发明公开
- 专利标题: ALUMINUM ALLOY MATERIAL FOR HIGH-PRESSURE HYDROGEN GAS CONTAINERS AND METHOD FOR PRODUCING SAME
- 专利标题(中): 用铝合金及其制造高压氢气储气罐和方法
-
申请号: EP13856013.1申请日: 2013-11-18
-
公开(公告)号: EP2921567A1公开(公告)日: 2015-09-23
- 发明人: NAKAI, Manabu , YASUNAGA, Shigenobu
- 申请人: Kabushiki Kaisha Kobe Seiko Sho (Kobe Steel, Ltd.) , UACJ Corporation , Nippon Light Metal Company, Ltd.
- 申请人地址: 2-4, Wakinohama-Kaigandori 2-chome Chuo-ku Kobe-shi, Hyogo 651-8585 JP
- 专利权人: Kabushiki Kaisha Kobe Seiko Sho (Kobe Steel, Ltd.),UACJ Corporation,Nippon Light Metal Company, Ltd.
- 当前专利权人: Kabushiki Kaisha Kobe Seiko Sho (Kobe Steel, Ltd.),UACJ Corporation,Nippon Light Metal Company, Ltd.
- 当前专利权人地址: 2-4, Wakinohama-Kaigandori 2-chome Chuo-ku Kobe-shi, Hyogo 651-8585 JP
- 代理机构: Müller-Boré & Partner Patentanwälte PartG mbB
- 优先权: JP2012253739 20121119
- 国际公布: WO2014077391 20140522
- 主分类号: C22C21/06
- IPC分类号: C22C21/06 ; C22C21/02 ; C22F1/05 ; F17C1/14 ; C22F1/00
摘要:
An aluminum alloy material for a high-pressure hydrogen gas container contains 0.6 to 1.5 mass% of Si, 0.6 to 1.6 mass% of Mg, 0.1 to 1.0 mass% of Cu, 0.05 to 0.4 mass% of Fe, 0.9 mass% or less of Mn, 0.3 mass% or less of Cr, 0.15 mass% or less of Zr, 0.2 mass% or less of V, 0.25 mass% or less of Zn, and 0.1 mass% or less of Ti, with the balance consisting in Al and inevitable impurities. The total content of Mn, Cr, Zr, and V is 0.05 mass% or more. The material has a yield strength S (MPa) and an electrical conductivity E (IACS%) satisfying formulae (1) and (2). The material has a yield strength S of 270 MPa or more and an electrical conductivity of 36 IACS% or more. (1): S ≤ -10.46 x E + 801, (2): S ≥ -25 x E + 1296
公开/授权文献