
-
申请号: EP10806342.1申请日: 2010-07-22
-
公开(公告)号: EP2463428B1公开(公告)日: 2016-07-06
- 发明人: KUNIMOTO, Naosuke
- 申请人: Mitsui Chemicals, Inc.
- 申请人地址: 5-2, Higashi-Shimbashi 1-chome Minato-ku Tokyo 105-7117 JP
- 专利权人: Mitsui Chemicals, Inc.
- 当前专利权人: Mitsui Chemicals, Inc.
- 当前专利权人地址: 5-2, Higashi-Shimbashi 1-chome Minato-ku Tokyo 105-7117 JP
- 代理机构: Hoffmann Eitle
- 优先权: JP2009182673 20090805; JP2010023197 20100204
- 国际公布: WO2011016343 20110210
- 主分类号: D04H3/153
- IPC分类号: D04H3/153 ; D04H3/14 ; A61F13/49 ; A61F13/511 ; A61F13/514 ; D04H3/007 ; D04H3/009 ; A61F13/513 ; D01D5/098 ; D01D5/08 ; D04H3/16
摘要:
It is an object of the present invention to provide a mixed fiber spunbonded nonwoven fabric which has excellent initial hydrophilicity, long-lasting hydrophilicity, liquid dispersibility, liquid transpiration property, moisture permeability, breathability, softness, resistance to fluff, stretchability and touch, and low stickiness, and which is suitable for sheets constituting absorbent articles such as sanitary napkins, panty liners, incontinence pads, and disposable diapers, the example of such sheets including a surface sheet, a second sheet, a sheet for lapping an absorber (core lap), and a back sheet. The present invention provides a mixed fiber spunbonded nonwoven fabric which comprises 90 to 10% by weight of a long fiber of thermoplastic resin (A) that has been hydrophilization-treated and 10 to 90% by weight of a long fiber of thermoplastic elastomer (B) and which has a strength ratio [the ratio of a strength at 20% of an elongation at a maximum strength (elongation at a maximum point) to the maximum strength] in at least one direction of not more than 40% and a bulk density of 0. 10 to 0. 40 g/cm 3 . The present invention also provides a production method thereof.