Invention Grant
- Patent Title: Lithium-ion secondary battery, fabricating method therof, and electronic device
-
Application No.: US15346932Application Date: 2016-11-09
-
Publication No.: US10128529B2Publication Date: 2018-11-13
- Inventor: Ai Nakagawa , Teppei Oguni , Kai Kimura , Rika Yatabe
- Applicant: SEMICONDUCTOR ENERGY LABORATORY CO., LTD.
- Applicant Address: JP Kanagawa-ken
- Assignee: Semiconductor Energy Laboratory Co., Ltd.
- Current Assignee: Semiconductor Energy Laboratory Co., Ltd.
- Current Assignee Address: JP Kanagawa-ken
- Agency: Nixon Peabody LLP
- Agent Jeffrey L. Costella
- Priority: JP2015-222748 20151113
- Main IPC: H01M6/04
- IPC: H01M6/04 ; H01M10/0525 ; H01M4/133 ; H01M4/136 ; H01M4/36 ; H01M4/58 ; H01M4/587 ; H01M4/66 ; H01M10/04 ; H01M10/0567 ; H01M10/058 ; G01R31/36 ; G01R31/44 ; H01M4/62 ; H01M10/0568 ; H01M10/0569 ; H02J7/00 ; H01M10/42

Abstract:
A lithium-ion secondary battery with a high capacity retention rate is provided. In addition, a fabricating method of a lithium-ion secondary battery with a high capacity retention rate is provided. The lithium-ion secondary battery includes a positive electrode, a negative electrode, and an electrolyte solution. The negative electrode includes a negative electrode active material layer. The electrolyte solution includes at least one of lithium bis(trifluoromethanesulfonyl)amide (LiTFSA) and lithium bis(fluorosulfonyl)amide (LiFSA). The electrolyte solution includes vinylene carbonate (VC). A coating film including lithium oxide is on a surface of the negative electrode active material layer. A fabricating method of a lithium-ion secondary battery includes a first step of enclosing a positive electrode, a negative electrode, and an electrolyte solution in an exterior body, and a second step of annealing the exterior body enclosing the positive electrode, the negative electrode, and the electrolyte solution for 24 hours or longer after the first step. The annealing in the second step is performed at a temperature higher than or equal to 80° C. and lower than or equal to 100° C.