Steel sheet, member, and method for producing them
Abstract:
A steel sheet with a tensile strength (TS) of 1180 MPa or more, a member, and a method for producing them. In a region of the steel sheet within 4.9 μm in the thickness direction, a region with a Si concentration not more than one-third of the Si concentration in the chemical composition of the steel sheet and with a Mn concentration not more than one-third of the Mn concentration in the chemical composition of the steel sheet has a thickness of 1.0 μm or more. The lowest Si concentration LSi and the lowest Mn concentration LMn in the region within 4.9 μm in the thickness direction from the surface of the steel sheet and a Si concentration TSi and a Mn concentration TMn at a quarter thickness position of the steel sheet satisfy the following formula (1): LSi+LMn≤(TSi+TMn)/4  (1).