EP2836637A2 PBO FIBERS WITH IMPROVED MECHANICAL PROPERTIES WHEN EXPOSED TO HIGH TEMPERATURES AND HIGH RELATIVE HUMIDITY
审中-公开
具有改进的机械性能在高温和高相对湿度PBO纤维
- 专利标题: PBO FIBERS WITH IMPROVED MECHANICAL PROPERTIES WHEN EXPOSED TO HIGH TEMPERATURES AND HIGH RELATIVE HUMIDITY
- 专利标题(中): 具有改进的机械性能在高温和高相对湿度PBO纤维
-
申请号: EP13785964.1申请日: 2013-04-11
-
公开(公告)号: EP2836637A2公开(公告)日: 2015-02-18
- 发明人: SAYRE, Jay, R. , MCGINNISS, Vince , TOLBERT, Byron, C. , JENKINS, Kelly, J. , ELLIS, Jeffrey, L. , HUTSON, Tim, B. , ANGEL, Sundee , THURSTON, Rachel
- 申请人: Battelle Memorial Institute
- 申请人地址: 505 King Avenue Columbus, OH 43201 US
- 专利权人: Battelle Memorial Institute
- 当前专利权人: Battelle Memorial Institute
- 当前专利权人地址: 505 King Avenue Columbus, OH 43201 US
- 代理机构: Müller-Boré & Partner Patentanwälte PartG mbB
- 优先权: US201261622638P 20120411
- 国际公布: WO2014011278 20140116
- 主分类号: D06M23/10
- IPC分类号: D06M23/10 ; D06M13/513
摘要:
A method of treating fibers to improve resistance to high temperatures and relative humidity includes providing poly(p-phenylene~2,6-benzobisoxazole) (PBO) fibers, exposing the PBO fibers to an atmosphere of supercritical CO
2 saturated with an epoxy silane, i.e. 3-glycidoxypropyl methyldimethoxysilane. The PBO fibers are subjected to a first pressurizing and heating stage at a first temperature (50°C) for a first period of time. The PBO fibers are then subjected to a second pressurizing and heating stage including increasing the temperature to a second temperature (110°C) and holding at the second temperature for an additional period of time. The PBO fibers include 2-5 wt% of 3-glycidoxypropyl methyldimethoxysilane after diffusing the CO
2 out of the PBO fibers. The fibers are particularly useful in making lightweight body armor system components.
2 saturated with an epoxy silane, i.e. 3-glycidoxypropyl methyldimethoxysilane. The PBO fibers are subjected to a first pressurizing and heating stage at a first temperature (50°C) for a first period of time. The PBO fibers are then subjected to a second pressurizing and heating stage including increasing the temperature to a second temperature (110°C) and holding at the second temperature for an additional period of time. The PBO fibers include 2-5 wt% of 3-glycidoxypropyl methyldimethoxysilane after diffusing the CO
2 out of the PBO fibers. The fibers are particularly useful in making lightweight body armor system components.