Invention Application
US20060096073A1 Method to make elastic shirting fabric comprising spandex and hard yarn 审中-公开
制造弹性衬衫的方法,包括氨纶和硬纱

Method to make elastic shirting fabric comprising spandex and hard yarn
Abstract:
Methods for making stretch shirting fabric having fabric weight less than 175 g/m2 and fabric stretch between 15% to 45% in the weft direction are disclosed. A corespun composite elastomeric yarn is produced either (a) by low draft (2.7× or below) core-spinning of the elastomeric yarn, or (b) by pretreating the corespun composite yarn in steam or heated water at temperatures of at least 110° C. to reduce yarn power before dyeing or weaving. The shirting fabric with such corespun composite elastomeric yarn in the weft meets end-use specifications without heat-setting.