Methods for reducing surface defects
Abstract:
Methods for reducing a defective area in a strengthened substrate to produce a non-defective substrate are provided. The methods include contacting a strengthened defective substrate with a heated salt bath containing at least one monovalent salt, and removing the strengthened substrate from the bath. The strengthened substrate, before being contacted with the salt bath, is a defective substrate having at least one defective area and one or more non-defective area. Upon removal from the salt bath, at least one defective area has been reduced or substantially removed to produce a non-defective substrate.